Polymer Property : CTE, linear = 50.6 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 91.0 µm/m-°C

@Temperature 20.0 °C
50.6 µin/in-°F

@Temperature 68.0 °F
Total Lacqrene® 1235 High Impact Polystyrene  (discontinued **)
LACQRENE® 1235 is a high gloss, high impact polystyrene used in injection molding and co-extrusion. This grade produces articles with a surface gloss level equivalent to that of certain grades of ..
CTE, linear 91.0 µm/m-°C

@Temperature 20.0 °C
50.6 µin/in-°F

@Temperature 68.0 °F
Total Lacqrene® 2551 Medium Impact Polystyrene  (discontinued **)
LACQRENE® 2551 is a high heat resistance, medium impact polystyrene for injection molding. The very high Vicat Softening Point of this grade gives moldings of high rigidity and a good dimensional ..
CTE, linear 91.0 µm/m-°C

@Temperature 20.0 °C
50.6 µin/in-°F

@Temperature 68.0 °F
Total Lacqrene® 3351(AS) Impact Polystyrene  (discontinued **)
LACQRENE® 3351 is a high heat resistance, high impact polystyrene for injection molding and extrusion/thermoforming. It is recommended for the manufacture of articles which require good dimensiona..
CTE, linear 91.0 µm/m-°C

@Temperature 20.0 °C
50.6 µin/in-°F

@Temperature 68.0 °F
Total Lacqrene® 3351(EU) Impact Polystyrene  (discontinued **)
LACQRENE® 3351 is a high heat resistance, high impact polystyrene for injection molding and extrusion/thermoforming. It is recommended for the manufacture of articles which require good dimensiona..
CTE, linear 91.0 µm/m-°C

@Temperature 20.0 °C
50.6 µin/in-°F

@Temperature 68.0 °F
Total Lacqrene® 4240(EU) High Impact Polystyrene  (discontinued **)
LACQRENE® 4240 is a high heat resistance, high impact polystyrene for the extrusion industry. Good mechanical and thermal properties leads to the production of thermoformed articles of good rigidi..
CTE, linear 91.0 µm/m-°C

@Temperature 20.0 °C
50.6 µin/in-°F

@Temperature 68.0 °F
Total Lacqrene® 4241 High Impact Polystyrene  (discontinued **)
DescriptionLACQRENE® 14240 is a high heat resistance, high impact polystyrene for the extrusion industry. Good mechanical and thermal properties leads to the production of thermoformed articles of..
CTE, linear 91.0 µm/m-°C
50.6 µin/in-°F
Total Polystyrene Impact 3450 Aesthetic, High Fluidity, High Heat Resistance, High Impact Polystyrene
POLYSTYRENE IMPACT 3450 is a high impact polystyrene with high heat resistance, good flow, high stiffness and good aesthetics. With such an ideal balance of properties, POLYSTYRENE IMPACT 3450 is w..
CTE, linear 91.0 µm/m-°C
50.6 µin/in-°F
Total Polystyrene Impact 6540 Easy Flow Impact Polystyrene
POLYSTYRENE IMPACT 6540 is an easy flowing, high impact polystyrene with a good balance of mechanical and thermal properties. This resin combines physical properties such as the flow necessary for ..
CTE, linear 91.0 µm/m-°C
50.6 µin/in-°F
Total Polystyrene Impact 8260 Improved Environmental Stress Crack Resistance High Impact Polystyrene
POLYSTYRENE IMPACT 8260 is a high impact polystyrene for extrusion and injection applications. This grade has an improved environmental stress crack resistance in comparison with standard high impa..
CTE, linear 91.0 µm/m-°C
50.6 µin/in-°F
ASTM D696
Total PS CPDS 849 High Flow, High Heat Resistance Polystyrene
Total Petrochemicals Polystyrene 849 is a high flow, high heat resistant polystyrene for injection molding. It is recommended for the manufacturing of articles which require good dimensional stabil..
CTE, linear 91.0 µm/m-°C
50.6 µin/in-°F
ASTM D696
Total PS CPDS 850S Chlorine and Bromine Free Flame Retardant High Impact Polystyrene
Total Petrochemicals Polystyrene 850S is a chlorine and bromine free flame retardant high impact polystyrene with excellent thermal stability and processability for injection molding.Suitable Applic..
CTE, linear 91.0 µm/m-°C
50.6 µin/in-°F
ASTM D696
Total PS CPDS 855S Chlorine and Bromine Free Flame Retardant High Impact Polystyrene
Total Petrochemicals Polystyrene 855S is a chlorine and bromine free flame retardant high impact polystyrene with excellent thermal stability and processability for injection molding.Suitable Applic..
CTE, linear 91.0 µm/m-°C
50.6 µin/in-°F
ASTM D696
Total PS CPDS 856S Chlorine and Bromine Free Flame Retardant High Impact Polystyrene
Total Petrochemicals Polystyrene 856S is a chlorine and bromine free flame retardant high impact polystyrene with excellent thermal stability and processability for injection molding.Suitable Applic..
CTE, linear 91.0 µm/m-°C
50.6 µin/in-°F
ASTM D696
Total PSI 3351 High Heat Resistance Impact Polystyrene
Total Petrochemicals Polystyrene 3351 is a high heat resistance, high impact polystyrene for injection molding. It is recommended for the manufacturing of articles which require good dimensional st..
CTE, linear 91.0 µm/m-°C

@Temperature 20.0 °C
50.6 µin/in-°F

@Temperature 68.0 °F
Total PSI 3630 Medium Impact Polystyrene
3630 is an easy flowing, medium impact polystyrene for injection molding. This grade offers a good compromise of flow and softening point allowing for the production of large and complex articles a..
CTE, linear 91.0 µm/m-°C

@Temperature 20.0 °C
50.6 µin/in-°F

@Temperature 68.0 °F
Total PSI 4440(EU) High Impact Polystyrene
4440 is a high impact polystyrene for the injection molding of parts demanding good dimensional stability at high temperatures, particularly front and back covers for television sets. In addition, ..
CTE, linear 91.0 µm/m-°C

@Temperature 20.0 °C
50.6 µin/in-°F

@Temperature 68.0 °F
Total PSI 7240 High Impact Polystyrene
7240 is a very high impact polystyrene for the extrusion industry. This grade has been designed to be diluted with crystal polystyrene (such as LACQRENE® 140, 1340 or 1540) at higher levels than c..
CTE, linear 91.0 µm/m-°C
50.6 µin/in-°F
ASTM D696
Total PSI 8350 (AS) High Impact Polystyrene
Total Petrochemicals Polystyrene 8350 (AS) is a very high impact polystyrene for extrusion and injection molding. This grade has improved environmental stress crack resistance in comparison with st..
CTE, linear 91.0 µm/m-°C

@Temperature 20.0 °C
50.6 µin/in-°F

@Temperature 68.0 °F
Total PSI 8350 High Impact Polystyrene
8350 is a very high impact polystyrene for extrusion. This grade has an improved environmental stress crack resistance in comparison with standard high impact grades. It is proposed for the produc..
CTE, linear 91.0 µm/m-°C

@Temperature 20.0 °C
50.6 µin/in-°F

@Temperature 68.0 °F
Total PSI 4440(AS) High Impact Polystyrene
4440 is a high impact polystyrene for the injection molding of parts demanding good dimensional stability at high temperatures, particularly front and back covers for television sets. In addition, ..
CTE, linear 91.0 µm/m-°C

@Temperature 20.0 °C
50.6 µin/in-°F

@Temperature 68.0 °F
Total Lacqrene® 2901 Medium Impact Polystyrene  (discontinued **)
LACQRENE® 2901 is a very easy flowing, medium impact polystyrene for injection molding. The very high flow of this grade allows for the production of thin wall section or long flow path molding on..
CTE, linear 91.0 µm/m-°C

@Temperature 20.0 °C
50.6 µin/in-°F

@Temperature 68.0 °F
Total Lacqrene® 4801  (discontinued **)
LACQRENE® 4801 is an easy flowing, high impact polystyrene for injection molding. The very good processing characteristics of this grade allows for the production of thin articles with long flow p..
CTE, linear 91.0 µm/m-°C

@Temperature 20.0 °C
50.6 µin/in-°F

@Temperature 68.0 °F
Total Lacqrene® 6630 Impact Polystyrene  (discontinued **)
LACQRENE® 6630 and 6631 are easy flowing, high impact polystyrenes for injection molding. With easy processing, good rigidity and ease of coloration. These grades find a wide range of application..
CTE, linear 91.0 µm/m-°C

@Temperature 20.0 °C
50.6 µin/in-°F

@Temperature 68.0 °F
Total Lacqrene® 6631 Impact Polystyrene  (discontinued **)
LACQRENE® 6630 and 6631 are easy flowing, high impact polystyrenes for injection molding. With easy processing, good rigidity and ease of coloration. These grades find a wide range of application..
CTE, linear 91.0 µm/m-°C

@Temperature 20.0 °C
50.6 µin/in-°F

@Temperature 68.0 °F
Total Lacqrene® 740 High Impact Polystyrene  (discontinued **)
LACQRENE® alpha 740 is a high gloss, high impact grade of polystyrene.ApplicationWhite goods (washing machines, driers), Toys and games, Garden equipment, All applications needing high gloss with g..