Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon 32580B035 0.035" (0.889 mm) Uncured Silicone Rubber on PET Carrier

Category Polymer , Thermoset , Silicone , Silicone Rubber
Manufacturer Arlon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 32580B035 0.035" (0.889 mm) Uncured Silicone Rubber on PET Carrier.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: PETThis data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.34 g/cc
0.0484 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 76.2 microns
3.00 mil
Interleave
127 microns
5.00 mil
Carrier; Arlon SQA-TMS-003
889 microns
35.0 mil
Overall; Arlon SQA-TMS-003
889 microns
35.0 mil
Side 1; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 37
37
Silicone Property; ASTM D2240
Tensile Strength 6.55 MPa
950 psi
Silicone Property; ASTM D412
Elongation at Break 320 %
320 %
Silicone Property; ASTM D412
Tear Strength 26.3 kN/m
150 pli
Die B, Silicone Property; ASTM D624
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Electrical Properties Metric English Comments
Dielectric Strength 15.7 kV/mm
400 kV/in
ASTM D149
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 204 °C
2.00 hour

@Temperature 400 °F
Recommended Postcure Cycle
15.0 min

@Pressure 0.345 MPa,
Temperature 121 °C
0.250 hour

@Pressure 50.0 psi,
Temperature 250 °F
Recommended Cure Cycle
Shelf Life 6.00 Month

@Temperature 23.9 °C
6.00 Month

@Temperature 75.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Black
Translucent
Carrier
Total Product Weight (oz/yd2) 37
Arlon SQA-TMS-025
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved