Physical Properties Metric English Comments
Density 2.12 - 2.17 g/cc
0.0766 - 0.0784 lb/in³
Solvay Specialty Polymers Hyflon® PFA 450 Fluoropolymer  (discontinued **)
Data provided by the manufacturer.Hyflon® PFA 450 has outstanding physical and chemical properties typical of fluoropolymers.Hyflon® PFA 420
Density 2.10 - 2.17 g/cc
0.0759 - 0.0784 lb/in³
Average value: 2.14 g/cc Grade Count:22
Overview of materials for Polyperfluoroalkoxyethylene (PFA), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyperfluoroalkoxyethylene, Molded/Extruded". Each property range of values reported is minimum and max..
Density 1.30 - 2.17 g/cc
0.0470 - 0.0784 lb/in³
Average value: 1.94 g/cc Grade Count:15
Overview of materials for Fluorinated Ethylene Propylene (FEP), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Fluorinated Ethylene Propylene (FEP), Molded/Extruded". Each property range of values reported is minimu..
Density 2.14 - 2.17 g/cc
0.0773 - 0.0784 lb/in³
ASTM D792
Guarniflon FEP Fluorinated Ethylene Propylene
Fluorinated thermoplastic material with excellent thermal, electrical and chemical inertness properties. Widely used for different industrial applications for its excellent chemical resistance up t..
Density 2.12 - 2.17 g/cc
0.0766 - 0.0784 lb/in³
ASTM D792
Guarniflon MFA Fluoropolymer
It’s a semi-crystalline fully-fluorinated melt processable fluoropolymer which offer the highest temperature rating and broadest chemical resistance of all melt processable fluoropolymers. It ..
Density 2.12 - 2.17 g/cc
0.0766 - 0.0784 lb/in³
ASTM D792
Guarniflon PFA Perfluoroalkoxy Polymer
Fluorinated thermoplastic material, offers the advantages of being thermo-processed whilst at the same time having the properties of PTFE, with excellent chemical and mechanical resistance for appli..
Density 2.12 - 2.17 g/cc
0.0766 - 0.0784 lb/in³
ASTM D792
Zeus FEP Tubing
FEP, fluorinated ethylene propylene, is a melt processable fluoropolymer that allows for long, continuous lengths and has several distinct advantages over PTFE. Applications where FEP tubing is usua..
Density 2.12 - 2.17 g/cc
0.0766 - 0.0784 lb/in³
ASTM D792
Zeus PFA Tubing
PFA, or perfluoroalkoxy, is well recognized for its ability to maintain mechanical integrity in extreme temperatures even when exposed to caustic chemicals. PFA comes in high purity versions that ar..
Density 2.12 - 2.17 g/cc
0.0766 - 0.0784 lb/in³
ASTM D792
Solvay Specialty Polymers Hyflon® PFA 120X Perfluoroalkoxy (PFA)  (discontinued **)
Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resis..
Density 2.12 - 2.17 g/cc
0.0766 - 0.0784 lb/in³
ASTM D792
Solvay Specialty Polymers Hyflon® PFA P220 Perfluoroalkoxy (PFA)  (Unverified Data**)
Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resis..
Density 1.21 - 2.17 g/cc
0.0437 - 0.0784 lb/in³
Average value: 1.50 g/cc Grade Count:256