Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Shell Carilon® DA6L1A10 Polyketone, Lubricated Injection Molding Grade  (discontinued **)

Category Polymer , Thermoplastic , Polyketone
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shell Carilon® DA6L1A10 Polyketone, Lubricated Injection Molding Grade  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer DA6L1A10 is a lubricated injection molding grade with mechanical properties which classify it as an engineering thermoplastic. Designed with demanding tribological applications in mind, such as gears, bearings etc., this cost efficient grade offers a high limiting pressure velocity ratio, low coefficient of friction and low wear. These benefits are achieved without sacrificing the toughness, moisture resistance and good fatigue performance which characterize the base polymer. CARILON Polymer DA6L1A10 can withstand short-term exposure to elevated temperatures. Moreover this polymer exhibits high resistance to hydrocarbons and other chemicals. CARILON Polymer DA6L1A10 is easy to process on standard injection molding equipment. Cycle times are generally short. Parts show good mold definition and little or no warpage. CARILON Polymers' low moisture sensitivity means that no conditioning of parts before assembly or use is necessary.Data provided by Shell Chemical.
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ASTM D792
Water Absorption 0.48 %
0.48 %
24 hour immersion; ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength, Yield 55.0 MPa
7980 psi
ASTM D638
Elongation at Break 23 %
23 %
ASTM D638
Tensile Modulus 1.70 GPa
247 ksi
ASTM D638
Flexural Modulus 1.70 GPa
247 ksi
ASTM D790
Izod Impact, Notched 2.30 J/cm
4.31 ft-lb/in
Izod Impact, Unnotched NB
NB
ASTM D256
Coefficient of Friction, Dynamic 0.14
0.14
Thrust washer testing against steel at 0.05 m/s (2 in/s) and 2 MPa
Limiting Pressure Velocity 1.60 MPa-m/sec
45700 psi-ft/min
at 0.5 m/s
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
Deflection Temperature at 0.46 MPa (66 psi) 204 °C
399 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 96.0 °C
205 °F
ASTM D648