Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 216 - 260 °C | 420 - 500 °F | |
Multibase Multi-Pro® 1508 M Polypropylene Mica Filled, 15% by weight.Features:Rigidity, HighImpact Resistance, GoodForms:PelletsProcessing Methods:Injection MoldingUses:Automotive ApplicationsInformation provided by Multibase |
|||
Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
RheTech Products CC40P100-00 40% Calcium Carbonate Reinforced Polypropylene, Natural Applications: Consumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
RheTech Products CC40P100-00EG 40% Calcium Carbonate Reinforced Polypropylene, Natural, Extrusion Grade Applications: Consumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
RheTech Products GC40P100-01 40% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black Applications: Consumer goodsBracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
RheTech Products GC43P250-00 43% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural Applications: Consumer goodsFunctional supportsHead lamp bracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
RheTech Products GC43P250-777 43% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Ivory Applications: BracketsStructural supportsDurable GoodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
RheTech Products GC45P200-01UV 45% Glass Fiber Reinforced Polypropylene Copolymer, UV Stabilized, Black Applications: BracketsUnderhood componentsLarge structural supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
RheTech Products M40P100-01 40% Mica Reinforced Polypropylene, Black Applications: Structural componentsAir ducts and dampenersFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
RheTech Products RCT140-01A 40% Talc Reinforced Polypropylene, Black, Recycled Content Applications: HVAC ductworkI/P componentsFuse panel assembliesUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
RheTech Products T40P100-04 40% Talc Reinforced Polypropylene, White Applications: Automotive componentsConsumer productsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
RheTech Products T40P105-04 40% Talc Reinforced Polypropylene, White, 5% Titanium Dioxide Applications: Instrument cluster masksAutomotive componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
RheTech Products T40P108-01A 40% Talc Reinforced Polypropylene, Black Applications: Underhood componentsHVAC ductworkFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
RheTech Products T40P250-00 40% Talc Reinforced Polypropylene Copolymer, Natural Applications: BracketsHousingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 216 °C | 420 °F | |
PTS Trilac® ABS-HH2500 Super High Heat ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 216 - 238 °C | 420 - 460 °F | |
Polymer Resources ABS-GP-HH General Purpose ABS, High Heat General Purpose Acrylonitrile Butadiene Styrene, High HeatProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Middle Barrel Temperature | 216 °C | 420 °F | |
PTS Trilac® ABS-HF5500 High Flow ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 216 °C | 420 °F | |
PTS Trilac® ABS-HS6500 High Impact ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 216 - 232 °C | 420 - 450 °F | |
Fiberfil® J-69/10/E High performance polypropylene Homopolymer, 10% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Middle Barrel Temperature | 216 - 232 °C | 420 - 450 °F | |
Fiberfil® J-69/30/E High performance polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Middle Barrel Temperature | 216 - 232 °C | 420 - 450 °F | |
Fiberfil® J-69/30/E/M High performance polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Middle Barrel Temperature | 216 - 238 °C | 420 - 460 °F | |
LTL Color Compounds ColorFast® ACR100 Polymethylmethacrylate High heat injection molding grade of PMMAAll information provided by LTL Color Compounders, Inc. |
|||
Middle Barrel Temperature | 216 °C | 420 °F | |
TPI Porene® ABS-GA803 High Gloss, UV Resistant ABS Resin Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 216 °C | 420 °F | |
TPI Porene® ABS-GA850 High Impact ABS Resin Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 216 - 227 °C | 420 - 440 °F | |
CTC X-PRO TF 1040 GP Polypropylene Homopolymer, 40% Talc Filled X-PRO TF 1040 GP is a 40% talc reinforced polypropylene homopolymer and made of 98% recycled content. It has applications in: automotive, industrial, construction, consumer and lawn & garden produc.. |
|||
Middle Barrel Temperature | 216 - 227 °C | 420 - 440 °F | |
CTC X-PRO TF 1113 HP Polypropylene Homopolymer, 13% Talc Filled X-PRO TF 1113 HP is a 13% talc reinforced polypropylene homopolymer, heat stabilized, and made of 98% recycled content. It has applications in: automotive under hood, IP components, fan and lightin.. |
|||
Middle Barrel Temperature | 216 - 227 °C | 420 - 440 °F | |
CTC X-PRO TF 1140 HP Polypropylene Homopolymer, 40% Talc Filled X-PRO TF 1140 HP is a 40% talc reinforced polypropylene homopolymer, heat stabilized, and made of 98% recycled content. It has applications in: automotive under hood, IP components, HVAC, and lawn .. |
|||
Middle Barrel Temperature | 216 - 227 °C | 420 - 440 °F | |
Advanced Polymer Alloys DuraGrip™ 6150 BK Melt Processable Elastomer DuraGrip™ 6150BK is designed to be a special purpose Melt Processable Elastomer (MPE) that is easy to use in injection molding and extrusion processes. DGR 6150BK has an excellent
soft touch feel a.. |
|||
Middle Barrel Temperature | 216 - 241 °C | 421 - 466 °F | |
A. Schulman ComAlloy Hiloy® 272 Polystyrene Alloy, Glass Reinforced, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Middle Barrel Temperature | 216 - 260 °C | 420 - 500 °F | |
LTL Color Compounds ColorFast® FRPA100X Polycarbonate-ABS Alloy V-0 rated polycarbonate-ABS alloy, excellent toughness and light stabilityAll information provided by LTL Color Compounders, Inc. |
|||
Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
RheTech Products HP507-01 38% Talc Reinforced High Performance Polypropylene, Non-UV Stabilized, Black Applications: IP structural componentsSpeaker housingsAutomotive interior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |