Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.230 - 0.251 W/m-K | 1.59 - 1.74 BTU-in/hr-ft²-°F | |
Polikim EFALON® T-100 Virgin PTFE Applications: Gaskets, seals, O-rings, V-Rings, compression packings and similar sealing parts, Bushes, bearings and piston rings, Electrical insulators, Sliding supports, Conveyor belts, Coated tu.. |
|||
Thermal Conductivity | 0.240 - 0.250 W/m-K | 1.67 - 1.74 BTU-in/hr-ft²-°F | Average value: 0.246 W/m-K Grade Count:5 |
Overview of materials for Polyetheretherketone, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PTFE Filled". Each property range of values reported is minimum and maximum values.. |
|||
Thermal Conductivity | 0.170 - 0.250 W/m-K | 1.18 - 1.74 BTU-in/hr-ft²-°F | Average value: 0.201 W/m-K Grade Count:11 |
Overview of materials for Polycarbonate/ASA Alloy, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ASA Alloy, Unreinforced". Each property range of values reported is minimum and maximum va.. |
|||
Thermal Conductivity | 0.150 - 0.251 W/m-K | 1.04 - 1.74 BTU-in/hr-ft²-°F | Average value: 0.238 W/m-K Grade Count:11 |
Overview of materials for Polyperfluoroalkoxyethylene (PFA), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyperfluoroalkoxyethylene, Molded/Extruded". Each property range of values reported is minimum and max.. |
|||
Thermal Conductivity | 0.190 - 0.250 W/m-K | 1.32 - 1.74 BTU-in/hr-ft²-°F | Average value: 0.238 W/m-K Grade Count:11 |
Overview of materials for Fluorinated Ethylene Propylene (FEP), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Fluorinated Ethylene Propylene (FEP), Molded/Extruded". Each property range of values reported is minimu.. |
|||
Thermal Conductivity | 0.150 - 0.250 W/m-K @Temperature 40.0 °C |
1.04 - 1.74 BTU-in/hr-ft²-°F @Temperature 104 °F |
ASTM C177 |
Solvay Specialty Polymers Hyflon® PFA 125 Perfluoroalkoxy (PFA) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res.. |
|||
Thermal Conductivity | 0.190 - 0.250 W/m-K | 1.32 - 1.74 BTU-in/hr-ft²-°F | ASTM C177 |
Zeus FEP Tubing FEP, fluorinated ethylene propylene, is a melt processable fluoropolymer that allows for long, continuous lengths and has several distinct advantages over PTFE. Applications where FEP tubing is usua.. |
|||
Thermal Conductivity | 0.150 - 0.250 W/m-K | 1.04 - 1.74 BTU-in/hr-ft²-°F | ASTM C177 |
Zeus PFA Tubing PFA, or perfluoroalkoxy, is well recognized for its ability to maintain mechanical integrity in extreme temperatures even when exposed to caustic chemicals. PFA comes in high purity versions that ar.. |
|||
Thermal Conductivity | 0.230 - 0.250 W/m-K | 1.60 - 1.74 BTU-in/hr-ft²-°F | Average value: 0.244 W/m-K Grade Count:15 |
Overview of materials for Ionomer, Molded This property data is a summary of similar materials in the MatWeb database for the category "Ionomer, Molded". Each property range of values reported is minimum and maximum values of appropriate Ma.. |