Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 87.8 - 93.3 °C | 190 - 200 °F | |
PTS Trilac® ABS-HS4000 General Purpose ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Drying Temperature | 87.8 - 93.3 °C | 190 - 200 °F | |
PTS Trilac® ABS-HS5500 High Impact ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Drying Temperature | 87.8 - 93.3 °C | 190 - 200 °F | |
PTS Trilac® ABS-HS7500 High Impact ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Drying Temperature | 87.8 °C | 190 °F | max 6 hours |
PTS Trilac® FR3800 Flame Retardant ABS Resin, RoHS Compliant Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Drying Temperature | 87.8 °C | 190 °F | max 6 hours |
PTS Trilac® FR3800-V Flame Retardant ABS Resin, RoHS Compliant Contains UV absorber.Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Drying Temperature | 87.8 °C | 190 °F | |
PolyOne Edgetek® X TR2-10GF/000 NATURAL Copolyester The Edgetek™ engineering thermoplastics compounds made with Eastman Tritan™ copolyester offer a wide range of performance and properties with the addition of reinforcing additives. By utilizing Ea.. |
|||
Drying Temperature | 88.0 °C @Time 14400 sec |
190 °F @Time 4.00 hour |
|
PlastiComp Complet® LCF40 - TPU Rigid Thermoplastic Polyurethane, 40% Long Carbon Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyurethane with 40% carbon fiber reinforcementInformation provided by PlastiComp, In.. |
|||
Drying Temperature | 88.0 °C @Time 14400 sec |
190 °F @Time 4.00 hour |
|
PlastiComp Complet® LCF50 - TPU Rigid Thermoplastic Polyurethane, 50% Long Carbon Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyurethane with 50% carbon fiber reinforcementInformation provided by PlastiComp, Inc. |
|||
Drying Temperature | 88.0 °C | 190 °F | |
Eastman Eastalloy MA510 Polymer
(discontinued **) Eastalloy MA510 Polymer is a clear copolyester/polycarbonate alloy. It affords the consumer excellent impact strength, chemical resistance, dimensional stability, low shrinkage rates and other enhan.. |
|||
Drying Temperature | 88.0 °C @Time 14400 sec |
190 °F @Time 4.00 hour |
|
PlastiComp Complet® LGF60 - TPU Rigid Thermoplastic Polyurethane, 60% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Rigid polyurethane with 60% long glass fiber reinforcementInformation provided by Plas.. |
|||
Drying Temperature | 88.0 °C @Time 7200 - 14400 sec |
190 °F @Time 2.00 - 4.00 hour |
|
Ineos ABS Triax® 1185 ABS/Nylon Alloy, Injection Molding Grade Triax® 1185 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with excellent processability, good chemical resistance, g.. |
|||
Drying Temperature | 88.0 °C @Time 7200 - 14400 sec |
190 °F @Time 2.00 - 4.00 hour |
|
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (Conditioned) Triax® 3050 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with improved stability to light exposure, excellent proce.. |
|||
Drying Temperature | 87.8 - 110 °C | 190 - 230 °F | |
Star Plastics PC/ABSQX7004 Molding Grade PC/ABS Information provided by Star Plastics, Inc. |
|||
Drying Temperature | 87.8 - 110 °C | 190 - 230 °F | |
Star Plastics PC/ABSQX7005 Molding Grade PC/ABS Information provided by Star Plastics, Inc. |
|||
Drying Temperature | 87.8 - 93.3 °C | 190 - 200 °F | |
TPI Porene® ABS-AN450 Flame Retardant ABS Resin Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Drying Temperature | 87.8 - 93.3 °C | 190 - 200 °F | |
TPI Porene® ABS-GA850 High Impact ABS Resin Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Drying Temperature | 87.8 - 93.3 °C | 190 - 200 °F | |
TPI Porene® ABS-KU650 Super High Heat ABS Resin Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Drying Temperature | 88.0 - 104 °C | 190 - 219 °F | air dew point <-40°C |
Lubrizol Estane® 2103-55D Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Load bearing capacityAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in .. |
|||
Drying Temperature | 88.0 - 104 °C | 190 - 219 °F | Air dew point <-40°C |
Lubrizol Estane® 2355-55DE Thermoplastic Polyurethane Type: Pellethane® 2355-55DE is a thermoplastic polyurethane elastomer.Information Provided by The Lubrizol Corporation |
|||
Drying Temperature | 88.0 - 104 °C | 190 - 219 °F | air dew point <-40°C |
Lubrizol Estane® 2355-95AE Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Fuel resistant, extrusion laminate coatingAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Dow Chemical.Lubrizol acquired the Pellethane.. |
|||
Drying Temperature | 88.0 - 104 °C | 190 - 219 °F | Air dew point <-40°C |
Lubrizol Estane® 2355-95AEF Thermoplastic Polyurethane Type: Pellethane® 2355-95AEF is a thermoplastic polyurethane elastomer.Feature: Film resin, Fuel resistant, Blow molding grade resin.Information Provided by The Lubrizol Corporation |
|||
Drying Temperature | 88.0 °C | 190 °F | |
Eastman Tritan LX150HF Copolyester Eastman Tritan LX150HF is a high flow grade of an amorphous copolyester with excellent appearance and clarity. Eastman Tritan LX150HF has viscosity reductions of 40-50% relative to standard grades .. |
|||
Drying Temperature | 88.0 °C | 190 °F | |
Eastman Tritan LX201 Copolyester Eastman Tritan LX201 is an amorphous copolyester with excellent appearance and clarity. Tritan LX201 contains a mold release derived from vegetable based sources. Its most outstanding features are.. |
|||
Drying Temperature | 88.0 °C | 190 °F | |
Eastman Tritan TX1500HF Copolyester Eastman Tritan TX1500HF is a high flow grade of Eastman Tritan. Eastman Tritan TX1500HF has viscosity reductions of 40-50% relative to Eastman Tritan copolyester TX1000. Other outstanding features.. |
|||
Drying Temperature | 88.0 °C | 190 °F | |
Eastman Tritan TX2001 Copolyester Eastman Tritan TX2001 is an amorphous copolyester with excellent appearance and clarity. Eastman Tritan TX2001 contains a mold release derived from vegetable based sources. Its most outstanding fe.. |
|||
Drying Temperature | 88.0 °C | 190 °F | |
Eastman Tritan WX510 Copolyester Eastman Tritan WX510 is a transparent blue resin specifically developed for blow molded bottles. Extremely high melt strength makes the resin an excellent choice when manufacturing large bottles. .. |
|||
Drying Temperature | 88.0 - 104 °C | 190 - 219 °F | air dew point <-40°C |
Lubrizol Estane® 2103-90AENH Film Grade Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: NSF Standard 61 Certified, FDA ComplianceAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane prod.. |