Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Schwartz Technical Plastics LAMINEX® 2101 Cotton Fabric, Phenolic Resin Impregnated

Category Polymer , Thermoset , Phenolic , Phenolic, Novolac, Fabric Filled
Manufacturer Schwartz Technical Plastics
Trade Name LAMINEX®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Schwartz Technical Plastics LAMINEX® 2101 Cotton Fabric, Phenolic Resin Impregnated.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Application: bearing segments and prismatic bearingsInformation provided by Schwartz Technical Plastics GmbH
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
ISO R 1183
Water Absorption at Saturation 2.2 %

@Temperature 20.0 °C
2.2 %

@Temperature 68.0 °F
ISO R 62
Mechanical Properties Metric English Comments
Ball Indentation Hardness 130 MPa
18900 psi
Hc 30; ISO 2039; partially
Tensile Strength, Yield 40.0 - 60.0 MPa
5800 - 8700 psi
ISO-DIS 527
Flexural Strength 60.0 MPa
8700 psi
DIN 54352
Flexural Modulus 7.00 - 10.0 GPa
1020 - 1450 ksi
DIN 53457
Compressive Strength 140 MPa
20300 psi
ISO 604
Izod Impact, Notched (ISO) >= 8.00 kJ/m²
>= 3.81 ft-lb/in²
DIN 53453
Izod Impact Resistance >= 0.800 J/cm²
>= 3.81 ft-lb/in²
swinging hammer 0,1 DIN 51222; DIN 53453
Thermal Properties Metric English Comments
CTE, linear 30.0 - 40.0 µm/m-°C

@Temperature 20.0 - 100 °C
16.7 - 22.2 µin/in-°F

@Temperature 68.0 - 212 °F
DIN 53752
Thermal Conductivity 0.300 W/m-K
2.08 BTU-in/hr-ft²-°F
DIN 52612
Maximum Service Temperature, Air 125 °C
257 °F
Continuous
150 °C
302 °F
Intermittent
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+9 ohm-cm
1.00e+9 ohm-cm
DIN 53482
Surface Resistance 1.00e+8 ohm
1.00e+8 ohm
DIN 53482
Dielectric Constant 6.0 - 10

@Frequency 1000 Hz
6.0 - 10

@Frequency 1000 Hz
DIN 53483
Dielectric Strength 20.0 kV/mm
508 kV/in
DIN 53481
Dielectric Loss Index 0.40

@Frequency 1000 Hz
0.40

@Frequency 1000 Hz
DIN 53483
Descriptive Properties Value Comments
Moisture Absorption at Equilibrium 300 mg
DIN 53472
Users viewing this material also viewed the following: