Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol STAT-RITE® S-1107 Static Dissipative TPU

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP
Manufacturer Lubrizol (former Noveon)
Trade Name Stat-Rite®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol STAT-RITE® S-1107 Static Dissipative TPU.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Stat-Rite® S-1107 is a static dissipative TPU alloy. Stat-Rite S-1107 utilizes the patented Stat-Rite inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD protection. Stat-Rite® IDP alloys provide consistent static dissipation even when extruded, injection molded or thermoformed into components.Features: Permanent static dissipativeHumidity insensitiveUltra-clean: low off-gassing, low ionic contaminationColorableDurable: Can be used for years and yearsApplications: ESD and Cleanroom TubingESD and Cleanroom HoseCleanroom CurtainsConveyor ESD Wear Strip, RollersESD and Cleanroom FilmAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol.
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 83
83
ASTM D2240
Tensile Strength 11.5 MPa
1670 psi
ASTM D412
4.52 MPa

@Strain 50.0 %
656 psi

@Strain 50.0 %
ASTM D412
5.21 MPa

@Strain 100 %
755 psi

@Strain 100 %
ASTM D412
6.43 MPa

@Strain 200 %
933 psi

@Strain 200 %
ASTM D412
Elongation at Break 695 %
695 %
ASTM D412
Electrical Properties Metric English Comments
Volume Resistivity 2.30e+8 ohm-cm
2.30e+8 ohm-cm
ASTM D257
Surface Resistance 4.80e+7 ohm
4.80e+7 ohm
12% RH; ESD S11.11
Surface Resistivity per Square 4.80e+8 ohm
4.80e+8 ohm
50%; ASTM D257
Static Decay 0.10 sec
0.10 sec
Charged Plate Monitor, 50% RH (+1000 V to 100 V)
<= 2.0 sec
<= 2.0 sec
12% RH (+5000 V to 50 V); FTMS-101C
<= 2.0 sec
<= 2.0 sec
12% RH (-5000 V to -50 V); FTMS-101C
Processing Properties Metric English Comments
Drying Temperature 105 °C
221 °F
dehumidifying hopper
Dry Time 2.00 - 3.00 hour
2.00 - 3.00 hour
Descriptive Properties Value Comments
Color Natural
Users viewing this material also viewed the following: