Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 3.60 J/cm² @Temperature -30.0 °C |
17.1 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Nilit Nilamid A H2 FR HF2 Unfilled, Flame Retardant PA66/6 Co-Polymer Description: Nilamid A H2 FR HF2 is an unfilled, flame retardant NYLON 66/6 co-polymer that does not contain halogen or red phosphorous. This product combines excellent flow characteristics and extr.. |
|||
Charpy Impact Unnotched | 3.60 J/cm² | 17.1 ft-lb/in² | ISO 179/1eU |
Nilit FRIANYL A63 CV-CM 0515 9005/Z Powder-coatable nylon 6.6 for injection molding, 15% ceramic filled Powder-coatable nylon 6.6 for injection molding, with conductive carbon blackInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 3.60 J/cm² @Temperature -40.0 °C |
17.1 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
Nilit FRIANYL A63 H-GV30 Nylon 6.6 for injection molding, 30% glass fiber reinforced Nylon 6.6 for injection molding, heat stabilized (dark natural color).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 3.60 J/cm² @Temperature -40.0 °C |
17.1 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
Nilit FRIANYL A63 HH-GV30 Nylon 6.6 for injection molding, 30% glass fiber reinforced Nylon 6.6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 3.60 J/cm² @Temperature -40.0 °C |
17.1 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
Nilit FRIANYL A63 HS-GV20 Nylon 6.6 for injection molding, 20% glass fiber reinforced Nylon 6.6 for injection molding, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 3.60 J/cm² | 17.1 ft-lb/in² | DIN 53453 |
Nilit RECONYL B KV30 Recycled nylon 6 for injection molding, 30% glass ball reinforced Recycled nylon 6 for injection molding (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 3.60 J/cm² | 17.1 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1850-7315 PBT, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Charpy Impact Unnotched | 3.60 J/cm² | 17.1 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 19-7221/OR Polyamide 46, with glass fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Highly dimensionally stable at elevated temperatures.Gear parts for automot.. |
|||
Charpy Impact Unnotched | 3.60 J/cm² | 17.1 ft-lb/in² | |
Ineos ABS Triax® 1315 GF ABS + Polyamide Blend (Conditioned) Key Features:Contains FillerSuitable processing methods:Injection molding |
|||
Charpy Impact Unnotched | 3.60 J/cm² @Temperature -30.0 °C |
17.1 ft-lb/in² @Temperature -22.0 °F |
|
Ineos ABS Triax® 1315 GF ABS + Polyamide Blend (Conditioned) Key Features:Contains FillerSuitable processing methods:Injection molding |
|||
Charpy Impact Unnotched | 3.60 J/cm² @Temperature -30.0 °C |
17.1 ft-lb/in² @Temperature -22.0 °F |
|
Ineos ABS Triax® 1315 GF ABS + Polyamide Blend (DAM) Key Features:Contains FillerSuitable processing methods:Injection molding |
|||
Charpy Impact Unnotched | 3.60 J/cm² @Temperature -30.0 °C |
17.1 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Lehmann & Voss LUVOCOM® 50/CF/5/GF/10 Polycarbonate, with carbon fiber and glass fiber Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Charpy Impact Unnotched | 3.60 J/cm² | 17.1 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 80-7919 Polyacetal-copolymer, with PTFE, easy flowing Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Charpy Impact Unnotched | 3.60 J/cm² | 17.1 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss Nylatron® MR 2007 Polyamide 6, with mineral filler Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Low warpage.Isotropic shrinkage characteristics.Information provided by Lehmann & Voss & Co.KG |
|||
Charpy Impact Unnotched | 3.60 J/cm² @Temperature -30.0 °C |
17.1 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics NORYL ZX09022 PPE+PP (Europe-Africa-Middle East) Thermocomp ZX09022 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile mod.. |
|||
Charpy Impact Unnotched | 3.60 J/cm² | 17.1 ft-lb/in² | ISO 179 |
Solvay Specialty Polymers Ixef® 3008 Polyarylamide (PARA), 30% Carbon Fiber Ixef® 3008 is a 30% carbon-fiber reinforced polyarylamide compound which exhibits extremely high strength and stiffness, good surface gloss, excellent creep resistance, and lower density than gla.. |
|||
Charpy Impact Unnotched | 3.60 J/cm² | 17.1 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics Valox® ENH4550 PBT 25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin. |
|||
Charpy Impact Unnotched | 3.60 J/cm² | 17.1 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics LNP THERMOCOMP EXTC8143 PC (Asia Pacific) LNP* Thermocomp* EXTC8143 is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus, good flatness, good ductility, No.. |
|||
Charpy Impact Unnotched | 3.60 J/cm² @Temperature -30.0 °C |
17.1 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics LNP THERMOCOMP ZX09022 PPE+PP (Europe-Africa-Middle East) Thermocomp ZX09022 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile mod.. |
|||
Charpy Impact Unnotched | 3.60 J/cm² @Temperature -30.0 °C |
17.1 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics NORYL PPX PPX830 PPE+PP Noryl* PPX830 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile modulus .. |
|||
Charpy Impact Unnotched | 3.60 J/cm² @Temperature -30.0 °C |
17.1 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics NORYL PPX PPX830 PPE+PP (Europe-Africa-Middle East) Noryl* PPX830 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile modulus .. |
|||
Charpy Impact Unnotched | 3.60 J/cm² @Temperature -30.0 °C |
17.1 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics NORYL PPX ZX09022 PPE+PP (Europe-Africa-Middle East) Thermocomp ZX09022 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile mod.. |
|||
Charpy Impact Unnotched | 3.60 J/cm² | 17.1 ft-lb/in² | 50%RH; ISO 179/1eU |
DuPont Performance Polymers Zytel® HTN FR52G45BL BK337 Polyphthalamide (PPA)
(Unverified Data**) 45% Glass Reinforced Flame Retardant PPA High Performance Polyamide Zytel HTNFR52G45BL BK337 is a 45% glass reinforced flame retardant lubricated high performance polyamide resin that has been devel.. |
|||
Charpy Impact Unnotched | 3.60 J/cm² @Temperature -30.0 °C |
17.1 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 179/1eU |
DuPont Performance Polymers Zytel® HTN FR52G45BL BK337 Polyphthalamide (PPA)
(Unverified Data**) 45% Glass Reinforced Flame Retardant PPA High Performance Polyamide Zytel HTNFR52G45BL BK337 is a 45% glass reinforced flame retardant lubricated high performance polyamide resin that has been devel.. |
|||
Charpy Impact Unnotched | 3.60 J/cm² @Temperature -30.0 °C |
17.1 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eU |
DuPont Performance Polymers Zytel® PLS FR95G15DH2 BK269 Nylon 6 15% Glass Reinforced Flame Retardant Heat Stabilized Polyamide Zytel PLSFR95G15DH2 BK269 is 15% glass reinforced flame retardant black PA using SHIELD Technology only from DuPont exceptional resista.. |
|||
Charpy Impact Unnotched | 3.60 J/cm² | 17.1 ft-lb/in² | ISO 179/IeU |
Addiplast Addilene H 211 V20 Polypropylene Homopolymer Glass fiber reinforced, high modulus and improved stiffnessInformation provided by Addiplast. |
|||
Charpy Impact Unnotched | 3.60 J/cm² | 17.1 ft-lb/in² | ISO 179/IeU |
Addiplast Addinyl B2 K20 Nylon 6 High density and high modulusInformation provided by Addiplast. |
|||
Charpy Impact Unnotched | 3.60 J/cm² | 17.1 ft-lb/in² | ISO 179 |
BASF Ultradur B 4406 G4 Q113 20% Glass Filled PBT Ultradur B4406 G4 Q113 is an UL V0 injection molding PBT grade with 20% glass fiber reinforcement. |
|||
Charpy Impact Unnotched | 3.60 J/cm² | 17.1 ft-lb/in² | |
LATI Latilub 88/50-20GRT K/10 PEEK, 10% Carbon Fiber Reinforced, Graphite/PTFE Filled Self-lubricating product based on Polyetheretherketone (PEEK). Graphite / PTFE. Carbon fiber. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provid.. |