Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 130 MPa | 18900 psi | ISO 2039-1 |
Nilit FRIANYL A63 CU90 Nylon 6.6 for injection molding, 90% copper filled Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 130 MPa | 18900 psi | ISO 2039-1 |
Nilit FRIANYL A63 TF10 Nylon 6.6 for injection molding, 10% PTFE lubricated Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 130 MPa | 18900 psi | ISO 2039-1 |
Nilit FRIANYL B63 K Nylon 6 for injection molding Nylon 6 for injection molding, specially formulated for knobs.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 130 MPa | 18900 psi | ISO 2039-1 |
Nilit FRIANYL B63 KLZ Nylon 6 for injection molding Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 130 MPa | 18900 psi | ISO 2039-1 |
Nilit RECONYL B Recycled nylon 6 for injection molding Recycled nylon 6 for injection molding (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 130 MPa | 18900 psi | ISO 2039-1 |
Nilit FRIANYL B63 D Nylon 6., std. viscosity for injection molding Nylon 6., std. viscosity for injection molding, permanently flexible, developed for dowels.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 130 MPa | 18900 psi | ISO 2039-1 |
Nilit FRIANYL B63 HS-GV30 Nylon 6 for injection molding, 30% glass fiber reinforced Nylon 6 for injection molding, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 130 MPa | 18900 psi | ISO 2039-1 |
Nilit FRIANYL B63 HS-KV20 Nylon 6 for injection molding, 20% glass ball reinforced Nylon 6 for injection molding, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 130 MPa | 18900 psi | ISO 2039-1 |
Nilit FRIANYL B63 M2 Nylon 6 for injection molding, 2% molybdenum disulphide lubricated Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 130 MPa | 18900 psi | ISO 2039-1 |
Nilit RECONYL B F Recycled nylon 6 for injection molding Recycled nylon 6 for injection molding, highly crystallized (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 130 - 310 MPa | 18900 - 45000 psi | Average value: 254 MPa Grade Count:23 |
Overview of materials for Nylon 66, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. .. |
|||
Ball Indentation Hardness | 130 - 310 MPa | 18900 - 45000 psi | Average value: 195 MPa Grade Count:8 |
Overview of materials for Nylon 6-3 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6-3". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Ball Indentation Hardness | 130 MPa | 18900 psi | Hc 30; ISO 2039; partially |
Schwartz Technical Plastics LAMIGAMID® 307 Cast Polyamide 6, Heat Stabilized, Dry Application: slippers, inserts for coupling boxesInformation provided by Schwartz Technical Plastics GmbH |
|||
Ball Indentation Hardness | 130 MPa | 18900 psi | Hc 30; ISO 2039; partially |
Schwartz Technical Plastics LAMIGAMID® 309 Cast Polyamide 6, Oil Filled, Dry Application: slippers, inserts for coupling boxes, wear linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Ball Indentation Hardness | 130 MPa | 18900 psi | Hc 30; ISO 2039; partially |
Schwartz Technical Plastics LAMIGAMID® 319 Cast Polyamide 6, Oil Filled, Conditioned Application: sheaves and wheels without additional bearings, sliding linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Ball Indentation Hardness | 130 MPa | 18900 psi | Hc 30; ISO 2039; partially |
Schwartz Technical Plastics LAMINEX® 2101 Cotton Fabric, Phenolic Resin Impregnated Application: bearing segments and prismatic bearingsInformation provided by Schwartz Technical Plastics GmbH |
|||
Ball Indentation Hardness | 130 MPa | 18900 psi | Hc 30; ISO 2039; partially |
Schwartz Technical Plastics LAMINEX® 2140 Cotton Fabric, Phenolic Resin Impregnated, MoS2 Filled Application: bearing shells and bearing collarsInformation provided by Schwartz Technical Plastics GmbH |
|||
Ball Indentation Hardness | 130 MPa | 18900 psi | Hc 30; ISO 2039; partially |
Schwartz Technical Plastics LAMINEX® 2141 Cotton Fabric, Phenolic Resin Impregnated, MoS2 Filled Application: bearing segments and prismatic bearingsInformation provided by Schwartz Technical Plastics GmbH |
|||
Ball Indentation Hardness | 130 MPa | 18900 psi | Hc 30; ISO 2039; partially |
Schwartz Technical Plastics LAMINEX® 2100 Cotton Fabric, Phenolic Resin Impregnated Application: bearing shells and bearing collarsInformation provided by Schwartz Technical Plastics GmbH |
|||
Ball Indentation Hardness | 130 MPa | 18900 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® AG-30 H PA66 Product description: Grilon AG-30 H black 9836 is a normal viscosity, specially heat stabilized PA 66 injection molding grade with 30% glass fibres. Grilon AG-30 H black 9836 has the following impor.. |
|||
Ball Indentation Hardness | 130 MPa | 18900 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® BS EC PA6 Product description: Grilon BS 23 is an unreinforced, low viscosity and fine crystalline PA 6 injection molding grade. Grilon BS 23 has the following important properties: Good flow behaviorEasy pro.. |
|||
Ball Indentation Hardness | 130 MPa | 18900 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® BRZ 340 H PA6 Product description: Grilon BRZ 340 H is a heat stabilized, high viscosity, impact modified PA6 extrusion grade. Grilon BRZ 340 H has the following important properties:High impact strength at low t.. |
|||
Ball Indentation Hardness | 130 MPa @Load 36.5 kg, Time 30.0 sec |
18900 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
BASF Ultraform® S2320 0035 LEV POM Description: Is a POM, free-flowing and rapidly solidifying standard grade with reduced emission potential for injection molding.Information provided by BASF |
|||
Ball Indentation Hardness | 130 MPa @Load 36.5 kg, Time 30.0 sec |
18900 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
BASF Ultraform® S2320 0035 POM Description: Is a POM, free-flowing and rapidly solidifying standard grade with improved impact strength for injection molding.Information provided by BASF |
|||
Ball Indentation Hardness | 130 MPa | 18900 psi | value at 30 sec.; ISO 2039-1 |
CENTROPLAST CENTROPHEN GF Polyphenylene ether 30% glass fiber This material is a lightweight plastic with low moisture absorption, and is impact resistant at low temperatures. Applications include electronic housings, valve pistons, and support rollers.Inform.. |
|||
Ball Indentation Hardness | 130 MPa | 18900 psi | ISO 2039-1 |
BASF Ultradur B 4500 PBT Ultradur B4500 is a general-purpose injection molding grade for high-precision, high-toughness, and dimensionally stable engineering parts. It conforms to FDA requirements of 21 CFR 177.1660. |
|||
Ball Indentation Hardness | 130 MPa @Load 36.5 kg, Time 30.0 sec |
18900 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
BASF Ultraform® W2320 0035 POM Description: Is a POM, very free-flowing and rapidly solidifying grade for high processing demands.Information provided by BASF |
|||
Ball Indentation Hardness | 130 MPa | 18900 psi | ISO 2039-1 |
BASF Ultradur B 6550 PBT Ultradur B 6550 is a high viscosity PBT extrusion grade.Applications; Used for loose buffer tubes for optical fibers, semi-finished products fro machining, profiles and pipes. |
|||
Ball Indentation Hardness | 130 MPa | 18900 psi | ISO 2039 |
GEHR Plastics PPE-30GF Polyphenylene Ether, 30% Glass Fiber
(discontinued **) The 30% glass fiber reinforced PPE has an improved dimensional stability, a very high stiffness and heat resistance that allows further uses. |