Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.70 - 2.20 GPa | 247 - 319 ksi | |
Prodways PLASTCure Model 100 3D Printing Polymer Allows production of precise components; high workability.Used for dental applications from models for restorations to orthodontics.Information provided by Genistar. |
|||
Flexural Modulus | 1.70 GPa | 247 ksi | Tangent; ASTM D 790 |
NOVA Chemicals Novapol® HE-W959-A HDPE Extrusion/Blow Molding Resin HE-W959-A complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food. It is also biolog.. |
|||
Flexural Modulus | 1.70 GPa | 247 ksi | STN EN ISO 178 |
Plastcom PLASTALEN® PH 52 T 20 Polypropylene reinforced with mineral filler PP homopolymer for injection molding with the content of 20 % mineral filler, heat stabilized. Application in automotive industry. Delivered in black grade.Information Provided by Plastcom spol. s r.. |
|||
Flexural Modulus | 1.70 GPa | 247 ksi | ASTM D790 |
Shell Carilon® DA6L1A10 Polyketone, Lubricated Injection Molding Grade
(discontinued **) Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer DA6L1A10 is a lubricated injection molding grade with mechanical properties which classify it as an.. |
|||
Flexural Modulus | 1.70 GPa | 247 ksi | 80x10x4 mm specimen, 2 mm/min; ISO 178 |
Solvay Engineered Polymers SEQUEL® 1733HI Engineered Polyolefin
(discontinued **) Description: SEQUEL® 1733HI engineered polyolefin is designed for large, painted automotive exterior applications that require dimensional stability over a broad temperature range. This material e.. |
|||
Flexural Modulus | 1.70 GPa @Temperature 23.0 °C |
247 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYfill PP HJ752 Polypropylene/Elastomer, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Modulus | 1.70 GPa | 247 ksi | ASTM D790A |
Ineos H00M-01 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Extrusion; ThermoformingFeatures: High melt strength, High stiffness, Medium-term heat agingComplies with FDA specification, Title 21, CFR 177.1520.Typical application.. |
|||
Flexural Modulus | 1.70 GPa | 247 ksi | 1.0 in/min; 0.125" thickness; ASTM D-790 |
Chevron Phillips K-Resin® KR01BR SBC
(discontinued **) K-Resin® Styrene-Butadiene Copolymer (SBC)Applications:Molded boxes with integral hingesMedical devicesDisplaysToysMedia packagingFeatures:Good stiffnessGood toughnessGood warpage resistanceExcelle.. |
|||
Flexural Modulus | 1.70 GPa | 247 ksi | ISO 178 |
Kuraray Genestarâ„¢ N1001D-U83/02 Nylon Standard unreinforced extrusion grade. Main Features:Outstanding fuel barrierHeat resistanceExample of applications:Multi-layered fuel tube |
|||
Flexural Modulus | 1.70 GPa | 247 ksi | ASTM D790 |
Ineos ABS Triax® 1220 S ABS + Polyamide Blend, Extrusion, Conditioned Properties tested in transverse direction (worst case) on 125-mil (3.2 mm) extruded sheets specimens with |
|||
Flexural Modulus | 1.70 GPa | 247 ksi | 1% Secant, 0.2 in/min; ASTM D790 |
LyondellBasell Hostacomâ„¢ BG722AC Polypropylene Copolymer Description: Hostacomâ„¢ BG722AC medium high melt flow, 1,700 MPa flexural modulus, precolored, mineral-filled polypropylene copolymer is designed with an excellent balance of stiffness, impact r.. |
|||
Flexural Modulus | 1.70 GPa | 247 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Noryl RF1132 PPE+PP PPE+PP blend for high frequency applications. Good heat resistance and low DK.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 1.70 GPa | 247 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics XYLEX X8300 PC+POLYESTER (Asia Pacific) PC+Polyester, UV Stabilized, Transparent |
|||
Flexural Modulus | 1.70 GPa | 247 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xylex X8300HP PC+POLYESTER (Europe-Africa-Middle East) Transparent, US Food Contact compliant, chemically resistant.
This grade will no longer be supported with biocompatibility information and should not be used for medical applications which require b.. |
|||
Flexural Modulus | 1.70 GPa | 247 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP V1000SU PA LNP* Thermotuf* V1000SU is a compound based on Nylon resin. Added features of this material include: Heat Stabilized, UV Stabilized. |
|||
Flexural Modulus | 1.70 GPa | 247 ksi | ISO 527-2 |
Total PPH 4022 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 4022 is a clarified nucleated homopolymer.ApplicationATOFINA Polypropylene PPH 4022 has been developed for extrusion-thermoforming, providing improved rigidity and impact r.. |
|||
Flexural Modulus | 1.70 GPa | 247 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 232H 10% Mineral Reinforced Ionomer / Nylon Alloy DescriptionFormion® FI 232H is an injection molding grade, 10% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, high stiffness and exceptional impact.. |
|||
Flexural Modulus | 1.70 GPa | 247 ksi | ISO 178 |
Total PPC 1645 Polypropylene, Heterophasic Copolymer, Pipes Polypropylene PPC 1645 is a nucleated heterophasic (block) copolymer with a Melt Flow index of 0.3 g/10 min. This resin has a long-term heat stabilization package. It offers a very high stiffness .. |
|||
Flexural Modulus | 1.70 GPa | 247 ksi | ASTM D 790 |
Cossa Polimeri ESTAPROP 1050 V0 HF K Flame Retardant Polypropylene PP copolymerFlame retardant class V0, halogen free, excellent mechanical characteristics, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Flexural Modulus | 1.70 GPa | 247 ksi | dry; ISO 178 |
DSM Novamid® ST120 NAT PA6-I Impact Modified, Injection Molding |
|||
Flexural Modulus | 1.70 GPa | 247 ksi | ISO 178 |
ExxonMobil Exxtral™ BMU 143 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance and designed for automotive interior application in which good surface finish, hig.. |
|||
Flexural Modulus | 1.70 GPa | 247 ksi | ASTM D790 |
Adell BI-30 Nylon 6, Impact Modified Data provided by Adell Plastics, Inc. |
|||
Flexural Modulus | 1.70 GPa | 247 ksi | ASTM D790 |
Ashley Polymers Ashlene® 527LDS Nylon 66 A very high impact, slightly lubricated and heat stabilized nylon resin.Data provided by the manufacturer |
|||
Flexural Modulus | 1.70 GPa | 247 ksi | ASTM D790 |
Ashley Polymers Ashlene® 527LDS-B2 Nylon 66 A high impact lubricated nylon resin containing well dispersed carbon black for maximum resistance to weathering.Data provided by the manufacturer |
|||
Flexural Modulus | 1.70 GPa | 247 ksi | ASTM D790 |
Ashley Polymers Ashlene® 527LDW Nylon 66 A specialized nylon with very high impact resistance.Data provided by the manufacturer |
|||
Flexural Modulus | 1.70 GPa | 247 ksi | ASTM D790 |
A. Schulman ComAlloy Comtuf® 607 Nylon 6/6, Impact Modified, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc.. |
|||
Flexural Modulus | 1.70 GPa | 247 ksi | ISO 178 |
Unitika ET2025 PA6, Dry High-impact nylonInformation provided by Unitika Ltd. |
|||
Flexural Modulus | 1.70 GPa | 247 ksi | ASTM D790 |
E-Polymers Tekaloy® T80FR , Flame Retardant Un-Reinforced PBT/ABS Alloy Flame RetardantInformation provided by E-Polymers Co. Ltd. |
|||
Flexural Modulus | 1.70 - 2.20 GPa @Temperature 60.0 - 120 °C |
247 - 319 ksi @Temperature 140 - 248 °F |
Average value: 1.88 GPa Grade Count:3 |
Overview of materials for Polycarbonate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Molded". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Flexural Modulus | 1.70 GPa | 247 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 232H 10% Mineral Reinforced Ionomer / Nylon Alloy DescriptionFormion® FI 232H is an injection molding grade, 10% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, high stiffness and exceptional impact.. |