EMS-Grivory Grivory® L 25 W 40 PA12

Category Polymer , Thermoplastic , Nylon , Nylon 12
Manufacturer EMS-Grivory (EMS-CHEMIE)
Trade Name Grivory®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Grivory Grivory® L 25 W 40 PA12.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: Grilamid L 25 W 40 is a flexible, plasticised, high viscosity extrusion grade of Polyamide 12 (PA12) Grilamid L 25 W 40 is UV and heat stabilized. The main features of Grilamid L 25 W 40 are: FlexibleUV and heat stabilityLow density, low weightEasy processing Application examples: Grilamid L 25 W 40 is particularly suitable for the production of flexible tubes and profiles used in automotive and industrial applications.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
ISO 1183
Water Absorption 1.4 %
1.4 %
ISO 62
Moisture Absorption 0.700 %
0.700 %
ISO 62
Linear Mold Shrinkage, Flow 0.0090 cm/cm
0.0090 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.013 cm/cm
0.013 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
conditioned, 15s; ISO 868
Tensile Strength at Break 40.0 MPa
5800 psi
conditioned; ISO 527-1/-2
45.0 MPa
6530 psi
dry; ISO 527-1/-2
Tensile Strength, Yield 25.0 MPa
3630 psi
dry; ISO 527-1/-2
30.0 MPa
4350 psi
dry; ISO 527-1/-2
Elongation at Break >= 50 %
>= 50 %
conditioned; ISO 527-1/-2
<= 50 %
<= 50 %
dry; ISO 527-1/-2
Elongation at Yield 15 %
15 %
dry; ISO 527-1/-2
20 %
20 %
conditioned; ISO 527-1/-2
Tensile Modulus 0.400 GPa
58.0 ksi
conditioned; ISO 527-1/-2
0.450 GPa
65.3 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched NB
NB
dry; ISO 179/1eU
NB
NB
conditioned; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
dry; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched NB
NB
conditioned; ISO 179/1eA
0.400 J/cm²

@Temperature 30.0 °C
1.90 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 140 µm/m-°C
77.8 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 180 µm/m-°C
100 µin/in-°F
ISO 11359-1/-2
Melting Point 173 °C
343 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 80.0 - 100 °C
176 - 212 °F
long term; EMS
150 °C
302 °F
short term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C
203 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 45.0 °C
113 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
conditioned; IEC 60093
Surface Resistance 1.00e+11 ohm
1.00e+11 ohm
IEC 60093
Dielectric Strength 32.0 kV/mm
813 kV/in
conditioned; IEC 60243-1
Comparative Tracking Index 600 V
600 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Additives Plasticizer
Form Granules
Industry & Consumer goods Hydraulics & Pneumatics
Processing Other Extrusion
Product Attributes Flexible
High viscosity
Special Characteristics Improved UV resistance (outdoor use)