Arlon 26122P020 0.020" Cured Silicone Rubber/Laminated PTFE Film

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , Thermoset , Silicone , Silicone Rubber
Manufacturer Arlon
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Arlon 26122P020 0.020" Cured Silicone Rubber/Laminated PTFE Film.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Design/Construction:Interleave: 0.002" ETFESide 1: Cured Silicone RubberLaminated Substrate: Cast PTFE FilmThis data represents typical values for the production material and should not be used as material specifications.Information provided by ARLON Silicone Technologies Division.
Physical Properties Metric English Comments
Density 1.28 g/cc
0.0462 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 76.2 microns
3.00 mil
Skived PTFE; Arlon SQA-TMS-003
432 microns
17.0 mil
Side 1; Arlon SQA-TMS-003
508 microns
20.0 mil
Overall Thickness; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
Silicone Property; ASTM D2240
Tensile Strength 6.89 MPa
1000 psi
Silicone Property; ASTM D412
Elongation at Break 150 %
150 %
Silicone Property; ASTM D412
Thermal Properties Metric English Comments
Maximum Service Temperature, Inert 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Processing Properties Metric English Comments
Shelf Life 60.0 Month

@Temperature 21.1 °C
60.0 Month

@Temperature 70.0 °F
Descriptive Properties Value Comments
Color Pink
Silicone
White
PTFE