Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 1.18 kV/mm | 30.0 kV/in | ASTM D149 |
ITW Devcon Metal Repair Stainless Steel Putty (ST), Grey Information provided by ITW Devcon |
|||
Dielectric Strength | 1.18 kV/mm | 30.0 kV/in | ASTM D149 |
ITW Devcon Plastic Steel® Metal Repair (A), Dark Grey Information provided by ITW Devcon |
|||
Dielectric Strength | 1.18 kV/mm | 30.0 kV/in | ASTM D149 |
ITW Devcon Plastic Steel® Metal Repair 5 Minute® Putty (SF), Dark Grey Information provided by ITW Devcon |
|||
Dielectric Strength | 1.18 kV/mm | 30.0 kV/in | |
Tra-Con Tra-Bond 2123 Metal Repair Steel/Epoxy Adhesive TRA-BOND 2123 is a versatile steel metal/epoxy adhesive formulation developed for modern industrial repair, casting and bonding applications where a steel-like or cast iron finish is required. This .. |
|||
Dielectric Strength | 1.18 kV/mm | 30.0 kV/in | |
ChevronTexaco ISO 68 Refrigeration Oil WF FeaturesChevron Refrigeration Oils WF are manufactured using medium viscosity index straight mineral oils. The base stocks are carefully selected to assure the low pour points that are necessary for.. |
|||
Dielectric Strength | 1.18 kV/mm | 30.0 kV/in | ASTM D149 |
Ensinger Tecamid® MDS® Molybdenum Disulfide Filled Nylon (PA) Tecamid MDS® has enhanced surface lubricity and wear resistance over unfilled nylon. It is an ideal material to replace metals in machinery. Low surface friction Increased surface hardness Incre.. |
|||
Dielectric Strength | 1.18 kV/mm | 30.0 kV/in | ASTM D149 |
Devcon Plastic Steel® Liquid (B) Epoxy General Repair EpoxyComments: Steel-filled liquid epoxy can be cast over models for accurate detail reproduction when making holding fixtures, light-gauge forming dies and molds. Hardens in about a.. |
|||
Dielectric Strength | 1.18 kV/mm | 30.0 kV/in | ASTM D149 |
Devcon Plastic Steel® Putty (A) Epoxy General Repair EpoxyComments: The original metal-filled epoxy putty used for hundreds of routine maintenance, production and tooling applications. Bonds to most metal, concrete and some plastics. .. |
|||
Dielectric Strength | 1.18 kV/mm | 30.0 kV/in | |
ChevronTexaco ISO 32 Refrigeration Oil WF FeaturesChevron Refrigeration Oils WF are manufactured using medium viscosity index straight mineral oils. The base stocks are carefully selected to assure the low pour points that are necessary for.. |