| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.48 g/cc | 1.48 g/cc | ASTM D792 |
| Density | 1.47 g/cc | 0.0531 lb/in³ | ASTM D792 |
| Moisture Absorption | 0.140 % | 0.140 % | 50% RH, 24 hrs; ASTM D570 |
| 0.220 % | 0.220 % | 23°C / 50% RH; ISO 62 | |
| Linear Mold Shrinkage, Flow | 0.0010 - 0.0030 cm/cm @Time 86400 sec |
0.0010 - 0.0030 in/in @Time 24.0 hour |
ASTM D955 |
| Linear Mold Shrinkage, Transverse | 0.0030 - 0.0050 cm/cm @Time 86400 sec |
0.0030 - 0.0050 in/in @Time 24.0 hour |
ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 179 MPa | 26000 psi | 5 mm/min; ISO 527 |
| 183 MPa | 26500 psi | Type I, 5 mm/min; ASTM D638 | |
| Tensile Strength, Yield | 179 MPa | 26000 psi | 5 mm/min; ISO 527 |
| 191 MPa | 27700 psi | Type I, 5 mm/min; ASTM D638 | |
| Elongation at Break | 1.5 % | 1.5 % | 5 mm/min; ISO 527 |
| 1.7 % | 1.7 % | Type I, 5 mm/min; ASTM D638 | |
| Elongation at Yield | 1.5 % | 1.5 % | 5 mm/min; ISO 527 |
| 1.7 % | 1.7 % | Type I, 5 mm/min; ASTM D638 | |
| Tensile Modulus | 13.99 GPa | 2029 ksi | 1 mm/min; ISO 527 |
| 14.82 GPa | 2149 ksi | 5 mm/min; ASTM D638 | |
| Flexural Strength | 248 MPa | 36000 psi | ASTM D790 |
| 264 MPa | 38300 psi | 1.3 mm/min, 50 mm span; ASTM D790 | |
| Flexural Yield Strength | 264 MPa | 38300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
| Flexural Modulus | 13.33 GPa | 1933 ksi | 2 mm/min; ISO 178 |
| 13.8 GPa | 2000 ksi | 1.3 mm/min, 50 mm span; ASTM D790 | |
| Izod Impact, Notched | 0.660 J/cm | 1.24 ft-lb/in | ASTM D256 |
| Izod Impact, Unnotched | 13.2 J/cm | 24.7 ft-lb/in | ASTM D4812 |
| Izod Impact, Notched (ISO) | 7.00 kJ/m² | 3.33 ft-lb/in² | 80*10*4; ISO 180/1A |
| Izod Impact, Unnotched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | 80*10*4; ISO 180/1U |
| Dart Drop, Total Energy | 11.0 J @Temperature 23.0 °C |
8.11 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
| Impact Test | 3.00 J | 2.21 ft-lb | Multiaxial Impact; ISO 6603 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 38.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
21.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
| CTE, linear, Transverse to Flow | 33.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
18.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
| Deflection Temperature at 0.46 MPa (66 psi) | 214 °C | 417 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
| 213 °C @Thickness 3.20 mm |
415 °F @Thickness 0.126 in |
unannealed; ASTM D648 | |
| Deflection Temperature at 1.8 MPa (264 psi) | 210 °C | 410 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
| 209 °C @Thickness 3.20 mm |
408 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistance | 1000 - 1.00e+6 ohm | 1000 - 1.00e+6 ohm | ASTM D257 |