Category | Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Molded |
Manufacturer | Polymer Technology & Services, LLC (PTS) |
Trade Name | Trilac® |
Port | Ningbo port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | PTS Trilac® ABS-HF5500 High Flow ABS Resin.pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.05 g/cc | 0.0379 lb/in³ | ASTM D792 |
Melt Flow | 20 g/10 min @Load 10.0 kg, Temperature 220 °C |
20 g/10 min @Load 22.0 lb, Temperature 428 °F |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Rockwell R | 118 | 118 | ASTM D785 |
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
Flexural Yield Strength | 70.3 MPa | 10200 psi | ASTM D790 |
Flexural Modulus | 2.34 GPa | 339 ksi | ASTM D790 |
Izod Impact, Notched | 2.67 J/cm @Thickness 6.35 mm |
5.00 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
2.99 J/cm @Thickness 3.17 mm |
5.60 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C | 205 °F | ASTM D648 |
Deflection Temperature at 1.8 MPa (264 psi) | 87.0 °C | 189 °F | ASTM D648 |
Flammability, UL94 | HB @Thickness 1.50 - 2.90 mm |
HB @Thickness 0.0591 - 0.114 in |
Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 193 °C | 380 °F | |
Middle Barrel Temperature | 216 °C | 420 °F | |
Front Barrel Temperature | 232 °C | 450 °F | |
Melt Temperature | 218 - 260 °C | 425 - 500 °F | Nozzle temp not greater than stock |
Mold Temperature | 48.9 - 65.6 °C | 120 - 150 °F | |
Drying Temperature | 87.8 - 93.3 °C | 190 - 200 °F | |
Dry Time | 2 - 24 hour | 2 - 24 hour | |
Injection Pressure | 68.9 - 82.7 MPa | 10000 - 12000 psi | |
Back Pressure | 0.689 MPa | 100 psi | |
Screw Speed | 50 - 60 rpm | 50 - 60 rpm |
Descriptive Properties | Value | Comments |
---|---|---|
Injection Fill Speed | Slow to Moderate |