Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 30 min | 30 min | |
NextGen Adhesives G907-31 Epoxy Adhesive Description: NGAC G907-31 is a medium viscosity epoxy adhesive system utilized extensively in industrial and structural applications.Advantages and Applications: The NGAC G907-31 provides excellent .. |
|||
Pot Life | 30 - 40 min | 30 - 40 min | Ambient |
Reltek BONDiT™ B-45TH Adhesive, Sealant & Coating System Key Properties: Excellent adhesion to low surface energy plastics without primer.Bonding dissimilar materials.Chemical and shock resistance.Ease of use.Applications: Bonds difficult-to-bond substrat.. |
|||
Pot Life | 30 - 40 min | 30 - 40 min | Ambient |
Reltek BONDiT™ B-52 Adhesive, Sealant & Potting System Key Properties: Outstanding for bonding dissimilar materials with high thermal expansion differential applications.Fast thermal cure, long pot life.Ease of use.Applications: Excellent for fast assem.. |
|||
Pot Life | 30 min | 30 min | |
Resin Technology Group 109-DP Oxy-Bond™ Two-Component Epoxy Adhesive Oxy-Bond and Millenium Adhesive SystemsEngineered for strength, durability, lightness, and formability, our Oxy-Bond and Millenium lines offer adhesives with physical and electrical properties to ma.. |
|||
Pot Life | >= 30 min | >= 30 min | |
Abatron 80056 A/B Filled Potting Compound
(discontinued **) Neutral gray liquid epoxy to bond new to old concrete and for wet surfaces. 100/43 ratio.Information provided by Abatron. |
|||
Pot Life | 30 min | 30 min | Small Mass |
Resin Technology Group TIGA 110-EXDP Low Viscosity, Optically Clear Glass Bonder Mix ratio 100/50 by volume.TIGA 110EX-DP is a transparent, low viscosity epoxy resin formulation recommended for industrial adhesive, small potting and laminating applications where sparkling clarit.. |
|||
Pot Life | 30 - 60 min | 30 - 60 min | Time before parts must be mated |
Lord Adhesives 7542E Two-Component Urethane Adhesive Lord Urethane AdhesivesLord® one- and two-part urethane adhesives provide superior bonds with minimal surface preparation for today's high performance thermosets and thermoplastics. They offe.. |
|||
Pot Life | 30 - 60 min @Temperature 24.0 °C |
30 - 60 min @Temperature 75.2 °F |
54g mass |
Lord Adhesives Fusor® 310 A/B Epoxy Adhesive Lord® 310 adhesive is a modified, thixotropic, two-part epoxy adhesive which bonds well to many types of prepared metals, prepared rubber, urethane, and plastics. Originally formulated for primer.. |
|||
Pot Life | 30 - 35 min | 30 - 35 min | |
ITW Plexus Plexusâ„¢ MA350 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Low viscosity adhesive, high strength, especially suitable for battery case applications.Informati.. |
|||
Pot Life | 30 - 50 min | 30 - 50 min | 100 gram mass |
Master Bond EP21ARHT Two component epoxy adhesive, sealant, coating and encapsulating system Product Description: Master Bond EP21ARHT is a two component epoxy resin system for high performance bonding, sealing, coating and encapsulating. It has a convenient 100 to 50 mix ratio by weight an.. |
|||
Pot Life | 30 - 50 min | 30 - 50 min | 100 gram mass |
Master Bond EP21ARHTND Two component epoxy adhesive, sealant, coating and encapsulating system Product Description: Master Bond EP21ARHTND is a two component epoxy resin system for high performance bonding, sealing and coating. It has a convenient 100 to 50 mix ratio by weight and is formulat.. |
|||
Pot Life | 30 - 40 min | 30 - 40 min | 50 gram mass |
Master Bond EP21TDCSMed Two Component, Silver Conductive USP Class VI Epoxy Master Bond Polymer System EP21TDCS MED is a two component, silver filled, electrically conductive adhesive/sealant that meets USP Class VI specifications for medical applications. The high strength.. |
|||
Pot Life | 30 - 45 min | 30 - 45 min | 100 gram batch |
Master Bond EP30AOHT Dimensionally Stable, Two Component Epoxy Description: Master Bond Polymer System EP30AOHT is a two component epoxy resin system for high performance bonding, potting, sealing and coating, formulated to cure at room temperature or more rapi.. |
|||
Pot Life | 30 - 35 min | 30 - 35 min | 100 gram batch |
Master Bond EP30P Epoxy Bonds Glass, Polycarbonates and Acrylics Description: Master Bond Polymer Adhesive EP30P is a two component, transparent, low viscosity epoxy resin system for high performance bonding, sealing, coating, encapsulating and casting. It is for.. |
|||
Pot Life | 30 min | 30 min | |
Tra-Con Tra-Bond 216L01 Clear Low Viscosity Epoxy Adhesive TRA-BOND 216L01 is a clear, low viscosity epoxy adhesive system that contains no solvents, cures at room temperature, has excellent flowability and wetting characteristics, and adheres strongly to g.. |
|||
Pot Life | 30 min | 30 min | 2 grams |
Tra-Con Tra-Bond F112 Fiber Optic Epoxy Adhesive TRA-BOND F112 is a long pot life, impact resistant, fiber-optic adhesive. This two-part, low viscosity epoxy has the distinct advantage of remaining below 3000 cps for a minimum of 40 minutes. This .. |
|||
Pot Life | 30 min | 30 min | |
Tra-Con Tra-Cast 3108 General Purpose Epoxy Casting Compound TRA-CAST 3108 is a low viscosity two-part formulation recommended for underfill and encapsulating applications where the combination of good mechanical thermal and electrical properties are required.. |
|||
Pot Life | 30 min | 30 min | 25 grams |
Tra-Con Tra-Cast 3110 Low Density Epoxy Casting System TRA-CAST 3110 is a unicellular, low density, syntactic-foam epoxy resin casting system of medium viscosity that easily handles, mixes and cures at room temperature. Developed for industrial encapsul.. |
|||
Pot Life | 30 min | 30 min | |
Tra-Con Tra-Cast 3113 General Purpose Epoxy Casting Compound TRA-CAST 3113 is a low viscosity two-part formulation recommended for general purpose electrical potting and encapsulating applications where the combination of good mechanical thermal and electrica.. |
|||
Pot Life | 30 min | 30 min | |
Tra-Con Tra-Cast F353 Optically Opaque Casting System TRA-CAST F353 is an optically opaque, low viscosity, two-part epoxy system recommended for molding, potting, embedding, encapsulating, sealing and casting applications involving fiber optic, optical.. |
|||
Pot Life | 30 min | 30 min | |
Tra-Con Tra-Bond 2101 General Purpose Epoxy Adhesive TRA-BOND 2101 is a medium viscosity epoxy formulation recommended for laminating, bonding, repair and other adhesive applications where the combination of its superior structural, mechanical and ele.. |
|||
Pot Life | 30 - 40 min @Temperature 25.0 °C |
30 - 40 min @Temperature 77.0 °F |
100 g |
Abatron AboCast 8005-6/AboCure 8005-6 Epoxy AboCast 8005-6 is a tan, viscous filled liquid resin with a weight of approximately 11 lbs/gallon. AboCure 8005-6 is an amber, viscous liquid converter with a weight of approximately 10 lbs/gallon. .. |
|||
Pot Life | 30 - 35 min @Temperature 24.0 °C |
30 - 35 min @Temperature 75.2 °F |
4 oz. mass |
BCC Products BC 6060 Epoxy Surface Coat/Casting BC 6060 is a blue epoxy, abrasion resistant surfacing resin. Commonly referred to as “die surface” material, this system may be applied by brush or if preferred, cast in thin sections to a maximum.. |
|||
Pot Life | 30 - 40 min | 30 - 40 min | Mass: 50g; TM R050-19 |
Resinlab® EP1056LV Black Urethane Modified Epoxy Casting Resin Resinlab™ EP1056LV Black is a two part urethane modified epoxy casting resin designed to give good adhesion to metals and PVC. It has good wetting to most surfaces and is free-flowing to penetrate .. |
|||
Pot Life | 30 - 45 min | 30 - 45 min | Mass: 100g; TM R050-17 |
Resinlab® EP1285HD-14 Highly Filled, Medium Viscosity Casting Resin Resinlab™ EP1285 (Formerly Lab Product W021901 series) is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity and a low C.. |
|||
Pot Life | 30 min | 30 min | |
Henkel Hysol EA 960F Paste Adhesive System Fast-set fairing and smoothing compound for exterior aircraft surfaces.Sandable after 6 hours |