| Category | Polymer , Thermoplastic , Nylon |
| Manufacturer | Kuraray Company |
| Trade Name | Genestar™ |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Kuraray Genestarâ„¢ N1001D-U83/02 Nylon.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.08 g/cc | 1.08 g/cc | |
| Density | 1.08 g/cc | 0.0390 lb/in³ | ISO 1183 |
| Water Absorption | 0.25 % | 0.25 % | ISO 62 |
| Linear Mold Shrinkage, Flow | 0.015 cm/cm | 0.015 in/in | ISO 294-4, 2577 |
| Linear Mold Shrinkage, Transverse | 0.017 cm/cm | 0.017 in/in | ISO 294-4, 2577 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 50.0 MPa | 7250 psi | ISO 527-1/-2 |
| Elongation at Break | 15 % | 15 % | ISO 527-1/-2 |
| Elongation at Yield | 7.0 % | 7.0 % | ISO 527-1/-2 |
| Tensile Modulus | 1.66 GPa | 241 ksi | ISO 527-1/-2 |
| Flexural Strength | 75.0 MPa | 10900 psi | ISO 178 |
| Flexural Modulus | 1.70 GPa | 247 ksi | ISO 178 |
| Charpy Impact, Notched | 1.90 J/cm² @Temperature -40.0 °C |
9.04 ft-lb/in² @Temperature -40.0 °F |
ISO 179/1eA |
| NB @Temperature 23.0 °C |
NB @Temperature 73.4 °F |
ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 264 °C | 507 °F | 10°C/min; ISO 11357-1/-3 |
| Deflection Temperature at 1.8 MPa (264 psi) | 110 °C | 230 °F | ISO 75-1/-2 |
| Glass Transition Temp, Tg | 125 °C | 257 °F | 10°C/min; ISO 11357-1/-2 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Applications | Automotive | |
| General Purpose | ||
| Chemical Resistance | Acid Resistance | |
| Alkali Resistance | ||
| Environmental Stress Crack Resistance | ||
| General Chemical Resistance | ||
| Grease Resistance | ||
| Hydrolytically Stable | ||
| Oil Resistance | ||
| Solvent Resistance | ||
| Delivery Form | Black | |
| Other Features | Barrier Properties | |
| Melt Strength | ||
| Thermal Stability | ||
| Weldable | ||
| Processing | Blow Molding | |
| Film Extrusion | ||
| Injection Molding | ||
| Pipe/Tube Extrusion | ||
| Thermoforming | ||
| Regional Availability | Asia Pacific | |
| Europe | ||
| Near East/Africa | ||
| North America | ||
| South and Central America | ||
| Special Characteristics | Heat Stabilized or Stable to Heat | |
| High Impact or Impact Modified |