Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 265 °C | 509 °F | ASTM D789 |
PolyOne Nymax™ GB 1200 20 HS BLACK 18 Polyamide 66 (Nylon 66) Preliminary Data SheetMolded Test Bars: Dry as MoldedInformation provided by PolyOne |
|||
Melting Point | 265 °C | 509 °F | ASTM D789 |
PolyOne Nymax™ GB 1200 30 HS BLACK 18 Polyamide 66 (Nylon 66) Preliminary Data SheetMolded Test Bars: Dry as MoldedInformation provided by PolyOne |
|||
Melting Point | 265 °C | 509 °F | 10°C/min; ISO 11357-1, -3 |
Lanxess Durethan® DP A 30 S FN30 DUS025 000000 Nylon 66 PA 66, non-reinforced, injection molding, halogen free flame retardant improved flowabilityInformation provided by LANXESS. |
|||
Melting Point | 265 °C | 509 °F | ASTM D789 |
MRC Polymers EMAREXâ„¢ 400 GF13 Nylon 6/6, 13% Glass Fiber Filled Available in Black onlyCan be UV and Heat StabilizedProperty data for DAM samples.Information provided by MRC Polymers Inc. |
|||
Melting Point | 265 °C | 509 °F | 10°C/min; ISO 11357-1, -3 |
Lanxess Durethan® A 30 S FN31 000000 Nylon 66, Flame Retardant PA 66, non-reinforced, injection molding, halogen-free flame retardant, improved flowabilityInformation provided by LANXESS. |
|||
Melting Point | 265 °C | 509 °F | ASTM D789 |
MRC Polymers EMAREXâ„¢ 400 GF33 Nylon 6/6, 33% Glass Fiber Filled Available in Black onlyCan be UV and Heat StabilizedProperty data for DAM samples.Information provided by MRC Polymers Inc. |
|||
Melting Point | 265 - 275 °C | 509 - 527 °F | DSC |
Solvay Specialty Polymers Hyflon® MFA® F1520 Perfluoropolymer Hyflon® F is a family of MFA polymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, high flexural endurance, inherent flame resistance, low s.. |
|||
Melting Point | 265 - 275 °C | 509 - 527 °F | DSC |
Solvay Specialty Polymers Hyflon® MFA® F1530 Perfluoropolymer Hyflon® MFA is a family of perfluoro polymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, high flexural endurance, inherent flame resistanc.. |
|||
Melting Point | 265 - 275 °C | 509 - 527 °F | DSC |
Solvay Specialty Polymers Hyflon® MFA® F1540 Perfluoropolymer Hyflon® MFA is a unique family of perfluoro polymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, high flexural endurance, inherent flame re.. |
|||
Melting Point | 265 °C | 509 °F | ISO 11357 |
Polyram PlusTek PA201 Nylon 66 for Extrusion High viscosity Nylon 66 for extrusion applications.Information provided by Polyram. |
|||
Melting Point | 265 - 275 °C | 509 - 527 °F | |
Zeus FEP Tubing FEP, fluorinated ethylene propylene, is a melt processable fluoropolymer that allows for long, continuous lengths and has several distinct advantages over PTFE. Applications where FEP tubing is usua.. |
|||
Melting Point | <= 265 °C | <= 509 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil HDPE HD 6733.17 High Density Polyethylene Copolymer Resin Product Description: HD 6733 is a narrow molecular weight hexane copolymer designed to maximize injection molding speed and productivity in thing wall articles. Lower processing temperatures enable .. |
|||
Melting Point | 265 °C | 509 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® TSG-60 PA666-GF60 Product description: Grilon TSG-60 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 60% glass fibers. Grilon TSG-60 has the following important properties: Very high st.. |
|||
Melting Point | 265 °C | 509 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® TSG-60/4 W PA666-GF60 Product description: Grilon TSG-60/4 W is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 60% glass fibers, modified for parts with high thermal demands. Grilon TSG-.. |
|||
Melting Point | 265 - 275 °C | 509 - 527 °F | |
Daikin NEOFLON NP-30 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding.Applications: Heavy wall wire insulation, tubes, cable jacketing.. |
|||
Melting Point | 265 - 275 °C | 509 - 527 °F | |
Daikin NEOFLON NP-40 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, transfer molding, compression molding.Applications: Films and s.. |
|||
Melting Point | 265 °C | 509 °F | ISO 3146 |
Eurostar Star L PA66 30V D61 PA66, Glass Fiber Filled, Injection Molded Star L PA66 30V D31 is a PTFE/Silicone Lubricated, Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Melting Point | 265 °C | 509 °F | ISO 3146 |
Eurostar Star L PA66 30Y D51 PA66, Carbon Fiber Filled, Injection Molded Star L PA66 30Y D51 is a PTFE Lubricated, Carbon Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Melting Point | 265 °C | 509 °F | ISO 3146 |
Eurostar Star L PA66 30Y D61 PA66, Carbon Fiber Filled, Injection Molded Star L PA66 30Y D51 is a PTFE/Silicone Oil Lubricated, Carbon Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Melting Point | 265 °C | 509 °F | ISO 3146 |
Eurostar Star L PA66 D51 PA66, Injection Molded Star L PA66 D51 is a PTFE Lubricated, Unreinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Melting Point | 265 °C | 509 °F | ISO 3146 |
Eurostar Star L PA66 D61 PA66, Injection Molded Star L PA66 D51 is a PTFE/Silicone Oil Lubricated, Unreinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Melting Point | 265 °C | 509 °F | ISO 3146 |
Eurostar Star L PA66 D91 PA66, Aramid Fiber Filled, Injection Molded Star L PA66 D91 is a PTFE lubricated, Aramid Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Melting Point | 265 °C | 509 °F | |
DuPont Teijin Films Melinex® ST507 Polyester Film Melinex® ST507 is a slightly hazy, heat stabilized, polyester film. It has good handling characteristics and is recommended for silver circuitry applications, particularly where an adhesion topcoat.. |
|||
Melting Point | 265 - 275 °C | 509 - 527 °F | |
Daikin NEOFLON NP-20 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, injection molding.Applications: Wire and cable coatings, films,.. |
|||
Melting Point | 265 °C | 509 °F | ISO 11357-3 |
Ascend Performance Materials Vydyne® ECO315 BK13 Nylon 66, Flame Retardant, DAM Vydyne® ECO366 BK13 is a non-halogenated, unfilled, flame-retardant PA66 homopolymer designed with superior flow properties to assist in filling thin-walled, intricate parts. It is lubricated for m.. |
|||
Melting Point | 265 °C | 509 °F | |
DuPont Teijin Films Melinex® ST557 Polyester Film, 200 Gauge Melinex® ST557 is a slightly hazy polyester film with low shrinkage, good flatness, and excellent handling properties. Melinex® ST557 is pretreated with a unique primer on both surfaces for adhesi.. |
|||
Melting Point | 265 °C | 509 °F | ISO 11357-3 |
Ascend Performance Materials Vydyne® ECO366 Nylon 66, Flame-retardant, DAM Vydyne® ECO366 is a non-halogenated, unfilled, flame-retardant PA66 homopolymer designed with superior flow properties to assist in filling thin-walled, intricate parts. It is lubricated for machin.. |
|||
Melting Point | 265 °C | 509 °F | ISO 3146 |
Eurostar Star L PA66 15Y D52 PA66, Carbon Filled, Injection Molded Star L PA66 15Y D52 is a PTFE Lubricated, Carbon Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Melting Point | 265 °C | 509 °F | ISO 3146 |
Eurostar Star L PA66 15Y D61 PA66, Carbon Filled, Injection Molded Star L PA66 15Y D61 is a PTFE/Silicone Oil Lubricated, Carbon Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Melting Point | 265 °C | 509 °F | 10°C/min; ISO 11357-1/-3 |
Lanxess Durethan® DP 2801 000000 Nylon 66 PA 66 injection molding grade, non-reinforced, UL 94V-2 off 0,75 mm (listed), GWFI: 960°C off 0.75 mm, GWIT: 775°C off 0,75 mm, halogen-free |