Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Zeus FEP Tubing

Category Polymer , Thermoplastic , Fluoropolymer , FEP , Fluorinated Ethylene Propylene (FEP), Molded/Extruded
Manufacturer Zeus
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zeus FEP Tubing.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FEP, fluorinated ethylene propylene, is a melt processable fluoropolymer that allows for long, continuous lengths and has several distinct advantages over PTFE. Applications where FEP tubing is usually chosen require more optical clarity and flexibility. In heat shrinkable form, FEP has a lower recovery temperature than PTFE. This fluoropolymer makes heat shrink and convoluted products that meet 23053/11 and 81914 Mil Spec certifications, respectively. The material has low gas and permeability properties; possesses an excellent UV transmission rating; Biocompatible –USP Class VI approved; and is Gamma sterilizable.
Physical Properties Metric English Comments
Density 2.12 - 2.17 g/cc
0.0766 - 0.0784 lb/in³
ASTM D792
Water Absorption 0.0040 %
0.0040 %
ASTM D257
Crystallinity 70 %
70 %
Mechanical Properties Metric English Comments
Hardness, Shore D 55 - 65
55 - 65
ASTM D2240
Tensile Strength, Ultimate 18.0 - 34.0 MPa
2610 - 4930 psi
ASTM D638
Elongation at Break 245 - 400 %
245 - 400 %
ASTM D638
Modulus of Elasticity 0.440 - 0.640 GPa
63.8 - 92.8 ksi
ASTM D638
Flexural Modulus 0.580 - 0.620 GPa
84.1 - 89.9 ksi
ASTM D790
Coefficient of Friction 0.040 - 0.20
0.040 - 0.20
Thermal Properties Metric English Comments
CTE, linear 100 - 135 µm/m-°C

@Temperature 20.0 °C
55.6 - 75.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Thermal Conductivity 0.190 - 0.250 W/m-K
1.32 - 1.74 BTU-in/hr-ft²-°F
ASTM C177
Melting Point 265 - 275 °C
509 - 527 °F
Maximum Service Temperature, Air 200 - 205 °C
392 - 401 °F
Minimum Service Temperature, Air -240 - -200 °C
-400 - -328 °F
Glass Transition Temp, Tg 80.0 °C
176 °F
Decomposition Temperature 380 - 430 °C
716 - 806 °F
ASTM E1131
Oxygen Index >= 95 %
>= 95 %
ASTM D2863
Optical Properties Metric English Comments
Refractive Index 1.33 - 1.35
1.33 - 1.35
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+17 - 1.00e+18 ohm-cm
1.00e+17 - 1.00e+18 ohm-cm
ASTM D257
Dielectric Constant 2.0 - 2.1

@Frequency 1.00e+6 Hz
2.0 - 2.1

@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 19.7 - 78.7 kV/mm
500 - 2000 kV/in
ASTM D149
Descriptive Properties Value Comments
Radiation Resistance (MRad) 10
Users viewing this material also viewed the following: