| Category | Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS) |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | Noryl |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | SABIC Innovative Plastics NORYL GFN1720 PPE+HIPS (Asia Pacific).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.24 g/cc | 1.24 g/cc | ASTM D792 |
| Density | 1.24 g/cc | 0.0448 lb/in³ | ISO 1183 |
| Moisture Absorption | 0.0600 % | 0.0600 % | 23°C / 50% RH; ISO 62 |
| Water Absorption at Saturation | 0.15 % | 0.15 % | ISO 62 |
| Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm | 0.0020 - 0.0040 in/in | on Tensile Bar; SABIC Method |
| 0.0020 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0040 in/in @Thickness 0.126 in |
SABIC Method | |
| Melt Flow | 4.5 g/10 min @Load 5.00 kg, Temperature 300 °C |
4.5 g/10 min @Load 11.0 lb, Temperature 572 °F |
ASTM D1238 |
| Melt Index of Compound | 11 g/10 min @Load 10.0 kg, Temperature 300 °C |
11 g/10 min @Load 22.0 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, H358/30 | 100 MPa | 14500 psi | ISO 2039-1 |
| Tensile Strength at Break | 90.0 MPa | 13100 psi | 5 mm/min; ISO 527 |
| 90.0 MPa | 13100 psi | Type I, 5 mm/min; ASTM D638 | |
| Tensile Strength, Yield | 90.0 MPa | 13100 psi | Type I, 5 mm/min; ASTM D638 |
| 90.0 MPa | 13100 psi | 5 mm/min; ISO 527 | |
| Elongation at Break | 2.0 % | 2.0 % | 5 mm/min; ISO 527 |
| 3.0 % | 3.0 % | Type I, 5 mm/min; ASTM D638 | |
| Elongation at Yield | 2.0 % | 2.0 % | 5 mm/min; ISO 527 |
| 2.5 % | 2.5 % | Type I, 5 mm/min; ASTM D638 | |
| Tensile Modulus | 5.50 GPa | 798 ksi | 5 mm/min; ASTM D638 |
| 6.00 GPa | 870 ksi | 1 mm/min; ISO 527 | |
| Flexural Strength | 135 MPa | 19600 psi | 2 mm/min; ISO 178 |
| Flexural Yield Strength | 145 MPa | 21000 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
| Flexural Modulus | 4.50 GPa | 653 ksi | 2 mm/min; ISO 178 |
| 4.80 GPa | 696 ksi | 1.3 mm/min, 50 mm span; ASTM D790 | |
| Izod Impact, Notched | 0.600 J/cm | 1.12 ft-lb/in | ASTM D256 |
| 0.500 J/cm @Temperature -30.0 °C |
0.937 ft-lb/in @Temperature -22.0 °F |
ASTM D256 | |
| Izod Impact, Unnotched (ISO) | 25.0 kJ/m² | 11.9 ft-lb/in² | 80*10*4; ISO 180/1U |
| 25.0 kJ/m² @Temperature -30.0 °C |
11.9 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U | |
| Charpy Impact Unnotched | 2.50 J/cm² | 11.9 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eU |
| 2.50 J/cm² @Temperature -30.0 °C |
11.9 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU | |
| Dart Drop, Total Energy | 14.0 J @Temperature 23.0 °C |
10.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
| Taber Abrasion, mg/1000 Cycles | 45 | 45 | CS-17, 1 kg; SABIC Method |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 30.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
16.7 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
| 40.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
22.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 | |
| CTE, linear, Transverse to Flow | 50.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
27.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
| 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 | |
| Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | ISO 8302 |
| Hot Ball Pressure Test | <= 165 °C | <= 329 °F | IEC 60695-10-2 |
| Deflection Temperature at 0.46 MPa (66 psi) | 170 °C | 338 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
| Deflection Temperature at 1.8 MPa (264 psi) | 160 °C | 320 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
| 171 °C @Thickness 3.20 mm |
340 °F @Thickness 0.126 in |
unannealed; ASTM D648 | |
| Vicat Softening Point | 170 °C | 338 °F | Rate B/50; ISO 306 |
| 180 °C | 356 °F | Rate B/120; ISO 306 | |
| 180 °C | 356 °F | Rate A/50; ISO 306 | |
| 181 °C | 358 °F | Rate B/50; ASTM D1525 | |
| UL RTI, Electrical | 65.0 °C | 149 °F | UL 746B |
| UL RTI, Mechanical with Impact | 65.0 °C | 149 °F | UL 746B |
| UL RTI, Mechanical without Impact | 65.0 °C | 149 °F | UL 746B |
| Flammability, UL94 | HB @Thickness 1.50 mm |
HB @Thickness 0.0591 in |
UL 94 |
| HB @Thickness 3.00 mm |
HB @Thickness 0.118 in |
UL 94 | |
| Oxygen Index | 23 % | 23 % | ISO 4589 |
| Glow Wire Test | 960 °C @Thickness 3.20 mm |
1760 °F @Thickness 0.126 in |
IEC 60695-2-12 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | IEC 60093 |
| Surface Resistance | >= 1.00e+15 ohm | >= 1.00e+15 ohm | ROA; IEC 60093 |
| Dielectric Constant | 2.6 @Frequency 1.00e+6 Hz |
2.6 @Frequency 1.00e+6 Hz |
IEC 60250 |
| 2.7 @Frequency 50.0 - 60.0 Hz |
2.7 @Frequency 50.0 - 60.0 Hz |
IEC 60250 | |
| Dielectric Strength | 16.0 kV/mm @Thickness 3.20 mm |
406 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
| 26.0 kV/mm @Thickness 1.60 mm |
660 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 | |
| 30.0 kV/mm @Thickness 0.800 mm |
762 kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 | |
| Dissipation Factor | 0.0020 @Frequency 1.00e+6 Hz |
0.0020 @Frequency 1.00e+6 Hz |
IEC 60250 |
| 0.0060 @Frequency 50.0 - 60.0 Hz |
0.0060 @Frequency 50.0 - 60.0 Hz |
IEC 60250 | |
| Comparative Tracking Index | 200 V | 200 V | IEC 60112 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Ball Pressure Test, 125°C +/- 2°C | PASSES | IEC 60695-10-2 |