Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 150 kV/mm | 3810 kV/in | |
Total Lacqrene® 1235 High Impact Polystyrene
(discontinued **) LACQRENE® 1235 is a high gloss, high impact polystyrene used in injection molding and co-extrusion. This grade produces articles with a surface gloss level equivalent to that of certain grades of .. |
|||
Dielectric Strength | 150 kV/mm | 3810 kV/in | |
Total Lacqrene® 2551 Medium Impact Polystyrene
(discontinued **) LACQRENE® 2551 is a high heat resistance, medium impact polystyrene for injection molding. The very high Vicat Softening Point of this grade gives moldings of high rigidity and a good dimensional .. |
|||
Dielectric Strength | 150 kV/mm | 3810 kV/in | |
Total Lacqrene® 3351(AS) Impact Polystyrene
(discontinued **) LACQRENE® 3351 is a high heat resistance, high impact polystyrene for injection molding and extrusion/thermoforming. It is recommended for the manufacture of articles which require good dimensiona.. |
|||
Dielectric Strength | 150 kV/mm | 3810 kV/in | |
Total Lacqrene® 3351(EU) Impact Polystyrene
(discontinued **) LACQRENE® 3351 is a high heat resistance, high impact polystyrene for injection molding and extrusion/thermoforming. It is recommended for the manufacture of articles which require good dimensiona.. |
|||
Dielectric Strength | 150 kV/mm | 3810 kV/in | |
Total Lacqrene® 4241 High Impact Polystyrene
(discontinued **) DescriptionLACQRENE® 14240 is a high heat resistance, high impact polystyrene for the extrusion industry. Good mechanical and thermal properties leads to the production of thermoformed articles of.. |
|||
Dielectric Strength | 150 kV/mm | 3810 kV/in | |
LyondellBasell Lupolen® 3821 D MDPE Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Dielectric Strength | 150 kV/mm | 3810 kV/in | |
LyondellBasell Lupolen® 4261 A HDPE, Blow Molding Grade Easy-to-process bow molding grade for technical containers such as fuel tanks, petrol filler inlets, expansion tanks, horticultural spray tanks, tanks for lawnmowers, disposable containers (up to 10.. |
|||
Dielectric Strength | 150 kV/mm | 3810 kV/in | |
LyondellBasell Lupolen® 5021 D HDPE, Blow Molding Grade Easy flow, blow molding grade for small containers (up to 5 l), bottles for surface-active substances, household chemicals, laundry and dishwashing detergents, sanitary cleaners, cosmetics and pharm.. |
|||
Dielectric Strength | 150 kV/mm | 3810 kV/in | |
LyondellBasell Lupolen® 5231 HX HDPE, Impact Grade Medium flow, impact resistant, very stress-crack resistant grade for closures, bottles that contain carbonated liquids, storage and tote boxes, as well as engineering components.Data was collected b.. |
|||
Dielectric Strength | 150 kV/mm | 3810 kV/in | |
LyondellBasell Lupolen® 5261 Z HDPE, Blow Molding Grade Relatively high viscosity blow molding grade for rigid, stackable and highly shock resistant containers for packaging all types of hazardous materials such as flammable, corrosive, poisonous and sur.. |
|||
Dielectric Strength | 150 kV/mm | 3810 kV/in | |
LyondellBasell Lupolen® 5261 Z HI HDPE Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Dielectric Strength | 150 kV/mm | 3810 kV/in | |
LyondellBasell Lupolen® 5261 ZS HDPE, Blow Molding Grade Relatively high viscosity blow molding grade (similar to Lupolen 5261 Z), but more resistant to stress cracking) for rigid, stackable and highly shock resistant containers for packaging all types of.. |
|||
Dielectric Strength | 150 kV/mm | 3810 kV/in | |
LyondellBasell Lupolen® 5361 A HDPE, Blow Molding Grade Easy-to-process blow molding grade for stackable canisters (up to 60 l), used for packing surface-active liquids, laundry and dishwashing detergents, disinfectants, drums (up to 220 l) for various s.. |
|||
Dielectric Strength | 150 kV/mm | 3810 kV/in | |
LyondellBasell Lupolen® 6031 M HDPE, Injection Molding Grade Easy flow, injection molding grade for fruit crates, tote boxes and bottle crates, cartridges, protective headgear, buckets, dishes, cartridges for adhesive film canisters, aerosol lids, child seats.. |
|||
Dielectric Strength | 150 kV/mm @Frequency 50.0 Hz, Temperature 23.0 °C |
3810 kV/in @Frequency 50.0 Hz, Temperature 73.4 °F |
DIN 40634 or VDE 0345 in air |
Mitsubishi Hostaphan® RN, 190 micron Nominal Thickness Universal Polyethylene Terephthalate Film Hostaphan® RN is a biaxially oriented film made of polyethylene terephthalate (PET) and characterized by outstanding physical properties.Applications:Films for industrial applicationsCoatingLamin.. |
|||
Dielectric Strength | 150 kV/mm @Frequency 50.0 Hz, Temperature 23.0 °C |
3810 kV/in @Frequency 50.0 Hz, Temperature 73.4 °F |
DIN 40634 or VDE 0345 in air or ASTM D149 |
Mitsubishi Hostaphan® WN, 190 micron Nominal Thickness Translucent White Polyethylene Terephthalate Film Hostaphan® WN is a white film made of polyethylene terephthalate (PET) and is well suited for electrical insulating of machines and appliances. The high dielectric strength and large volume resis.. |
|||
Dielectric Strength | 150 kV/mm | 3810 kV/in | |
Total Polystyrene Impact 3450 Aesthetic, High Fluidity, High Heat Resistance, High Impact Polystyrene POLYSTYRENE IMPACT 3450 is a high impact polystyrene with high heat resistance, good flow, high stiffness and good aesthetics. With such an ideal balance of properties, POLYSTYRENE IMPACT 3450 is w.. |
|||
Dielectric Strength | 150 kV/mm | 3810 kV/in | |
Total Polystyrene Impact 6540 Easy Flow Impact Polystyrene POLYSTYRENE IMPACT 6540 is an easy flowing, high impact polystyrene with a good balance of mechanical and thermal properties. This resin combines physical properties such as the flow necessary for .. |
|||
Dielectric Strength | 150 kV/mm | 3810 kV/in | |
Total Polystyrene Impact 8260 Improved Environmental Stress Crack Resistance High Impact Polystyrene POLYSTYRENE IMPACT 8260 is a high impact polystyrene for extrusion and injection applications. This grade has an improved environmental stress crack resistance in comparison with standard high impa.. |
|||
Dielectric Strength | 150 kV/mm | 3810 kV/in | ASTM D149 |
Total PSI 3441 High Heat Resistance Impact Polystyrene Total Petrochemicals Polystyrene 3441 is a high heat resistance, high impact polystyrene for injection molding. It is recommended for the manufacturing of articles which require good dimensional st.. |
|||
Dielectric Strength | 150 kV/mm | 3810 kV/in | |
Total PSI 4440(EU) High Impact Polystyrene 4440 is a high impact polystyrene for the injection molding of parts demanding good dimensional stability at high temperatures, particularly front and back covers for television sets. In addition, .. |
|||
Dielectric Strength | 150 kV/mm | 3810 kV/in | ASTM D149 |
Total PSI 8350 (AS) High Impact Polystyrene Total Petrochemicals Polystyrene 8350 (AS) is a very high impact polystyrene for extrusion and injection molding. This grade has improved environmental stress crack resistance in comparison with st.. |
|||
Dielectric Strength | 150 kV/mm | 3810 kV/in | |
Total PSI 8350 High Impact Polystyrene 8350 is a very high impact polystyrene for extrusion. This grade has an improved environmental stress crack resistance in comparison with standard high impact grades. It is proposed for the produc.. |
|||
Dielectric Strength | 150 kV/mm | 3810 kV/in | ASTM D149 |
Total PSI 3341 High Impact Polystyrene Total Petrochemicals Polystyrene 3341 is a high impact polystyrene for the extrusion industry. Its good mechanical and thermal properties leads to the production of thermoformed articles of good ri.. |
|||
Dielectric Strength | 150 kV/mm | 3810 kV/in | |
Total PSI 4440(AS) High Impact Polystyrene 4440 is a high impact polystyrene for the injection molding of parts demanding good dimensional stability at high temperatures, particularly front and back covers for television sets. In addition, .. |
|||
Dielectric Strength | 150 kV/mm | 3810 kV/in | Breakdown; DIN 53 481, IEC-243, VDE 0303 Part 1 |
Hippe PE 300 Polyethylene Tough, flexible and stiff, depending on the crystalline structure (density). Resinous surface. Excellent dielectric properties, Good resistance against solvents, acids and alkalis. Physiologicall.. |
|||
Dielectric Strength | 150 kV/mm | 3810 kV/in | |
Total Lacqrene® 4801
(discontinued **) LACQRENE® 4801 is an easy flowing, high impact polystyrene for injection molding. The very good processing characteristics of this grade allows for the production of thin articles with long flow p.. |
|||
Dielectric Strength | 150 kV/mm | 3810 kV/in | |
Total Lacqrene® 6630 Impact Polystyrene
(discontinued **) LACQRENE® 6630 and 6631 are easy flowing, high impact polystyrenes for injection molding. With easy processing, good rigidity and ease of coloration. These grades find a wide range of application.. |
|||
Dielectric Strength | 150 kV/mm | 3810 kV/in | |
Total Lacqrene® 6631 Impact Polystyrene
(discontinued **) LACQRENE® 6630 and 6631 are easy flowing, high impact polystyrenes for injection molding. With easy processing, good rigidity and ease of coloration. These grades find a wide range of application.. |
|||
Dielectric Strength | 150 kV/mm | 3810 kV/in | |
Total Lacqrene® 740 High Impact Polystyrene
(discontinued **) LACQRENE® alpha 740 is a high gloss, high impact grade of polystyrene.ApplicationWhite goods (washing machines, driers), Toys and games, Garden equipment, All applications needing high gloss with g.. |