Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 290 - 320 °C | 554 - 608 °F | |
PolyOne OnForce™ LFT NN-30LCF/002 Grey Polyamide 66 (Nylon 66) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Melt Temperature | 290 - 320 °C | 554 - 608 °F | |
Idemitsu Kosan Xarec® N WA 7010 SPS, 10% Glass Filled
(discontinued **) Crystalline Polymer Blend, Glass Filled. Used in Automotive Electronics applications. |
|||
Melt Temperature | 290 °C | 554 °F | DAM; Optimum |
DuPont Performance Polymers Zytel® 101L BKB080 Nylon 66
(Unverified Data**) Zytel® 101L BKB080 is a lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Melt Temperature | 290 °C | 554 °F | DAM; Optimum |
DuPont Performance Polymers Zytel® 103FHS BKB009 Nylon 66
(Unverified Data**) Zytel® 103FHS BKB009 is a heat stabilized, internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Perf.. |
|||
Melt Temperature | 290 °C | 554 °F | DAM; Optimum |
DuPont Performance Polymers Zytel® E41HSB NC010 Nylon 66
(Unverified Data**) Zytel® E41HSB is an unreinforced, high viscosity, heat stabilized polyamide 66 for injection molding and extrusion.Information provided by DuPont Performance Polymers |
|||
Melt Temperature | 290 - 329 °C | 554 - 625 °F | Average value: 316 °C Grade Count:8 |
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 40% Carbon Fiber Filler". Specific grades with carbon fiber content bet.. |
|||
Melt Temperature | 290 °C | 554 °F | for test specimens; ISO 294 |
Lanxess Durethan® AKV 30 000000 Nylon 66, Glass Fiber Reinforced PA 66, 30% glass fibers, injection moldingInformation provided by LANXESS. |
|||
Melt Temperature | 290 °C | 554 °F | for test specimens; ISO 294 |
Lanxess Durethan® AKV 35 HR H2.0 901510 Nylon 66, Glass Fiber Reinforced PA 66, 35% glass fibers, injection molding, heat-aging stabilized, hydrolysis stabilizedInformation provided by LANXESS. |
|||
Melt Temperature | 290 - 310 °C | 554 - 590 °F | |
LATI Larton G/40 PPS, 40% Glass Fiber Reinforced Polyphenylene Sulfide (PPS) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Melt Temperature | 290 - 320 °C | 554 - 608 °F | |
LATI Larton GK/400 PPS, Glass/Carbon Fiber Reinforced Polyphenylene Sulfide (PPS) based compound. Glass fibers / Carbon fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa &.. |
|||
Melt Temperature | 290 - 310 °C | 554 - 590 °F | |
LATI Larton MDT16-02 PPS Polyphenylene Sulfide (PPS) based compound. Magnetic detectable filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & M.. |
|||
Melt Temperature | 290 °C | 554 °F | for test specimens; ISO 294 |
Lanxess Durethan® AKV 40 H3.0 000000 Nylon 66, Glass Fiber Reinforced PA 66, 40% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS. |
|||
Melt Temperature | 290 - 310 °C | 554 - 590 °F | |
LATI Larton L K/20 L-PPS, 20% Carbon Fiber Reinforced Linear Polyphenylene Sulfide (L-PPS) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle.. |
|||
Melt Temperature | 290 - 310 °C | 554 - 590 °F | |
LATI Latilub 80-10T G/40 PPS, 40% Glass Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyphenylene Sulfide (PPS). PTFE. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |
|||
Melt Temperature | 290 - 315 °C | 554 - 599 °F | |
Styron EMERGEâ„¢ 4202-15 MFR Polycarbonate EMERGEâ„¢ PC 4202-15 advanced resin is 20% glass reinforced polycarbonate containing mold release for optimal processing. This resin exhibits high modulus and excellent dimensional stability. A.. |
|||
Melt Temperature | 290 - 310 °C | 554 - 590 °F | |
A. Schulman SCHULAMID® 66 GF13 13% Glass Fiber Reinforced Nylon 66 Information provided by A. Schulman. |
|||
Melt Temperature | 290 - 310 °C | 554 - 590 °F | |
A. Schulman SCHULAMID® 66 GF33HS 33% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Melt Temperature | 290 - 310 °C | 554 - 590 °F | |
A. Schulman SCHULAMID® 66 GF20H 20% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Melt Temperature | 290 - 310 °C | 554 - 590 °F | |
A. Schulman SCHULAMID® 66 MK4015 40% Glass Fiber/Mineral Reinforced 66 Information provided by A. Schulman. |
|||
Melt Temperature | 290 - 310 °C | 554 - 590 °F | |
A. Schulman SCHULAMID® 66 GF20H 20% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Melt Temperature | 290 °C | 554 °F | Injection Molding; ISO 294 |
Covestro Makrolon® 2656 Polycarbonate ISO 7391-PC,MR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 12.5 cm3/10 minFood contact qualityMedium viscosityEasy releaseGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CAv.. |
|||
Melt Temperature | 290 °C | 554 °F | Injection Molding; ISO 294 |
Covestro Makrolon® 2665 Polycarbonate, Flame Retardant Grade ISO 7391-PC,MFR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 12.5 cm3/10 minChlorine- and bromine-free flame retardantUL 94V-2/1.5 mm and 3.0 mmMedium viscosityEasy releaseInjection molding - Melt temp.. |
|||
Melt Temperature | 290 °C | 554 °F | Injection Molding; ISO 294 |
Covestro Makrolon® LTG2623 Polycarbonate PreprocessingMax. Water content |
|||
Melt Temperature | 290 °C | 554 °F | DAM; Optimum |
DuPont Performance Polymers Zytel® EFE8089B BK416 Nylon 66 Zytel® EFE8089B BK416 is a 33% fiber reinforced, heat stabilized, lubricated, toughened polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Melt Temperature | 290 - 310 °C | 554 - 590 °F | Injection-molding/Extrusion |
BASF Ultramid® A3WG10 BK 00564 50% Glass Filled PA66 (Conditioned) Description: 50% glass-fiber reinforced injection-molding grade with high heat aging resistance for technical articles of very high stiffness.Information provided by BASF |
|||
Melt Temperature | 290 - 300 °C | 554 - 572 °F | Injection-molding/Extrusion |
BASF Ultramid® A4H PA66 (Dry) Description: Highly heat aging resistant, medium-viscosity injection-molding grade for highly stressed parts such as bearing cages, gearwheels, spool bodies and chain drive tensioners.Information pr.. |
|||
Melt Temperature | 290 °C | 554 °F | DAM; Optimum |
DuPont Performance Polymers Zytel® 77G43L BK031 Nylon 612
(Unverified Data**) Zytel® 77G43L BK031 is a 43% glass fiber reinforced, black polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Melt Temperature | 290 - 310 °C | 554 - 590 °F | |
LATI LARTON GCE/60 60% Mixed Glass Fiber and Special Mineral Filled Polyphenylene sulfide (PPS)
(discontinued Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex.. |
|||
Melt Temperature | 290 °C | 554 °F | DAM; Optimum |
DuPont Performance Polymers Zytel® EFE1068 NC010T Nylon 66
(Unverified Data**) Zytel® EFE1068 NC010T is a lubricated polyamide 66 for injection molding. It has excellent flow characteristics and was developed for fast production cycles and high productivity applications.Info.. |
|||
Melt Temperature | 290 °C | 554 °F | DAM; Optimum |
DuPont Performance Polymers Zytel® FE5382 BK276 Nylon 612
(Unverified Data**) Zytel® FE5382 BK276 is a 33% glass fiber reinforced, heat stabilized, black polyamide 612 resin developed for electrical bobbins and encapsulation applications.Information provided by DuPont Perfor.. |