| Category | Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Impact Grade |
| Manufacturer | Unitika |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Unitika ET2025 PA6, Dry.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.07 g/cc | 0.0387 lb/in³ | ISO 1183 |
| Moisture Absorption at Equilibrium | 1.7 % | 1.7 % | 50% RH; ISO 62 |
| Linear Mold Shrinkage, Flow | 0.022 cm/cm @Thickness 3.20 mm |
0.022 in/in @Thickness 0.126 in |
|
| Linear Mold Shrinkage, Transverse | 0.024 cm/cm @Thickness 3.20 mm |
0.024 in/in @Thickness 0.126 in |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 45.0 MPa | 6530 psi | ISO 527-1/-2 |
| Elongation at Break | 60 % | 60 % | ISO 527-1/-2 |
| Tensile Modulus | 1.80 GPa | 261 ksi | ISO 527-1/-2 |
| Flexural Strength | 55.0 MPa | 7980 psi | ISO 178 |
| Flexural Modulus | 1.70 GPa | 247 ksi | ISO 178 |
| Charpy Impact Unnotched | NB | NB | ISO 179-1 |
| Charpy Impact, Notched | 8.00 J/cm² | 38.1 ft-lb/in² | ISO 179-1 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 100 µm/m-°C | 55.6 µin/in-°F | ISO 11359-2 |
| Deflection Temperature at 0.46 MPa (66 psi) | 161 °C | 322 °F | ISO 75-1/-2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 62.0 °C | 144 °F | ISO 75-1/-2 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+13 ohm-cm | 1.00e+13 ohm-cm | IEC 60093 |
| Dielectric Strength | 31.0 kV/mm @Thickness 1.00 mm |
787 kV/in @Thickness 0.0394 in |
IEC 60243-1 |