Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 30 min | 30 min | |
NextGen Adhesives G907-31 Epoxy Adhesive Description: NGAC G907-31 is a medium viscosity epoxy adhesive system utilized extensively in industrial and structural applications.Advantages and Applications: The NGAC G907-31 provides excellent .. |
|||
Pot Life | 30 - 40 min | 30 - 40 min | |
NextGen Adhesives P907-03 Fiber Optic Adhesive Description: NGAC P907-03 is a low viscosity and room temperature curing adhesive specifically formulated for fiber optic terminations.Advantages and Applications: Uses include the termination of si.. |
|||
Pot Life | 30 - 40 min | 30 - 40 min | Ambient |
Reltek BONDiT™ B-45 Adhesive, Sealant & Coating System Key Properties: Excellent adhesive for low surface energy plastics without primer.Used in potting, painting and protective coating applications.Excellent thermal and mechanical shock resistance.Ease.. |
|||
Pot Life | 30 min | 30 min | |
Resin Technology Group 109-DP Oxy-Bond™ Two-Component Epoxy Adhesive Oxy-Bond and Millenium Adhesive SystemsEngineered for strength, durability, lightness, and formability, our Oxy-Bond and Millenium lines offer adhesives with physical and electrical properties to ma.. |
|||
Pot Life | 30 min | 30 min | |
Huntsman HY 355 Cycloaliphatic Amine Approx. H+ equivalent weight 48.5. Mix Ratio with GY 6010 is 26.Comments/Applications: Modified cycloaliphatic polyamine adduct for resistance to solvents and high temperature, especially when use.. |
|||
Pot Life | 30 - 40 min | 30 - 40 min | 50 gram mass |
Master Bond EP21TDCSMed Two Component, Silver Conductive USP Class VI Epoxy Master Bond Polymer System EP21TDCS MED is a two component, silver filled, electrically conductive adhesive/sealant that meets USP Class VI specifications for medical applications. The high strength.. |
|||
Pot Life | 30 - 45 min | 30 - 45 min | 100 gram batch |
Master Bond EP30AN-1 Low Viscosity, NASA Low Outgassing Epoxy Description: Master Bond EP30AN-1 is a two part epoxy for high performance potting, sealing, coating and bonding featuring high thermal conductivity, excellent electrical insulation properties and N.. |
|||
Pot Life | 30 min | 30 min | |
Tra-Con Tra-Bond 2112 Rigid Epoxy Staking Compound TRA-BOND 2112 is a thixotropic epoxy system recommended for critical electronic, aerospace and industrial bonding, laminating and reinforcing applications requiring an adhesive with high-fill, non-s.. |
|||
Pot Life | 30 min | 30 min | |
Tra-Con Tra-Bond 216L01 Clear Low Viscosity Epoxy Adhesive TRA-BOND 216L01 is a clear, low viscosity epoxy adhesive system that contains no solvents, cures at room temperature, has excellent flowability and wetting characteristics, and adheres strongly to g.. |
|||
Pot Life | 30 min | 30 min | |
Tra-Con Tra-Bond F110 Optically Transparent Low Viscosity Epoxy Adhesive TRA-BOND F110 is a rigid, optically clear adhesive with a very low viscosity. This room temperature curing system is an excellent choice for thin bond-line assembly and repair applications of prisms.. |
|||
Pot Life | 30 min | 30 min | 25 grams |
Tra-Con Tra-Bond F113SC BLK High Tg Fiber Optic Epoxy Adhesive TRA-BOND F113SC BLK is a fiber optic adhesive used for terminating ALL types of fiber optic connectors as well as LED displays, lenses and other optical components. It produces a typical Tg of 95°C.. |
|||
Pot Life | 30 min | 30 min | |
Tra-Con Tra-Cast 3103 General Purpose Epoxy Casting Compound TRA-CAST 3103 is a low viscosity two-part formulation recommended for general purpose electrical potting and encapsulating application where the combination of good mechanical thermal and electrical.. |
|||
Pot Life | 30 min | 30 min | |
Tra-Con Tra-Cast F353 Optically Opaque Casting System TRA-CAST F353 is an optically opaque, low viscosity, two-part epoxy system recommended for molding, potting, embedding, encapsulating, sealing and casting applications involving fiber optic, optical.. |
|||
Pot Life | 30 - 40 min | 30 - 40 min | 100 gram mass |
Master Bond EP30QF Quartz Filled, Two Component Epoxy System Master Bond Polymer System EP30QF is a quartz filled, two component epoxy for high performance bonding, sealing, coating and casting that is formulated to cure at room temperature or more rapidly at.. |
|||
Pot Life | 30 min | 30 min | |
Tra-Con Tra-Bond 2101 General Purpose Epoxy Adhesive TRA-BOND 2101 is a medium viscosity epoxy formulation recommended for laminating, bonding, repair and other adhesive applications where the combination of its superior structural, mechanical and ele.. |
|||
Pot Life | 30 min | 30 min | |
Tra-Con Tra-Bond 2129 Clear Low Viscosity Epoxy Adhesive TRA-BOND 2129 is a low viscosity epoxy adhesive recommended for industrial and electronic production, repair, small casting, coating, tooling, and rigid laminating applications where a clear system .. |
|||
Pot Life | 30 min | 30 min | 100 grams |
Tra-Con Tra-Bond 2143D Medium Viscosity Polyamide Epoxy Adhesive TRA-BOND 2143D is a medium viscosity adhesive recommended for industrial bonding and sealing applications where toughness, impact resistance, and superior mechanical properties are required. This tw.. |
|||
Pot Life | 30 min | 30 min | |
Tra-Con Tra-Duct 916D01 Electrically Conductive Silver-Filled Epoxy TRA-DUCT 916D01 is an electrically conducting silver-filled epoxy compound recommended for electronic bonding and sealing applications that require a combination of good mechanical and electrical pr.. |
|||
Pot Life | 30 min | 30 min | |
Loctite® Durabond® E-30CL Epoxy Adhesive Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 appli.. |
|||
Pot Life | 30 min | 30 min | |
Epoxy Technology EPO-TEK® 320NC-2 Optically Opaque Epoxy Material Description: A two component, black colored and optically opaque epoxy designed for optical, medical, and opto-electronic packaging of semiconductor devices and components. It is a modific.. |
|||
Pot Life | 30 min @Temperature 25.0 °C |
30 min @Temperature 77.0 °F |
200 g |
Abatron AboCast 8110-4/AboCure 8110-3 Flexible Epoxy This epoxy system can achieve flexibility and plasticity without sacrificing adhesive, electrical, structural, and other properties. This compound is a clear (unfilled) basic formulation. Its applic.. |
|||
Pot Life | 30 - 35 min @Temperature 24.0 °C |
30 - 35 min @Temperature 75.2 °F |
4 oz. mass |
BCC Products BC 6060 Epoxy Surface Coat/Casting BC 6060 is a blue epoxy, abrasion resistant surfacing resin. Commonly referred to as “die surface” material, this system may be applied by brush or if preferred, cast in thin sections to a maximum.. |
|||
Pot Life | 30 min @Temperature 25.0 °C |
30 min @Temperature 77.0 °F |
200 g |
Abatron AboCast 8110-7/AboCure 8110-1 Flexible Epoxy This epoxy system can achieve flexibility and plasticity without sacrificing adhesive, electrical, structural, and other properties. This compound is a clear (unfilled) basic formulation. Its applic.. |
|||
Pot Life | 30 min @Temperature 24.0 °C |
30 min @Temperature 75.2 °F |
125 gram mass |
BCC Products BC 5009 General Purpose Epoxy System BC5009 is a very low viscosity, modified, unfilled, room temperature curing, general purpose resin system. BC5009 is a clear-amber epoxy adhesive especially formulated for the bonding of wood and u.. |
|||
Pot Life | 30 min @Temperature 25.0 °C |
30 min @Temperature 77.0 °F |
|
Parker Chomerics Tecknit® 73-00025 Electrically Conductive Acrylic and Polyurethane Paint Description: TECKNIT manufactures a highly conductive acrylic and polyurethane paints filled with silver. These coatings provide a cost effective method for shielding and grounding plastic enclosure.. |
|||
Pot Life | 30 - 40 min | 30 - 40 min | Mass: 50g; TM R050-19 |
Resinlab® EP1056LV Black Urethane Modified Epoxy Casting Resin Resinlab™ EP1056LV Black is a two part urethane modified epoxy casting resin designed to give good adhesion to metals and PVC. It has good wetting to most surfaces and is free-flowing to penetrate .. |
|||
Pot Life | 30 min | 30 min | |
Henkel Hysol EA 9323 Paste Adhesive System Viscous, but pourable, liquid adhesive that yields tough, durable adhesive bonds over a wide temperature range.Application: Structural Repair |
|||
Pot Life | 30 min | 30 min | Mass: 50g; TM R050-19 |
Resinlab® EP1056LC Urethane Modified Epoxy Adhesive Resinlab™ EP1056LC is a two part urethane modified epoxy adhesive designed to give good adhesion to metals and hard to bond surfaces such as PVC. It is thixotropic to provide good gap filling abili.. |