Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Total Lumicene® mPE M6040 S01 Metallocene Polyethylene, Cast Film

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Film Grade
Manufacturer Total Atofina
Trade Name Lumicene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total Lumicene® mPE M6040 S01 Metallocene Polyethylene, Cast Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Lumicene® mPE M 6040 S01 is a second generation metallocene high density polyethylene.Lumicene® mPE M 6040 S01 can be processed at high output rates with low extrusion pressure, low neck-in, excellent drawability and gauge control in comparison with conventional LLDPE and first generation metallocene based polyethylene. The high stiffness combined with good optical properties brings a significant down-gauging potential.Lumicene® mPE M 6040 S01 is a versatile resin that can be used in pure or in blend for the production of both monolayer and multilayer film. Typical applications are: specialty film, hygiene film, embossed film, compounds and consumer and automatic packaging, such as produce bags, mailing and overwrap film. The high density of Lumicene® mPE M 6040 S01 enables its use in applications with moisture barrier requirements, such as dry food packaging, and brings improved heat resistance, compared to commonly used HDPE.Information provided by Total Petrochemicals.
Physical Properties Metric English Comments
Specific Gravity 0.960 g/cc
0.960 g/cc
ISO 1183
Thickness 20.0 microns
0.787 mil
Melt Flow 4.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
4.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 23.0 MPa
3340 psi
ISO 527-3
Film Tensile Strength at Yield, TD 24.0 MPa
3480 psi
ISO 527-3
Film Elongation at Break, MD 520 %
520 %
ISO 527-3
Film Elongation at Break, TD 850 %
850 %
ISO 527-3
Elmendorf Tear Strength, MD 0.800 g/micron
20.3 g/mil
ISO 6383-2
Elmendorf Tear Strength, TD 7.10 g/micron
180 g/mil
ISO 6383-2
Dart Drop Test 40.0 g
0.0882 lb
ISO 7765-1
Film Tensile Strength at Break, MD 26.0 MPa
3770 psi
ISO 527-3
Film Tensile Strength at Break, TD 34.0 MPa
4930 psi
ISO 527-3
Thermal Properties Metric English Comments
Melting Point 134 °C
273 °F
ISO 11357
Vicat Softening Point 132 °C
270 °F
ISO 306
Optical Properties Metric English Comments
Haze 12 %
12 %
ISO 14782
Gloss 51 %
51 %
at 45°; ASTM D2457
Processing Properties Metric English Comments
Processing Temperature 20.0 - 80.0 °C
68.0 - 176 °F
Chill Roll
Melt Temperature 220 - 280 °C
428 - 536 °F
Extrusion