| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | |
|
PolyOne OnFlex™ HFFR 310-01 Thermoplastic Elastomer (TPE)
OnFlex™ HFFR 310-01 is a non-halogen flame retardant material designed for cable jackets. New Product. Commercial specifications have not been established. - Non-halogen flame retardant - UL62 comp..
|
|||
| Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | |
|
PolyOne Stat-Tech™ AT-CB2/000 CR Acetal (POM) Copolymer
Stat-Tech™ AT-CB2/000 CR XP020229R2Information provided by PolyOne
|
|||
| Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | |
|
Oxford Polymers C-Acetal 10MF-900 BK Acetal
Product Description: Acetal Injection Molding Grade, 10 melt flow Processing and Delivery Form: Pellets and Injection MoldingSpecial Characteristics: Pre-colored blackInformation provided by Oxford..
|
|||
| Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | Injection Molding |
|
DuPont Performance Polymers Hytrel® 6646 NC010 TPC-ET
(Unverified Data**)
Hytrel® 6646 NC010 is a medium modulus grade with nominal hardness of 66D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like ..
|
|||
| Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | Dehumidified Dryer; Extrusion |
|
DuPont Performance Polymers Hytrel® 7246HS BK320 TPC-ET
(Unverified Data**)
Hytrel® 7246HS BK320 is a high modulus, heat stabilized, black grade with nominal hardness of 72D.Information provided by DuPont
|
|||
| Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | Injection Molding |
|
LG Chemical LI911 ASA
Description: Good Weatherability, High FlowApplication: Air-conditioner grill, Sawing Machine Cover, Electric/Electronic ApplicationsCAS: 26299-47-8Information provided by LG Chemical
|
|||
| Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | Extrusion Molding |
|
LG Chemical LI933 Co-Extrusion ASA
Description: Good Weatherability, Low GlossApplication: Canopy, Siding, Fence, (Roofing) TilesCAS: 26299-47-8Information provided by LG Chemical
|
|||
| Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | Injection Molding |
|
LG Chemical LUCEL FW700N Modified POM, Friction Resistance, Abrasion Resistance
Feature: Injection Molding, Modified POM, Friction Resistance, Abrasion ResistanceApplication: Gears, Printer Roller Pumps, Gear Worm WheelsCAS No. 66455-31-0Information provided by LG Chemical
|
|||
| Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | Injection Molding |
|
LG Chemical LUCEL FW715CS Modified POM, Friction Resistance, Abrasion Resistance
Feature: Injection Molding, Modified POM, Friction Resistance, Abrasion ResistanceApplication: Gears, Printer Roller Pumps, Gear Worm WheelsCAS No. 66455-31-0 and 471-34-1Information provided by LG ..
|
|||
| Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | Injection Molding |
|
LG Chemical LUCEL GC240 POM+GF40%, High Rigidity
Feature: Injection Molding, POM+GF40%, High RigidityApplication: Casings of Pump and Pivot BearingsCAS No. 66455-31-0 and 65997-17-3Information provided by LG Chemical
|
|||
| Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | Injection Molding |
|
LG Chemical LUCEL HI510 POM+Rubber, High Impact
Feature: Injection Molding, POM+Rubber, High ImpactApplication: Gears, Automobile ClipCAS No. 66455-31-0Information provided by LG Chemical
|
|||
| Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | Injection Molding |
|
LG Chemical LUCEL HI520 POM+Rubber, High Impact
Feature: Injection Molding, POM+Rubber, High ImpactApplication: GearsCAS No. 66455-31-0 and 155123-66-3Information provided by LG Chemical
|
|||
| Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | |
|
Lubrizol STAT-RITE® S-1107 Static Dissipative TPU
Description: Stat-Rite® S-1107 is a static dissipative TPU alloy. Stat-Rite S-1107 utilizes the patented Stat-Rite inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD ..
|
|||
| Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | |
|
Lubrizol Estane® GP 55 DB Thermoplastic Polyurethane
Type: Estane® GP 55DB is an aromatic polyester-based thermoplastic polyurethane (TPU).Features: Translucent spherical pellets.Uses: Injection molding partsAvailable in EuropeInformation Provided by..
|
|||
| Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | |
|
Lubrizol Estane® GP 58 DT Thermoplastic Polyurethane
Type: Estane® GP 58DT is an aromatic polyether-based thermoplastic polyurethane (TPU).Features: Translucent spherical pellets.Uses: Injection molding parts, animal identification tagsAvailable in E..
|
|||
| Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | |
|
Lubrizol ESTANE® GP52DB Ester Based Thermoplastic Polyurethane
Type: Estane® GP 52DB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b..
|
|||
| Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | |
|
Lubrizol ESTANE® GP55DT Ether Based Thermoplastic Polyurethane
Type: Estane® GP 55DT is an aromatic polyether-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding parts, animal identification tagsAvailable in ..
|
|||
| Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | |
|
Lubrizol ESTANE® GP60DB Ester Based Thermoplastic Polyurethane
Type: Estane® GP 60DB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding parts, animal identification tags.Available in..
|
|||
| Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | |
|
Lubrizol ESTANE® GP65AE Ester Based Thermoplastic Polyurethane
Type: Estane® GP 65AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b..
|
|||
| Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | |
|
Lubrizol ESTANE® GP80AB Ester Based Thermoplastic Polyurethane
Type: Estane® GP 80AB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b..
|
|||
| Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | |
|
Lubrizol ESTANE® GP85AB Ester Based Thermoplastic Polyurethane
Type: Estane® GP 85AB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsInformation provided by Lubrizol.
|
|||
| Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | |
|
Lubrizol ESTANE® GP95AB Ester Based Thermoplastic Polyurethane
Type: Estane® GP 95AB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding parts, animal identification tagsAvailable in ..
|
|||
| Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | Extrusion |
|
DuPont Performance Polymers Hytrel® HTR6108 TPC-ET
(Unverified Data**)
Hytrel® HTR6108 is a medium modulus grade, specially designed for good flexibility and low permeability to hydrocarbon fuels and oils. It has nominal hardness of 61D and can be processed by various..
|
|||
| Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | Injection Molding |
|
DuPont Performance Polymers Hytrel® HTR8636 NC010 TPC-ET
(Unverified Data**)
Hytrel® HTR8636 NC010 is a medium modulus Hytrel® grade with nominal durometer hardness of 40D. It contains non_discoloring stabilizer. It is specially suitable for extrusion processing.Informatio..
|
|||
| Dry Time | 1.00 - 3.00 hour | 1.00 - 3.00 hour | |
|
Ascend Performance Materials Vydyne® 20NSP1 Nylon 66, DAM
Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 43% Filler by Weight Additive:Nucleating AgentLubricant Features:Fast Molding CycleGeneral PurposeGood Mold Release Good..
|
|||
| Dry Time | 1.00 - 3.00 hour | 1.00 - 3.00 hour | |
|
Ascend Performance Materials Vydyne® 21SPG1 Nylon 66, DAM
Availability:Asia PacificEuropeNorth America Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood ToughnessHigh Rigidit..
|
|||
| Dry Time | 1.00 - 3.00 hour | 1.00 - 3.00 hour | |
|
Ascend Performance Materials Vydyne® 20NSP1 Nylon 66, DAM
Availability:Asia PacificEuropeNorth AmericaAdditive:LubricantNucleating Agent Features: Fast Molding CycleGeneral PurposeGood Mold ReleaseGood StiffnessHigh RigidityLubricatedNucleatedUses:Bearings..
|
|||
| Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | Extrusion |
|
DuPont Performance Polymers Hytrel® 4068FG TPC-ET
(Unverified Data**)
Hytrel® 4068FG is a high performance thermoplastic polyester elastomer with food compliance specificity.Information provided by DuPont Performance Polymers
|
|||
| Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | Dehumidified Dryer; Injection Molding |
|
DuPont Performance Polymers Hytrel® 7246HS NC010 TPC-ET
(Unverified Data**)
Hytrel® 7246HS NC010 is a high modulus, heat stabilized grade with nominal hardness of 72D.Information provided by DuPont
|
|||
| Dry Time | 1.00 - 3.00 hour | 1.00 - 3.00 hour | |
|
Ascend Performance Materials Vydyne® 21SPF1 Nylon 66, DAM
Vydyne® 21SPF1 is a general-purpose PA66 resin available in natural color. It is designed principally for injection-molding applications with the added benefits of improved flow during the molding ..
|
|||