Material Notes:
Star L PA66 D51 is a PTFE/Silicone Oil Lubricated, Unreinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar.
Physical Properties Metric English Comments
Density 1.21 g/cc
0.0437 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.024 - 0.030 cm/cm

@Thickness 4.00 mm
0.024 - 0.030 in/in

@Thickness 0.157 in
E2P method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 69.0 MPa
10000 psi
ISO 527
Elongation at Break 8.0 %
8.0 %
ISO 527
Flexural Strength 89.0 MPa
12900 psi
ISO 178
Flexural Modulus 2.40 GPa
348 ksi
ISO 178
Izod Impact, Notched (ISO) 6.30 kJ/m²
3.00 ft-lb/in²
80x10x4; ISO 180/1A
Izod Impact, Unnotched (ISO) 53.0 kJ/m²
25.2 ft-lb/in²
80x10x4; ISO 180/1U
Thermal Properties Metric English Comments
Melting Point 265 °C
509 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 165 °C
329 °F
Flatw 80x10x4, sp=64 mm; ISO 75/Af