Material Notes:
Polyphenylene Sulfide (PPS) based compound. Magnetic detectable filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A.
Physical Properties Metric English Comments
Density 2.95 g/cc
0.107 lb/in³
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break 30.0 MPa

@Temperature 23.0 °C
4350 psi

@Temperature 73.4 °F
Elongation at Break 0.40 %

@Temperature 23.0 °C
0.40 %

@Temperature 73.4 °F
Tensile Modulus 12.0 GPa

@Temperature 23.0 °C
1740 ksi

@Temperature 73.4 °F
Charpy Impact Unnotched 0.600 J/cm²
2.86 ft-lb/in²
Charpy Impact, Notched 0.150 J/cm²
0.714 ft-lb/in²
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 210 °C
410 °F
Deflection Temperature at 1.8 MPa (264 psi) 180 °C
356 °F
Processing Properties Metric English Comments
Melt Temperature 290 - 310 °C
554 - 590 °F
Mold Temperature 130 - 140 °C
266 - 284 °F
Drying Temperature 130 - 150 °C

@Time 10800 sec
266 - 302 °F

@Time 3.00 hour
Descriptive Properties Value Comments
ISO Shrinkage - Pressure 60 MPa