| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Middle Barrel Temperature | 193 - 232 °C | 380 - 450 °F | |
|
Multibase Multi-Pro® 2514 XU Polypropylene
Mineral Filled, 25% by weight.Features:Heat Resistance, HighForms:PelletsProcessing Methods:Injection MoldingUses:AppliancesFurnitureTable ProductsInformation provided by Multibase
|
|||
| Middle Barrel Temperature | 199 - 232 °C | 390 - 450 °F | |
|
Multibase Multi-Pro® 3019 CXUW Polypropylene
Calcium Carbonate Filler, 30% by weight.Features:Gloss, High Impact Resistance, GoodUV Resistance, Good Forms:PelletsProcessing Methods:Injection MoldingUses:FurnitureLawn EquipmentInformation prov..
|
|||
| Middle Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
|
RheTech Products CC20P200-00 20% Calcium Carbonate Reinforced Polypropylene Copolymer, Natural
Applications: Electrical housingsDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
|
RheTech Products F52-01 20% Mica Reinforced Polypropylene Copolymer, Black
Applications: Functional support ductsHousingsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
|
RheTech Products FT4702-698UV Thermoplastic Polyolefin, UV Stabilized, RXF Jet Black
Applications: Bumper trimExterior componentsDoor claddingsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
|
RheTech Products FT4802-692UV Thermoplastic Polyolefin, UV Stabilized, RS8 Grey
Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
|
RheTech Products FT4802-693UV Thermoplastic Polyolefin, UV Stabilized, SPN Dark Teal
Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
|
RheTech Products G20P100-00 20% Glass Fiber Reinforced Polypropylene, Natural
Applications: Arm rest insertVacuum canisterStorage binConsolesBattery traysInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
|
RheTech Products GC20P255-01UV 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, UV Stabilized, Black
Applications: Durable goodsStructural componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
|
RheTech Products M20P100-01 20% Mica Reinforced Polypropylene, Black
Applications: Fan shroudsFiller panelsAir ductsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
|
RheTech Products RCT120-01 20% Talc Reinforced Polypropylene, Black, Recycled Content
Applications: HVAC and I/P ComponentsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
|
RheTech Products T12P600-430UVBG 12% Talc Reinforced Polypropylene Copolymer, UV Stabilized, Interior 848 Black, Blow Molding Grade
Applications: Flipper panelsSeat backsLoad floorInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
|
RheTech Products T20P100-517UV 20% Talc Reinforced Polypropylene, UV Stabilized, Interior DX9 Black
Applications: Center consolesIP componentsClose out panelsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 210 - 232 °C | 410 - 450 °F | |
|
Polymer Resources ABS-G30 ABS, 30% Glass Reinforced
Acrylonitrile Butadiene Styrene, 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information..
|
|||
| Middle Barrel Temperature | 210 - 232 °C | 410 - 450 °F | |
|
PlastiComp Complet® LCF50 - TPU Rigid Thermoplastic Polyurethane, 50% Long Carbon Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyurethane with 50% carbon fiber reinforcementInformation provided by PlastiComp, Inc.
|
|||
| Middle Barrel Temperature | 210 - 232 °C | 410 - 450 °F | |
|
PlastiComp Complet® LGF20 - TPU Rigid Thermoplastic Polyurethane, 20% Long Glass Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyurethane with 20% long glass fiber reinforcementInformation provided by PlastiComp, Inc..
|
|||
| Middle Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
|
RheTech Products HP531-01UV 22% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Black
Applications: IP structural componentsAir ducts - distributionA/B/ PillarsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
|
RheTech Products HP531-678UV 22% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Medium Scratch Resistant, IT3A Medium Light Stone
Applications: I/P componentsInterior trimA/B/C/ PillarsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
|
RheTech Products HP532-00 20% Talc Reinforced High Performance Polypropylene, Non-UV Stabilized, Natural
Applications: Interior trimCenter tail light bezelPackage trayInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
|
RheTech Products HP534-00 22% Talc Reinforced High Performance Polypropylene Copolymer, Natural
Applications: Door trim panelsCenter consolesSteering columnsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
|
RheTech Products M25P251-01 25% Mica Reinforced Polypropylene Copolymer, Black
Applications: Fan shroudsGlove box binFiller panelsClose-out panelsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 210 - 232 °C | 410 - 450 °F | |
|
Ineos Nova 240 High Performance Styrenic Enhanced Polystyrene
(discontinued **)
Extremely high impact with good flexural stiffness, Custom colorsApplications: Injection molding, Small appliances, Photographic equipmentPerformance grades of polystyrene are engineered to have spe..
|
|||
| Middle Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
|
Star Plastics ABS405 Extrusion Grade ABS
Information provided by Star Plastics, Inc.
|
|||
| Middle Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
|
Star Plastics ABSGF20 Molding Grade ABS With 20% Glass
Information provided by Star Plastics, Inc.
|
|||
| Middle Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
|
Star Plastics ABSHFL Molding Grade ABS High Flow
Information provided by Star Plastics, Inc.
|
|||
| Middle Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
|
Star Plastics ABSLG3030 Molding Grade ABS, Low Gloss
Information provided by Star Plastics, Inc.
|
|||
| Middle Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
|
Star Plastics ABS448T Molding Grade ABS
Information provided by Star Plastics, Inc.
|
|||
| Middle Barrel Temperature | 199 - 232 °C | 390 - 450 °F | |
|
Styrolution NAS® 36 UV Stabilized Acrylic Copolymer
Features:Sparkling clarity Excellent indoor light stability Styrenic processing advantages Scratch resistant Enhanced mold releaseApplications:Appliances Point-of -Purchase Displays Toys Office Acce..
|
|||
| Middle Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
|
RheTech Products G20P252-00 20% Glass Fiber Reinforced Polypropylene Copolymer, Natural
Applications: Interior trimArm rest insertConsolesDome light housingInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
|
RheTech Products GC20P600-01UV 20% Glass Fiber Reinforced Polypropylene, Chemically Coupled, UV Stabilized, Black
Applications: Sun roof trimFan shroudInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||