Category Polymer , Thermoset , Silicone , Silicone Rubber
Manufacturer Arlon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 32980X040 0.040" Uncured Silicone Rubber on Polyester Film.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Design/Construction:Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: Polyester FilmThis data represents typical values for the production material and should not be used as material specifications.Information provided by ARLON Silicone Technologies Division.
Physical Properties Metric English Comments
Density 1.60 g/cc
0.0578 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 127 microns
5.00 mil
Carrier; Arlon SQA-TMS-003
1020 microns
40.0 mil
Silicone; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 72
72
Silicone Property; ASTM D2240
Tensile Strength 4.83 MPa
700 psi
Silicone Property; ASTM D412
Elongation at Break 190 %
190 %
Silicone Property; ASTM D412
Thermal Properties Metric English Comments
Maximum Service Temperature, Inert 180 °C
356 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Flammability, UL94 V-0
V-0
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature 21.1 °C
12.0 Month

@Temperature 70.0 °F
Descriptive Properties Value Comments
Color Gray
Silicone
Translucent
Carrier
Total Product Weight (oz/yd2) 47.2
Arlon SQA-TMS-025