Total Petrochemicals Polystyrene 8350 (AS) is a very high impact polystyrene for extrusion and injection molding. This grade has improved environmental stress crack resistance in comparison with standard high impact grades. Total Petrochemicals Polystyrene 8350 (AS) retains good mechanical properties at low temperatures making it suitable for frozen packaging. It receives printing well.Suitable applications for Total Petrochemicals Polystyrene 8350 (AS) includes production of packaging intended for products likely to cause stress cracking.Information provided by Total Petrochemicals.
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D792
Water Absorption 0.060 %
0.060 %
ASTM D570
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
ASTM D955
Melt Flow 5.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
5.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Spiral Flow 45.0 cm

@Temperature 220 °C
17.7 in

@Temperature 428 °F
ASTM D3123
Mechanical Properties Metric English Comments
Hardness, Rockwell R 78
78
ASTM D785
Tensile Strength at Break 24.0 MPa
3480 psi
ASTM D638
Tensile Strength, Yield 26.0 MPa
3770 psi
ASTM D638
Elongation at Break 60 %
60 %
ASTM D638
Tensile Modulus 1.60 GPa
232 ksi
ASTM D638
Flexural Modulus 1.70 GPa
247 ksi
ASTM D790
Izod Impact, Notched (ISO) 14.0 kJ/m²
6.66 ft-lb/in²
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 91.0 µm/m-°C
50.6 µin/in-°F
ASTM D696
Vicat Softening Point 96.0 °C

@Load 1.02 kg
205 °F

@Load 2.25 lb
50°C per hour; ASTM D1525
Heat Distortion Temperature 80.0 °C
176 °F
ASTM D648
Electrical Properties Metric English Comments
Surface Resistance >= 1.00e+13 ohm
>= 1.00e+13 ohm
ISO IEC 93
Dielectric Strength 150 kV/mm
3810 kV/in
ASTM D149