| Category | Polymer , Thermoplastic , Elastomer, TPE , Polyester, TP , Polyester Thermoplastic Elastomer |
| Manufacturer | |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | DuPont Performance Polymers Hytrel® 7246HS NC010 TPC-ET
(Unverified Data**).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.25 g/cc | 0.0452 lb/in³ | ISO 1183 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 66 | 66 | 15s; ISO 868 |
| <= 70 | <= 70 | ISO 868 | |
| Tensile Strength at Break | 52.0 MPa @Temperature 23.0 °C |
7540 psi @Temperature 73.4 °F |
ISO 527 |
| Tensile Stress | 23.0 MPa @Strain 10.0 %, Temperature 23.0 °C |
3340 psi @Strain 10.0 %, Temperature 73.4 °F |
ISO 527 |
| 24.0 MPa @Strain 50.0 %, Temperature 23.0 °C |
3480 psi @Strain 50.0 %, Temperature 73.4 °F |
ISO 527 | |
| Elongation at Break | 450 % @Temperature 23.0 °C |
450 % @Temperature 73.4 °F |
ISO 527 |
| 560 % @Temperature 23.0 °C |
560 % @Temperature 73.4 °F |
ISO 527 | |
| Tensile Modulus | 0.430 GPa @Temperature 23.0 °C |
62.4 ksi @Temperature 73.4 °F |
ISO 527 |
| Flexural Modulus | 0.500 GPa @Temperature 23.0 °C |
72.5 ksi @Temperature 73.4 °F |
ISO 178 |
| Charpy Impact, Notched | 0.500 J/cm² @Temperature -40.0 °C |
2.38 ft-lb/in² @Temperature -40.0 °F |
ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 216 °C | 421 °F | 10°C/min; ISO 11357-1/-3 |
| Brittleness Temperature | -65.0 °C | -85.0 °F | ISO 974 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 240 °C | 464 °F | Optimum; Extrusion |
| 235 - 250 °C | 455 - 482 °F | Extrusion | |
| 235 - 255 °C | 455 - 491 °F | Injection Molding | |
| 245 °C | 473 °F | Optimum; Injection Molding | |
| Mold Temperature | 45.0 °C | 113 °F | Optimum; Injection Molding |
| 45.0 - 55.0 °C | 113 - 131 °F | Injection Molding | |
| Drying Temperature | 110 °C | 230 °F | Extrusion |
| 110 °C | 230 °F | Injection Molding | |
| Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | Dehumidified Dryer; Extrusion |
| 2.00 - 3.00 hour | 2.00 - 3.00 hour | Dehumidified Dryer; Injection Molding | |
| Moisture Content | <= 0.060 % | <= 0.060 % | Extrusion |
| <= 0.080 % | <= 0.080 % | Injection Molding |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Appearance | Natural | |
| Features | Chemical Resistance | |
| Creep Resistance, Good | ||
| Energy Absorption, High | ||
| Food Contact Acceptable | ||
| Hardness, High | ||
| Noise Dampening | ||
| Forms | Pellets | |
| Generic | TPC-ET | |
| Material Status | Preliminary Data | |
| Part Marking Code | >TPC-ET< | ISO 11469 |
| Processing Method | Extrusion | |
| Injection Molding | ||
| Product Category | Extrusion Resins | |
| High Performance Hytrel®® Resins | ||
| Region Available - Global | Yes | |
| Resin Identification | TPC-ET | ISO 1043 |
| RoHS Compliance | Contact Manufacturer | |
| Uses | Automotive | |
| Compounding | ||
| Hose | ||
| Industrial Applications | ||
| Monofilaments |