Lubrizol STAT-RITE® E-1150 Ether-Type Static Dissipative Polymer

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP
Manufacturer Lubrizol (former Noveon)
Trade Name Stat-Rite®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol STAT-RITE® E-1150 Ether-Type Static Dissipative Polymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: IStat-Rite® E-1150 blend is a static dissipative thermoplastic polyurethane (TPU) alloy. Stat-Rite E-1150 utilizes the patented Stat-Rite inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD protection. Stat-Rite alloys retain uniform static dissipation properties even when injection molded or extruded.Features: Permanently static dissipativeHumidity independentSee-through clarityNo particulatesUltra-clean: low off-gassing, low ionics, low particulatesApplications: Cleanroom soft walls, windows and doorsVacuum tubingWork surface matsAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 88
88
ASTM D2240
Tensile Strength at Break 65.0 MPa
9430 psi
ASTM D412
Elongation at Break 760 %
760 %
ASTM D412
100% Modulus 0.00520 GPa
0.754 ksi
ASTM D412
300% Modulus 0.0124 GPa
1.80 ksi
ASTM D412
Tear Strength 68.0 kN/m
388 pli
ASTM D646
Electrical Properties Metric English Comments
Volume Resistivity 4.00e+10 ohm-cm
4.00e+10 ohm-cm
ASTM D257
Surface Resistivity per Square 1.00e+11 ohm
1.00e+11 ohm
ASTM D257
Static Decay 1.3 sec
1.3 sec
12% RH (+5000 V to 50 V); FTMS-101C
1.3 sec
1.3 sec
12% RH (-5000 V to -50 V); FTMS-101C
Processing Properties Metric English Comments
Drying Temperature 105 °C
221 °F
dehumidifying hopper
Dry Time 2.00 - 3.00 hour
2.00 - 3.00 hour