Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol Estane® GP 52 DT Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Lubrizol Estane® GP 52 DT Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Type: Estane® GP 52DT is an aromatic polyester-based thermoplastic polyurethane (TPU).Features: Translucent spherical pellets.Uses: Injection molding parts, animal identification tagsAvailable in EuropeInformation Provided by The Lubrizol Corporation
Physical Properties Metric English Comments
Specific Gravity 1.15 g/cc
1.15 g/cc
ISO 2781
Maximum Moisture Content 0.050
0.050
Melt Flow 20 - 40 g/10 min

@Load 8.70 kg,
Temperature 205 °C
20 - 40 g/10 min

@Load 19.2 lb,
Temperature 401 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 53
53
ISO 868
Tensile Strength, Ultimate 52.0 MPa
7540 psi
ISO 527
Elongation at Break 525 %
525 %
Modulus of Elasticity 0.0780 GPa
11.3 ksi
ISO 527
50% Modulus 0.0120 GPa
1.74 ksi
100% Modulus 0.0140 GPa
2.03 ksi
300% Modulus 0.0540 GPa
7.83 ksi
Rebound 27 %
27 %
ISO 4662
Tear Strength 105 kN/m
599 pli
Nicked; ISO 34-1B
132 kN/m
753 pli
Unnicked; ISO 34-1B
Abrasion 50
50
mm<sup>3</sup>; ISO 4649
Compression Set 25 %

@Temperature 22.0 °C,
Time 252000 sec
25 %

@Temperature 71.6 °F,
Time 70.0 hour
ISO 815
38 %

@Temperature 70.0 °C,
Time 86400 sec
38 %

@Temperature 158 °F,
Time 24.0 hour
ISO 815
Thermal Properties Metric English Comments
Vicat Softening Point 94.0 °C
201 °F
A50; ISO 306
Processing Properties Metric English Comments
Feed Temperature 40.0 °C
104 °F
Injection
Nozzle Temperature 205 - 215 °C
401 - 419 °F
Injection
Zone 1 195 - 205 °C
383 - 401 °F
Injection
Zone 2 200 - 210 °C
392 - 410 °F
Injection
Zone 3 205 - 215 °C
401 - 419 °F
Injection
Zone 4 210 - 220 °C
410 - 428 °F
Injection
Drying Temperature 100 °C
212 °F
Dry Time 2.00 - 3.00 hour
2.00 - 3.00 hour
Dew Point -30.0 °C
-22.0 °F
Users viewing this material also viewed the following: