| Category | Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber , Silicone, Molded, Glass Fiber Filled |
| Manufacturer | Arlon |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Arlon 19646B025 Silicone Rubber/Fiberglass Laminate.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.36 g/cc | 1.36 g/cc | Side 2 Silicone Property; Arlon SQA-TMS-024 |
| 1.38 g/cc | 1.38 g/cc | Side 1 Silicone Property; Arlon SQA-TMS-024 | |
| Thickness | 102 microns | 4.00 mil | silicone, side 1; Arlon SQA-TMS-003 |
| 178 microns | 7.00 mil | silicone, side 2; Arlon SQA-TMS-003 | |
| 356 microns | 14.0 mil | substrate; Arlon SQA-TMS-003 | |
| 635 microns | 25.0 mil | overall; Arlon SQA-TMS-003 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 51 | 51 | Side 1 Silicone Property; ASTM D2240 |
| 56 | 56 | Side 2 Silicone Property; ASTM D2240 | |
| Tensile Strength, Ultimate | 5.17 MPa | 750 psi | Side 2 Silicone Property; ASTM D412 |
| 5.31 MPa | 770 psi | Side 1 Silicone Property; ASTM D412 | |
| Elongation at Break | 265 % | 265 % | Side 1 Silicone Property; ASTM D412 |
| 765 % | 765 % | Side 2 Silicone Property; ASTM D412 | |
| Adhesive Bond Strength | 0.0689 MPa | 10.0 psi | Arlon SQA-TMS-011 |
| Tear Strength | 10.5 kN/m | 60.0 pli | Side 2 Silicone Property; ASTM D624 |
| 10.9 kN/m | 62.0 pli | Side 1 Silicone Property; ASTM D624 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
| Minimum Service Temperature, Air | -56.7 °C | -70.0 °F |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Strength | 18.7 kV/mm | 476 kV/in | ASTM D149 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Cure Time | 15.0 min @Pressure 0.345 MPa, Temperature 121 °C |
0.250 hour @Pressure 50.0 psi, Temperature 250 °F |
|
| Shelf Life | 6.00 Month @Temperature 21.1 °C |
6.00 Month @Temperature 70.0 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Color | Black |