| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.20 g/cc | 0.0434 lb/in³ | ISO 1183 |
| Water Absorption | 0.20 % @Temperature 23.0 °C |
0.20 % @Temperature 73.4 °F |
Equilibrium 50%RH; ISO 62 |
| 0.60 % @Temperature 23.0 °C |
0.60 % @Temperature 73.4 °F |
Immersion 24h; ISO 62 | |
| 0.60 % @Temperature 23.0 °C |
0.60 % @Temperature 73.4 °F |
Saturation, immersed; ISO 62 | |
| Linear Mold Shrinkage, Flow | 0.014 cm/cm @Thickness 2.00 mm |
0.014 in/in @Thickness 0.0787 in |
ISO 294-4 |
| Linear Mold Shrinkage, Transverse | 0.014 cm/cm @Thickness 2.00 mm |
0.014 in/in @Thickness 0.0787 in |
ISO 294-4 |
| Melt Flow | 8.0 g/10 min @Load 2.16 kg, Temperature 220 °C |
8.0 g/10 min @Load 4.76 lb, Temperature 428 °F |
ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 51 | 51 | 15s; ISO 868 |
| <= 56 | <= 56 | ISO 868 | |
| Tensile Strength at Break | 40.0 MPa @Temperature 23.0 °C |
5800 psi @Temperature 73.4 °F |
ISO 527 (1BA bar) |
| Tensile Stress | 6.60 MPa @Strain 5.00 %, Temperature 23.0 °C |
957 psi @Strain 5.00 %, Temperature 73.4 °F |
ISO 527 (1BA bar) |
| 10.2 MPa @Strain 10.0 %, Temperature 23.0 °C |
1480 psi @Strain 10.0 %, Temperature 73.4 °F |
ISO 527 (1BA bar) | |
| Elongation at Break | 480 % @Temperature 23.0 °C |
480 % @Temperature 73.4 °F |
ISO 527 (1BA bar) |
| 600 % @Temperature 23.0 °C |
600 % @Temperature 73.4 °F |
ISO 527 (1BA bar) | |
| Tensile Modulus | 0.167 GPa @Temperature 23.0 °C |
24.2 ksi @Temperature 73.4 °F |
ISO 527 |
| Charpy Impact, Notched | 14.5 J/cm² @Temperature -40.0 °C |
69.0 ft-lb/in² @Temperature -40.0 °F |
ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 201 °C | 394 °F | 10°C/min; ISO 11357-1/-3 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 225 °C | 437 °F | Optimum; Extrusion |
| 220 - 235 °C | 428 - 455 °F | Extrusion | |
| 230 °C | 446 °F | Optimum; Injection Molding | |
| 220 - 250 °C | 428 - 482 °F | Injection Molding | |
| Mold Temperature | 45.0 °C | 113 °F | Optimum; Injection Molding |
| 45.0 - 55.0 °C | 113 - 131 °F | Injection Molding | |
| Drying Temperature | 100 °C | 212 °F | Extrusion |
| 100 °C | 212 °F | Injection Molding | |
| Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | Dehumidified Dryer; Extrusion |
| 2.00 - 3.00 hour | 2.00 - 3.00 hour | Dehumidified Dryer; Injection Molding | |
| Moisture Content | <= 0.060 % | <= 0.060 % | Extrusion |
| <= 0.080 % | <= 0.080 % | Injection Molding |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Generic | TPC-ET | |
| Material Status | Preliminary Data | |
| Part Marking Code | >TPC-ET< | ISO 11469 |
| Region Available - Global | Yes | |
| Resin Identification | TPC-ET | ISO 1043 |