Polyram Bondyram® TL1306 Maleic Anhydride Modified Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Polyram
Trade Name BondyRam®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram Bondyram® TL1306 Maleic Anhydride Modified Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Polyram.
Physical Properties Metric English Comments
Melt Flow 2.8 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.8 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133