Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.020 - 0.030 cm/cm | 0.020 - 0.030 in/in | ASTM D955 |
PolyOne LubriOne™ 5209 FPL 20 Natural Acetal (POM) Copolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Linear Mold Shrinkage, Flow | 0.020 - 0.030 cm/cm | 0.020 - 0.030 in/in | ASTM D955 |
PolyOne LubriOne™ AT-000/10T 2S Acetal (POM) Copolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Linear Mold Shrinkage, Flow | 0.020 - 0.030 cm/cm | 0.020 - 0.030 in/in | ASTM D955 |
PolyOne LubriOne™ AT-000/20T Black Acetal (POM) Copolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.030 cm/cm @Thickness 3.18 mm |
0.010 - 0.030 in/in @Thickness 0.125 in |
ASTM D955 |
PolyOne Edgetek® PC-30CF/000 BLACK Polycarbonate (PC) Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.030 cm/cm | 0.015 - 0.030 in/in | ASTM D955 |
PolyOne Maxxam™ FR PP 301 EXT Polypropylene, Unspecified (PP, Unspecified) Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.030 cm/cm @Thickness 3.20 mm |
0.010 - 0.030 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUPOY SC2202 PC+GF20%, High Impact Description: Injection Molding, PC+GF20%, Good Toughness, Good Impact, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 65997-17-3Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.030 cm/cm @Time 86400 sec |
0.010 - 0.030 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Lubricomp KI001A Acetal LNP* Lubricomp Fulton 441D is an Acetal based compound with Silicone.This data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.030 cm/cm @Time 86400 sec |
0.010 - 0.030 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Lubricomp KZL34 POM LNP* Lubricomp* KZL34 is a compound based on Acetal resin containing Milled Glass and PTFE. Characteristic of this grade is Internally Lubricated.This data was supplied by SABIC-IP for the Americas.. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.030 cm/cm @Time 86400 sec |
0.010 - 0.030 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Lubricomp ML002S PP LNP* Lubricomp* ML002S is a compound based on Polypropylene containing PTFE. Characteristics of this grade are: Heat Stabilized and Internally Lubricated.This data was supplied by SABIC-IP for the.. |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.030 cm/cm @Time 86400 sec |
0.0090 - 0.030 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP QL002 PA 6/10 LNP* LUBRICOMP* QL002 is a compound based on Nylon 6/10 containing 10% PTFE. Added features of this grade are: Wear Resistant. |
|||
Linear Mold Shrinkage, Flow | 0.025 - 0.030 cm/cm @Time 86400 sec |
0.025 - 0.030 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRILOY KL201 Acetal LNP LUBRILOY* KL201 is a compound based on Acetal resin containing Proprietary Lubricant. PTFE. Added feature of this material is: Wear Resistant. |
|||
Linear Mold Shrinkage, Flow | 0.025 - 0.030 cm/cm @Time 86400 sec |
0.025 - 0.030 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRILOY KL201 Acetal (Europe-Africa-Middle East) LNP LUBRILOY* KL201 is a compound based on Acetal resin containing PTFE, Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Linear Mold Shrinkage, Flow | 0.020 - 0.030 cm/cm | 0.020 - 0.030 in/in | |
Solvay Specialty Polymers Solef® 11010 Polyvinylidene Fluoride (PVDF) Solef® 11010 PVDF is a medium-viscosity flexible PVDF copolymer resin and is typically processed by extrusion.Features: Copolymer; Good Flexibility; Medium ViscosityAdditional Properties: Crystal.. |
|||
Linear Mold Shrinkage, Flow | 0.020 - 0.030 cm/cm | 0.020 - 0.030 in/in | |
Solvay Specialty Polymers Solef® 6010 Polyvinylidene Fluoride (PVDF) Solef® 6010 PVDF homopolymer has medium viscosity and is typically processed by extrusion.Features: Homopolymer; Medium ViscosityAdditional Properties: Crystallization Heat - ASTM D3417 54.0 to 6.. |
|||
Linear Mold Shrinkage, Flow | 0.020 - 0.030 cm/cm | 0.020 - 0.030 in/in | |
Solvay Specialty Polymers Solef® 6012 Polyvinylidene Fluoride (PVDF) Solef® 6012 PVDF homopolymer is a high-viscosity PVDF resin and is typically processed by extrusion or compression molding.Features: High Viscosity; HomopolymerAdditional Properties: Crystallizat.. |
|||
Linear Mold Shrinkage, Flow | 0.020 - 0.030 cm/cm | 0.020 - 0.030 in/in | |
Solvay Specialty Polymers Solef® 60512 Polyvinylidene Fluoride (PVDF) Solef® 60512 PVDF copolymer has high viscosity of the melt and it is a grade for offshore piping.Features: Copolymer; High ViscosityUses: PipingAdditional Properties: Crystallization Heat - ASTM .. |
|||
Linear Mold Shrinkage, Flow | 0.020 - 0.030 cm/cm | 0.020 - 0.030 in/in | |
Solvay Specialty Polymers Solef® 9007 Polyvinylidene Fluoride (PVDF) Solef® 9007 PVDF homopolymer has low viscosity and is used in film extrusion and injection molding.Features: Homopolymer; Low ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 53... |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.030 cm/cm @Time 86400 sec |
0.010 - 0.030 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Stat-kon TD000 LNP* Stat-kon* TD000 is a compound based on Polyurethane resin. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.030 cm/cm @Time 86400 sec |
0.010 - 0.030 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Thermocomp 5X06476 FP-V (PVDF) LNP* FP-VM-3830 is a compound based on Polyvinylidine Fluoride (PVDF) containing Mineral.This data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.030 cm/cm @Time 86400 sec |
0.010 - 0.030 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Thermocomp FF004 PE LNP THERMOCOMP* FF004 is a compound based on Polyethylene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.030 cm/cm @Time 86400 sec |
0.0010 - 0.030 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP LX03447 PEEK LNP* THERMOCOMP* LX03447 is a compound based on Polyetheretherketone containing Proprietary Filler(s). |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.030 cm/cm @Time 86400 sec |
0.010 - 0.030 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Thermocomp RW008XXZ PA 66 LNP* Thermocomp* RW008XXZ is a compound based on Nylon 6/6 resin containing Wollastonite.This data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.030 cm/cm @Time 86400 sec |
0.010 - 0.030 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Thermocomp WF006SXC PBT LNP* Thermocomp* WF006SXC is a compound based on PBT containing Glass FIber. Characteristic of this grade is: Heat Stabilized.This data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.030 cm/cm @Time 86400 sec |
0.010 - 0.030 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Stat-kon IS000LX PA6.12 LNP* Stat-Kon* IS000LX is a compound based on Nylon 6/12 containing Stainless Steel Fibers.This data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.030 cm/cm @Time 86400 sec |
0.010 - 0.030 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Thermocomp WB008 PBT LNP* Thermocomp* WB008 is a compound based on Thermoplastic Polyester (PBT) containing Glass Beads.This data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Flow | 0.025 - 0.030 cm/cm | 0.025 - 0.030 in/in | ISO DIS 294-4 |
Wellman Wellamid® XT1867-BK1 High Impact Nylon 66 Description: High Impact Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.024 - 0.030 cm/cm @Thickness 4.00 mm |
0.024 - 0.030 in/in @Thickness 0.157 in |
E2P method |
Eurostar Star L PA66 D61 PA66, Injection Molded Star L PA66 D51 is a PTFE/Silicone Oil Lubricated, Unreinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.020 - 0.030 cm/cm | 0.020 - 0.030 in/in | |
Solvay Specialty Polymers Solef® 11010 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 11010 PVDF is a medium-viscosity flexible PVDF copolymer resin and is typically processed by extrusion.Information provided by Solvay Specialty Polymers. |
|||
Linear Mold Shrinkage, Flow | 0.020 - 0.030 cm/cm | 0.020 - 0.030 in/in | |
Solvay Specialty Polymers Solef® 9009 Polyvinylidene Fluoride (PVDF)
(discontinued **) Solef® 9009 PVDF homopolymer has low/medium viscosity and is used in film extrusion and injection molding.Information provided by Solvay Specialty Polymers. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.030 cm/cm @Time 86400 sec |
0.010 - 0.030 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Stat-kon R PA 66 LNP* Stat-kon* R is a compound based on Nylon 66 resin containing Carbon Powder. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the Americas.. |