| Category | Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Impact Grade |
| Manufacturer | Ashley Polymers |
| Trade Name | Ashlene® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Ashley Polymers Ashlene® 527LDW Nylon 66.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.07 g/cc | 0.0387 lb/in³ | ASTM D792 |
| Water Absorption | 1.3 % | 1.3 % | ASTM D570 |
| Linear Mold Shrinkage | 0.016 cm/cm | 0.016 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 113 | 113 | ASTM D785 |
| Tensile Strength, Yield | 51.0 MPa | 7400 psi | ASTM D638 |
| Elongation at Break | 55 % | 55 % | ASTM D638 |
| Flexural Modulus | 1.70 GPa | 247 ksi | ASTM D790 |
| Izod Impact, Notched | 10.13 J/cm | 18.98 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 254 °C | 489 °F | ASTM D3418 |
| Deflection Temperature at 0.46 MPa (66 psi) | 213 °C | 415 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 68.0 °C | 154 °F | ASTM D648 |
| Flammability, UL94 | HB | HB |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | ASTM D257 |
| Dielectric Constant | 2.9 <br>@Frequency 1000 Hz |
2.9 <br>@Frequency 1000 Hz |