SABIC Innovative Plastics NORYL PPX ZX09022 PPE+PP (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polypropylene (PP)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl PPX
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL PPX ZX09022 PPE+PP (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Thermocomp ZX09022 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile modulus of 7600 MPa; this grade has been developed for application where dimension stability, temperature and chemical resistance could be required.Thermocomp ZX09022 is an opaque material available in limited colors only.
Physical Properties Metric English Comments
Specific Gravity 1.19 g/cc
1.19 g/cc
ASTM D792
Density 1.19 g/cc
0.0430 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0020 - 0.0025 cm/cm

@Thickness 3.20 mm
0.0020 - 0.0025 in/in

@Thickness 0.126 in
SABIC Method
Linear Mold Shrinkage, Transverse 0.0040 - 0.0060 cm/cm

@Thickness 3.20 mm
0.0040 - 0.0060 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 6.0 g/10 min

@Load 5.00 kg,
Temperature 280 °C
6.0 g/10 min

@Load 11.0 lb,
Temperature 536 °F
ASTM D1238
Melt Index of Compound 6.0 g/10 min

@Load 5.00 kg,
Temperature 280 °C
6.0 g/10 min

@Load 11.0 lb,
Temperature 536 °F
MVR [cm^3/10 min]; ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 98.0 MPa
14200 psi
5 mm/min; ISO 527
101 MPa
14600 psi
Type I, 5 mm/min; ASTM D638
Tensile Strength, Yield 98.0 MPa
14200 psi
5 mm/min; ISO 527
101 MPa
14600 psi
Type I, 5 mm/min; ASTM D638
Elongation at Break 3.2 %
3.2 %
5 mm/min; ISO 527
101 %
101 %
Type I, 5 mm/min; ASTM D638
Elongation at Yield 2.9 %
2.9 %
Type I, 5 mm/min; ASTM D638
3.2 %
3.2 %
5 mm/min; ISO 527
Tensile Modulus 7.60 GPa
1100 ksi
5 mm/min; ASTM D638
7.70 GPa
1120 ksi
1 mm/min; ISO 527
Flexural Yield Strength 141 MPa
20500 psi
2 mm/min; ISO 178
144 MPa
20900 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 6.60 GPa
957 ksi
1.3 mm/min, 50 mm span; ASTM D790
7.10 GPa
1030 ksi
2 mm/min; ISO 178
Izod Impact, Notched 0.950 J/cm
1.78 ft-lb/in
ASTM D256
Izod Impact, Unnotched 6.50 J/cm
12.2 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 10.0 kJ/m²
4.76 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 42.0 kJ/m²
20.0 ft-lb/in²
80*10*4; ISO 180/1U
42.0 kJ/m²

@Temperature -30.0 °C
20.0 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
Charpy Impact Unnotched 3.90 J/cm²
18.6 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eU
3.60 J/cm²

@Temperature -30.0 °C
17.1 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Dart Drop, Total Energy 10.0 J

@Temperature -30.0 °C
7.38 ft-lb

@Temperature -22.0 °F
ASTM D3763
15.0 J

@Temperature 23.0 °C
11.1 ft-lb

@Temperature 73.4 °F
ASTM D3763
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 25.0 µm/m-°C

@Temperature -40.0 - 95.0 °C
13.9 µin/in-°F

@Temperature -40.0 - 203 °F
ASTM E 831
25.0 µm/m-°C

@Temperature -30.0 - 80.0 °C
13.9 µin/in-°F

@Temperature -22.0 - 176 °F
ISO 11359-2
CTE, linear, Transverse to Flow 120 µm/m-°C

@Temperature -30.0 - 80.0 °C
66.7 µin/in-°F

@Temperature -22.0 - 176 °F
ISO 11359-2
130 µm/m-°C

@Temperature -40.0 - 95.0 °C
72.2 µin/in-°F

@Temperature -40.0 - 203 °F
ASTM E 831
Deflection Temperature at 0.46 MPa (66 psi) 168 °C
334 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
166 °C

@Thickness 3.20 mm
331 °F

@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 153 °C
307 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
156 °C

@Thickness 3.20 mm
313 °F

@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 150 °C
302 °F
Rate B/120; ISO 306
Flammability, UL94 HB

@Thickness 1.00 mm
HB

@Thickness 0.0394 in
UL 94
Glow Wire Test 650 °C

@Thickness 3.00 mm
1200 °F

@Thickness 0.118 in
IEC 60695-2-12
Descriptive Properties Value Comments
Ball Pressure Test, 125°C +/- 2°C Passes
IEC 60695-10-2