| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Linear Mold Shrinkage, Flow |
0.015
-
0.019
cm/cm <br>@Thickness 2.00 mm,<br> Temperature 23.0 °C
|
0.015
-
0.019
in/in <br>@Thickness 0.0787 in,<br> Temperature 73.4 °F
|
Internal Method |
|
PolyOne OnFlex™ HT 70A-3S2103 Thermoplastic Elastomer (TPE)
OnFlex™ HT thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds is specially formulated to deliver very good compression set performance at..
|
|||
| Linear Mold Shrinkage, Flow | 0.015 - 0.019 cm/cm | 0.015 - 0.019 in/in | ASTM D955 |
|
PolyOne Geon™ Vinyl Flexible A8500 Polyvinyl Chloride, Flexible (PVC, Flexible)
Recommended for interior applications.Information provided by PolyOne
|
|||
| Linear Mold Shrinkage, Flow |
0.015
cm/cm <br>@Time 86400 sec
|
0.015
in/in <br>@Time 24.0 hour
|
ISO 294 |
|
SABIC Innovative Plastics LNP Faradex MS002P PP (Europe-Africa-Middle East)
LNP* Faradex* MS002P is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, Exceptional Processi..
|
|||
| Linear Mold Shrinkage, Flow | 0.015 - 0.019 cm/cm | 0.015 - 0.019 in/in | ASTM D955 |
|
PolyOne Geon™ Vinyl Flexible A80U0 Polyvinyl Chloride, Flexible (PVC, Flexible)
Recommended for interior applications.Information provided by PolyOne
|
|||
| Linear Mold Shrinkage, Flow | 0.015 cm/cm | 0.015 in/in | |
|
Solvay TECHNYL® A 225F PA66, DRY
Description: Unreinforced polyamide 66, medium viscosity, for injection molding, with a special crystallizing agent, for very fast cycles.Available in: Europe, Latin America and North AmericaProduct..
|
|||
| Linear Mold Shrinkage, Flow |
0.015
cm/cm <br>@Time 86400 sec
|
0.015
in/in <br>@Time 24.0 hour
|
ASTM D955 |
|
SABIC Innovative Plastics LNP LUBRICOMP RA004 PA 66 (Asia Pacific)
LNP LUBRICOMP* RA004 is a compound based on Nylon 66 resin containing Aramid. Added features of this material include: Internally Lubricated.
|
|||
| Linear Mold Shrinkage, Flow | 0.015 - 0.020 cm/cm | 0.015 - 0.020 in/in | SABIC Method |
|
SABIC Innovative Plastics LNP LUBRICOMP RP004 PA6.6 (Europe-Africa-Middle East)
LNP* LUBRICOMP* RP004 is a compound based on PA66 resin containing PTFE, Silicone. Added features include: Internally Lubricated.
|
|||
| Linear Mold Shrinkage, Flow |
0.015
-
0.025
cm/cm <br>@Time 86400 sec
|
0.015
-
0.025
in/in <br>@Time 24.0 hour
|
ISO 294 |
|
SABIC Innovative Plastics LNP LUBRICOMP YL003 Polyester Elastomer (Europe-Africa-Middle East)
LNP* LUBRICOMP* YL003 is a compound based on Polyester Elastomer containing PTFE. Added features include; Internally Lubricated.
|
|||
| Linear Mold Shrinkage, Flow |
0.015
cm/cm <br>@Thickness 3.17 mm
|
0.015
in/in <br>@Thickness 0.125 in
|
ASTM D955 |
|
Techmer ES HiFill® HDPE TM30 30% Talc Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Talc Filler, 30% Filler by WeightInformation provided by TP Composites, Inc.
|
|||
| Linear Mold Shrinkage, Flow |
0.015
-
0.035
cm/cm <br>@Time 86400 sec
|
0.015
-
0.035
in/in <br>@Time 24.0 hour
|
ASTM D955 |
|
SABIC Innovative Plastics LNP STAT-KON KD000 Acetal Copolymer (Europe-Africa-Middle East)
LNP STAT-KON KD000* is also know as: LNP STAT-KON K, LNP STAT-KON KXC. It is a compound based on Acetal resin containing Carbon Powder. Added features of this material include: Electrically Conduct..
|
|||
| Linear Mold Shrinkage, Flow |
0.015
cm/cm <br>@Thickness 3.17 mm
|
0.015
in/in <br>@Thickness 0.125 in
|
ASTM D955 |
|
Techmer ES HiFill® PA6 GF/M15 A1 BK 15% Glass/Mineral Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 15% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized Appearance: BlackInformation provided by TP Compo..
|
|||
| Linear Mold Shrinkage, Flow |
0.015
cm/cm <br>@Thickness 3.17 mm
|
0.015
in/in <br>@Thickness 0.125 in
|
ASTM D955 |
|
Techmer ES Luriblend® PA12 TS18
Availability: North AmericaForms: PelletsAdditive: Silicone Lubricant(2%) and PTFE Lubricant(18%)Features: LubricatedInformation provided by TP Composites, Inc.
|
|||
| Linear Mold Shrinkage, Flow |
0.015
cm/cm <br>@Thickness 3.17 mm
|
0.015
in/in <br>@Thickness 0.125 in
|
ASTM D955 |
|
Techmer ES Luriblend® PA6/6 TL20 HS L Nylon 66
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and PTFE Lubricant(20%)Features: Lubricated, Heat Stabilized and Good Wear ResistanceInformation provided by TP Composites, Inc.
|
|||
| Linear Mold Shrinkage, Flow |
0.015
cm/cm <br>@Thickness 3.17 mm
|
0.015
in/in <br>@Thickness 0.125 in
|
ASTM D955 |
|
Techmer ES Luriblend® PA6/6 TL20 Nylon 66
Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(20%)Features: Lubricated, Low Friction and Good Wear ResistanceUL File Number: E157318TPCI# 9740101Information provided by TP Compos..
|
|||
| Linear Mold Shrinkage, Flow | 0.015 - 0.016 cm/cm | 0.015 - 0.016 in/in | mold temp=100°C; SABIC Method |
|
SABIC Innovative Plastics LNP STAT-KON KD000 Acetal Copolymer
LNP* STAT-KON* KD000 is a compound based on Acetal resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive.
|
|||
| Linear Mold Shrinkage, Flow |
0.015
-
0.035
cm/cm <br>@Time 86400 sec
|
0.015
-
0.035
in/in <br>@Time 24.0 hour
|
ASTM D955 |
|
SABIC Innovative Plastics LNP STAT-KON KD000 Acetal Copolymer
LNP* STAT-KON* KD000 is a compound based on Acetal resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive.
|
|||
| Linear Mold Shrinkage, Flow | 0.015 cm/cm | 0.015 in/in | MCI Method 2 |
|
Goodfellow TPX® RT31 Injection Molding Grade Polymethylpentene
This grade is highly recommended for injection molding; also for film and fiber extrusion.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensive. It has good release c..
|
|||
| Linear Mold Shrinkage, Flow | 0.015 cm/cm | 0.015 in/in | ISO 294-4 |
|
DSM Novamid® ST220 NAT PA6-I
Impact Modified, Injection Molding, Medium Viscosity
|
|||
| Linear Mold Shrinkage, Flow | 0.015 cm/cm | 0.015 in/in | ISO 294-4 2577 |
|
DuPont Performance Polymers Delrin® 500T BK602 Acetal (POM)
(Unverified Data**)
Toughened Medium Viscosity Acetal Homopolymer Delrin 500T BK602 is a toughened medium viscosity acetal homopolymer resin with impact resistance similar to Delrin 100. It can be used in parts requiri..
|
|||
| Linear Mold Shrinkage, Flow | 0.015 cm/cm | 0.015 in/in | ISO 294-4 2577 |
|
DuPont Performance Polymers Hytrel® 6356 Polyester Elastomer TPC-ET
(Unverified Data**)
63 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
|
|||
| Linear Mold Shrinkage, Flow | 0.015 - 0.020 cm/cm | 0.015 - 0.020 in/in | ASTM D955 |
|
Clariant Renol PA213 Nylon 6, Heat Stabilized, Lubricated
Data provided by Clariant Masterbatches
|
|||
| Linear Mold Shrinkage, Flow | 0.015 - 0.025 cm/cm | 0.015 - 0.025 in/in | ASTM D955 |
|
Elastocon TPE Technologies Elastocon® CLR45 Thermoplastic Elastomer
Elastocon® CLR45 is a transparent thermoplastic elastomer that has been developed for applications that require resilience, high strength properties and a good surface finish. Elastocon® CLR45 is..
|
|||
| Linear Mold Shrinkage, Flow | 0.015 - 0.025 cm/cm | 0.015 - 0.025 in/in | ASTM D955 |
|
Elastocon TPE Technologies Elastocon® SMR1450 Thermoplastic Polyolefin Elastomer
Elastocon® SMR1450 thermoplastic polyolefin elastomer has been developed for applications that require low temperature impact resistance and a high gloss scratch and mar resistant surface finish. E..
|
|||
| Linear Mold Shrinkage, Flow | 0.015 cm/cm | 0.015 in/in | ISO 294-4 2577 |
|
DuPont Performance Polymers Hytrel® G4774 Polyester Elastomer TPC-ET
(Unverified Data**)
47 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4774 is a medium modulus grade with nominal hardness of 47D. It contains discoloring stabilizer. It can be proc..
|
|||
| Linear Mold Shrinkage, Flow | 0.015 cm/cm | 0.015 in/in | ISO 294-4 |
|
Azoty Tarnow™ Tarnamid® T-27 MCS 850 Polyamide 6 - Flame Retarded, Unreinforced
Glow wire resistance 850°C, bromine and red phosphorus free, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has ..
|
|||
| Linear Mold Shrinkage, Flow | 0.015 cm/cm | 0.015 in/in | Sheet |
|
BASF Ultradur® B 4406 PBT
Description: Is a PBT, flame-retardant injection-molding grades, unreinforced for parts requiring enhanced fire resistance, e.g. plug-and-socket connectors, housings, coil formers and lighting compo..
|
|||
| Linear Mold Shrinkage, Flow | 0.015 cm/cm | 0.015 in/in | Eurotec |
|
Eurotec® Tecomid® NB40 NL IH PA6, impact modified, natural
Information provided by Eurotec®
|
|||
| Linear Mold Shrinkage, Flow | 0.015 cm/cm | 0.015 in/in | 60x60x2mm; ISO 294 |
|
BASF Ultradur B 4520 PBT
Ultradur B4520 is a medium viscosity, rapidly freezing injection molding grade.
|
|||
| Linear Mold Shrinkage, Flow | 0.015 cm/cm | 0.015 in/in | Sheet |
|
BASF Ultradur B 6550 PBT
Ultradur B 6550 is a high viscosity PBT extrusion grade.Applications; Used for loose buffer tubes for optical fibers, semi-finished products fro machining, profiles and pipes.
|
|||
| Linear Mold Shrinkage, Flow | 0.015 - 0.019 cm/cm | 0.015 - 0.019 in/in | DIS 294-4 |
|
Wellman Wellamid® 42LH-WBK Nylon 6, Engineering Grade
All information provided by Wellman Engineered Resins.
|
|||