Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Spiral Flow = 17.7 in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Spiral Flow 45.0 cm

@Temperature 220 °C
17.7 in

@Temperature 428 °F
ASTM D3123
Total PSI 8350 (AS) High Impact Polystyrene
Total Petrochemicals Polystyrene 8350 (AS) is a very high impact polystyrene for extrusion and injection molding. This grade has improved environmental stress crack resistance in comparison with st..
Spiral Flow 45.0 cm
17.7 in
AKRO
Akro-Plastic Akromid® S3 GF 23 1 (2917) PA 6.10 Dry, 23% Glass Filled
A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia..
Spiral Flow 45.0 cm
17.7 in
AKRO
Akro-Plastic Akromid® S3 GF15 1 (3223) PA 6.10 Dry, 15% Glass Filled
A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia..
Copyright © lookpolymers.com All Rights Reserved