Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 25.0 kJ/m²
11.9 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP DCL33E PC (Europe-Africa-Middle East)
LNP* LUBRICOMP* DCL33E is a compound based on Polycarbonate resin containing Carbon Fiber, PTFE. Added features include; Internally Lubricated, Electrically Conductive, Easy Molding.
Izod Impact, Unnotched (ISO) 25.0 - 50.0 kJ/m²

@Temperature -30.0 - -30.0 °C
11.9 - 23.8 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 41.0 kJ/m² Grade Count:8
Overview of materials for PBT + ASA Blend, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PBT + ASA Blend, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum ..
Izod Impact, Unnotched (ISO) 25.0 kJ/m²
11.9 ft-lb/in²
ISO 180A
Chevron Phillips Xtel® XK2760BL Polyphenylene Sulfide Alloy  (discontinued **)
Xtel® XK2760BL is a high performance, glass fiber and mineral filled PPS based alloy developed to provide excellent mechanical strength with a unique blend of toughness, rigidity, and low flash cha..
Izod Impact, Unnotched (ISO) 25.0 - 90.0 kJ/m²

@Temperature -30.0 - -30.0 °C
11.9 - 42.8 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 62.5 kJ/m² Grade Count:12
Overview of materials for Nylon 66, Heat Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Heat Stabilized". Each property range of values reported is minimum and maximum values of appr..
Izod Impact, Unnotched (ISO) 25.0 kJ/m²
11.9 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics NORYL SE1GFN1 PPE+HIPS (Europe-Africa-Middle East)
Noryl* SE1GFN1 is a 10% glass reinforced, injection moldable modified polyphenylene ether resin. Designed for improved dimensional stability and good flow , this resin also uses non-chlorinated, non..
Izod Impact, Unnotched (ISO) 25.0 kJ/m²

@Temperature -30.0 °C
11.9 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics NORYL SE1GFN2 PPE+HIPS (Europe-Africa-Middle East)
Noryl* SE1GFN2 is a 20% glass reinforced, injection moldable modified polyphenylene ether resin. Designed for improved dimensional stability and good flow , this resin also uses non-chlorinated, non..
Izod Impact, Unnotched (ISO) 25.0 kJ/m²
11.9 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics NORYL SE1GFN3 PPE+HIPS (Europe-Africa-Middle East)
Noryl* SE1GFN3 is a 30% glass reinforced, injection moldable modified polyphenylene ether resin. Designed for improved dimensional stability and good flow , this resin also uses non-chlorinated, non..
Izod Impact, Unnotched (ISO) 25.0 kJ/m²

@Temperature -30.0 °C
11.9 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics NORYL V02570 PPE+HIPS (Asia Pacific)
Noryl* V02570 is a 25% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t..
Izod Impact, Unnotched (ISO) 25.0 kJ/m²
11.9 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP RL0019 PA 66
LNP LUBRICOMP* RL0019 is a compound based on Nylon 66 resin containing 5% PTFE. Added features of this material include: Flame Retardant, Wear Resistant.
Izod Impact, Unnotched (ISO) 25.0 kJ/m²
11.9 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP UX05051 PPA (Europe-Africa-Middle East)
Internally lubricated Polyphthalamide compound, containing Glass Fiber and PTFE. Added features include Heat Stabilized, Flame Retardant and Hot Water Moldable
Izod Impact, Unnotched (ISO) 25.0 kJ/m²

@Temperature -30.0 °C
11.9 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics ULTEM 2312EPR PEI
30% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.
Izod Impact, Unnotched (ISO) 25.0 kJ/m²
11.9 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP WL004 PBT (Europe-Africa-Middle East)
LNP* Lubricomp* WL004 is a compound based on Polybutylene Terephalate resin containing PTFE.
Izod Impact, Unnotched (ISO) 25.0 kJ/m²

@Temperature -30.0 °C
11.9 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics Valox® 815 PBT (Europe-Africa-Middle East)
VALOX 815 is a 15% glass reinforced PBT+PET blend with excellent surface finish. Applications: hot air gun housings assemblies, industrial glue guns, appliance housings and handles.
Izod Impact, Unnotched (ISO) 25.0 kJ/m²

@Temperature 23.0 °C
11.9 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Stat-kon OCL13 PPS - LINEAR (Europe-Africa-Middle East)
LNP* Stat-kon* OCL13 is a compound based on PPS - LINEAR resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for..
Izod Impact, Unnotched (ISO) 25.0 kJ/m²
11.9 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP KB006 Acetal
LNP* THERMOCOMP* KB006 is a compound based on Acetal containing 30% Glass Bead.
Izod Impact, Unnotched (ISO) 25.0 kJ/m²

@Temperature 23.0 °C
11.9 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Thermocomp MX96070 PP (Europe-Africa-Middle East)
LNP* STARFLAM* MX96070 is a compound based on Polypropylene resin containing Flame Retardant. Added features include: Flame Retardant.This data was supplied by SABIC-IP for the Europe-Africa-Middl..
Izod Impact, Unnotched (ISO) 25.0 kJ/m²

@Temperature 23.0 °C
11.9 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Thermocomp WC003 PBT (Europe-Africa-Middle East)
LNP* Thermocomp* WC003 is a compound based on Polybutylene Terephalate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABI..
Izod Impact, Unnotched (ISO) 25.0 kJ/m²

@Temperature -30.0 °C
11.9 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics NORYL GFN1720 PPE+HIPS (Europe-Africa-Middle East)
Noryl* GFN1720 is a 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Noryl ..
Izod Impact, Unnotched (ISO) 25.0 kJ/m²

@Temperature -30.0 °C
11.9 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics NORYL NH7112 PPE+HIPS
Noryl* NH7112 resin is a 10% glass reinforced, modified PPE-PS blend. The material offers an exceptional balance of strength and dimensional stability while using non-halogenated flame retardants to..
Izod Impact, Unnotched (ISO) 25.0 kJ/m²

@Temperature -30.0 °C
11.9 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics NORYL NH7112 PPE+HIPS (Asia Pacific)
Noryl* NH7112 resin is a 10% glass reinforced, modified PPE-PS blend. The material offers an exceptional balance of strength and dimensional stability while using non-halogenated flame retardants to..
Izod Impact, Unnotched (ISO) 25.0 kJ/m²
11.9 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics Valox® SHF4930 PBT
Super high flow FR PBT grade with 15% Glass reinforced
Izod Impact, Unnotched (ISO) 25.0 kJ/m²
11.9 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics Valox® SHF4930 PBT (Europe-Africa-Middle East)
Super high flow FR PBT grade with 15% Glass reinforced
Izod Impact, Unnotched (ISO) 25.0 kJ/m²
11.9 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP MC002 PP
LNP* THERMOCOMP* MC002 is a compound based on Polypropylene resin containing 10% Carbon Fiber. Added feature of this material is: Electrically Conductive.
Izod Impact, Unnotched (ISO) 25.0 kJ/m²

@Temperature 23.0 °C
11.9 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Thermocomp RB004 PA 66 (Europe-Africa-Middle East)
LNP* THERMOCOMP* RB004 is a compound based on PA 66 resin containing Glass Beads.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Izod Impact, Unnotched (ISO) 25.0 kJ/m²
11.9 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics NORYL GFN1720 PPE+HIPS (Asia Pacific)
Noryl* GFN1720 is a 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Noryl ..
Izod Impact, Unnotched (ISO) 25.0 kJ/m²

@Temperature -30.0 °C
11.9 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics NORYL GFN3V PPE+HIPS (Europe-Africa-Middle East)
NORYL GFN3V is a 30 % glass fibre reinforced material with a HDT/A of 145C according ISO 75. NORYL GFN3V has been approved for potable water applications up to 85C by the UK WFBS according BS 6920 i..
Izod Impact, Unnotched (ISO) 25.0 kJ/m²
11.9 ft-lb/in²
80x10x4; ISO 180/1U
Eurostar Starflam PK0022E PA6, 10% Mineral Filled, Injection Molded
PK0022E is a Halogen Free and Phosphorous Free, Mineral Filed, Polyamide 6 Injection Molding (also known as PM3620Z22 or PA 10E6 U9 Z22)Information provided by Polymer Technology & Services, the Nor..
Izod Impact, Unnotched (ISO) 25.0 - 45.0 kJ/m²

@Temperature -40.0 - -30.0 °C
11.9 - 21.4 ft-lb/in²

@Temperature -40.0 - -22.0 °F
Average value: 34.4 kJ/m² Grade Count:8
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% ..
Izod Impact, Unnotched (ISO) 25.0 kJ/m²
11.9 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP GFL36 PSU (Europe-Africa-Middle East)
LNP* Lubricomp* GFL36 is a compound based on Polysulfone resin containing Glass Fiber, PTFE. Added features include: Internally Lubricated.
Izod Impact, Unnotched (ISO) 25.0 kJ/m²
11.9 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics NORYL PX1786G PPE+HIPS (Europe-Africa-Middle East)
NORYL PX1786G is a 30 % glass filled material with a Vicat B/120 of 160 °C.
Copyright © lookpolymers.com All Rights Reserved