Tra-Con Tra-Bond 2123 Metal Repair Steel/Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy , Filled/Reinforced Thermoset
Manufacturer Tra-Con, Inc.
Trade Name Tra-Bond
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tra-Con Tra-Bond 2123 Metal Repair Steel/Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TRA-BOND 2123 is a versatile steel metal/epoxy adhesive formulation developed for modern industrial repair, casting and bonding applications where a steel-like or cast iron finish is required. This easy-to-use adhesive system contains no solvents and cures fairly rapidly at room temperature to a hard, low shrinkage solid, which bonds readily to steel, aluminum, and other metals, wood, concrete, glass, ceramics and many plastics. Fully cured TRA-BOND 2123 is tough and durable, resistant to water, mild acids and alkalis, salts and salt solutions, lubricating oils, petroleum solvents, gasoline, jet fuels, alcohol and many other organic and inorganic materials, While it may be attracted to a magnet, it is essentially an electrical insulator which can be readily drilled, cut, sawed and machined with regular metal working tools Typical repair applications: jigs, molds, dies, fixtures, plumbing, automotive, castings, aircraft, ships, marine, salvage. Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Specific Gravity 2.35 g/cc
2.35 g/cc
Mixed
Solids Content 100 %
100 %
Reactive Solids Content
Viscosity 32000 cP

@Temperature 25.0 °C
32000 cP

@Temperature 77.0 °F
After mixing
Mechanical Properties Metric English Comments
Hardness, Shore D 88
88
Thermal Properties Metric English Comments
CTE, linear 38.0 µm/m-°C

@Temperature 20.0 °C
21.1 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 0.590 W/m-K
4.09 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 135 °C
275 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Glass Transition Temp, Tg 110 °C
230 °F
Ultimate Tg
Shrinkage 0.080 %
0.080 %
Electrical Properties Metric English Comments
Dielectric Constant 65

@Frequency 1000 Hz
65

@Frequency 1000 Hz
Dielectric Strength 1.18 kV/mm
30.0 kV/in
Dissipation Factor 0.20

@Frequency 1000 Hz
0.20

@Frequency 1000 Hz
Processing Properties Metric English Comments
Cure Time 240 min

@Temperature 65.0 °C
4.00 hour

@Temperature 149 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 30 min
30 min
Descriptive Properties Value Comments
Color Steel Gray
Mix Ratio, parts by weight 100/10
Resin/Hardener