Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 83.0 - 135 µm/m-°C
46.1 - 75.0 µin/in-°F
Average value: 98.9 µm/m-°C Grade Count:10
Overview of materials for Fluorinated Ethylene Propylene (FEP), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Fluorinated Ethylene Propylene (FEP), Molded/Extruded". Each property range of values reported is minimu..
CTE, linear 135 - 135 µm/m-°C

@Temperature 85.0 - 125 °C
75.0 - 75.0 µin/in-°F

@Temperature 185 - 257 °F
Average value: 135 µm/m-°C Grade Count:2
Overview of materials for ECTFE Fluoropolymer
This property data is a summary of similar materials in the MatWeb database for the category "ECTFE Fluoropolymer". Each property range of values reported is minimum and maximum values of appropriat..
CTE, linear 100 - 135 µm/m-°C

@Temperature 20.0 °C
55.6 - 75.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Zeus FEP Tubing
FEP, fluorinated ethylene propylene, is a melt processable fluoropolymer that allows for long, continuous lengths and has several distinct advantages over PTFE. Applications where FEP tubing is usua..