Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 20.0 - 30.0 °C | 68.0 - 86.0 °F | Curing Agent Temperature |
Northstar Polymers MYP-V40A Polyurethane Filler Gel This polyurethane casting material is developed for applications that require inexpensive liquid resin filler such as encapsulation of a large electric components or puncture-free tire for low-speed.. |
|||
Processing Temperature | 20.0 - 50.0 °C | 68.0 - 122 °F | |
Celanese Celanex® 2002-3 PBT
(Unverified Data**) Celanex 2002-3 is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability. Celanex 2002-3 is a medium flow material that contains .. |
|||
Processing Temperature | 20.0 - 50.0 °C | 68.0 - 122 °F | |
Celanese Celanex® 3316 PBT, 30% Glass Reinforced
(Unverified Data**) Celanex 3316 is a non-exuding flame retarded (UL and CSA approved V-0 at 1/32 inch and 5V at 1/16 inch), 30% fiberglass reinforced polybutylene terephthalate which has an excellent balance of mechan.. |
|||
Processing Temperature | 20.0 - 50.0 °C | 68.0 - 122 °F | |
Celanese Celanex® 4300 PBT, 30% Glass Reinforced
(Unverified Data**) Celanex 4300 is a toughened, 30% glass reinforced PBT.30% glass-fiber, good impact strengthInformation provided by Celanese |
|||
Processing Temperature | 20.0 - 50.0 °C | 68.0 - 122 °F | |
Celanese Celanex® 6400-2 PBT, Mineral / Glass Reinforced
(Unverified Data**) 40% glass/mineral reinforced polyester, providing warp resistance and improved surface finish.40% glass/mineral filled, low warpInformation provided by Celanese |
|||
Processing Temperature | 20.0 - 50.0 °C | 68.0 - 122 °F | |
Celanese Celstran® PBT-GF40-08 PBT, 40% Glass Reinforced
(Unverified Data**) 40% Long Glass Fiber Reinforced PBT40% Long Glass Fiber Reinforced PBTCelstran can be processed on a standard injection molding unit.Information provided by Celanese |
|||
Processing Temperature | 20.0 - 50.0 °C | 68.0 - 122 °F | |
Celanese Vandar® 4602Z PBT
(Unverified Data**) 4602Z is an unfilled thermoplastic alloy with good weatherability and chemical resistance.Unreinforced, good chemical resistanceInformation provided by Celanese |
|||
Processing Temperature | 20.0 - 30.0 °C | 68.0 - 86.0 °F | |
Celanese Hostaform® C 13031 K POM, Tribological
(Unverified Data**) Chemical abbreviation according to ISO 1043-1: POMInjection molding grade with moderate flow and higher strength, rigidity and hardness, with special chalk modifiedInformation provided by Celanese |
|||
Processing Temperature | 20.0 - 30.0 °C | 68.0 - 86.0 °F | |
Celanese Hostaform® C 9021 G POM, Tribological
(Unverified Data**) Chemical abbreviation according to ISO 1043-1: POMInjection molding type like C 9021, with (R) GUR (PE-UHMW) modifiedInformation provided by Celanese |
|||
Processing Temperature | 20.0 - 30.0 °C | 68.0 - 86.0 °F | |
Celanese Hostaform® MT8U05 POM, Medical Technology
(Unverified Data**) Hostaform® acetal copolymer grade MT8U05 is a special grade developed for medical industry applications containing low residual monomers and no animal products. The material can be identified by U.. |
|||
Processing Temperature | 20.0 - 30.0 °C | 68.0 - 86.0 °F | |
Celanese VECTRA A430 LCP, 25% Specialty
(Unverified Data**) Provides many of the characteristics of A130 with added lubricity. Suitable for applications requiring excellent wear characteristics. Excellent electrical properties at high frequencies. LCP/PTF.. |
|||
Processing Temperature | 20.0 - 30.0 °C | 68.0 - 86.0 °F | |
Celanese VECTRA E115i LCP, 15% Glass Reinforced
(Unverified Data**) 15% Glass ReinforcedInformation provided by Celanese |
|||
Processing Temperature | 20.0 - 30.0 °C | 68.0 - 86.0 °F | |
Celanese VECTRA MT1310 LCP, 30% Medical Technology
(Unverified Data**) The Standard for the Industry. Excellent balance of properties, including easy flow, easy processing, thermal stability, chemical resistance, mechanical and electrical properties. Suitable for vapo.. |
|||
Processing Temperature | 20.0 - 30.0 °C | 68.0 - 86.0 °F | |
Celanese ZENITE 5145L LCP, 45% Glass Reinforced
(Unverified Data**) Zenite® 5145L is a 45% glass fiber reinforced and toughened liquid crystal polymer for injection molding. It has improved toughness.45% glass reinforced, lubricatedInformation provided by Celanese |
|||
Processing Temperature | 20.0 - 30.0 °C | 68.0 - 86.0 °F | |
Celanese FORTRON 1140L4 PPS, 40% Glass Reinforced
(Unverified Data**) Fortron 1140L4 is a 40% glass-reinforced grade that is the strongest and toughest product available. It exhibits excellent heat and chemical resistance, good electrical properties and is inherently .. |
|||
Processing Temperature | 20.0 °C | 68.0 °F | typically used at ambient temperature |
Elmer's Products Aron Alpha® 102 Cyanoacrylate Adhesive (Industrial Krazy Glue™) Superior tensile and shear strengths, well suited for metal bondingMedium gap fill. Methyl base monomer. Excellent on rubber/plastic substrates. Excellent on metal substrates. Poor on porous sub.. |
|||
Processing Temperature | 20.0 °C | 68.0 °F | typically used at ambient temperature |
Elmer's Products Aron Alpha® 402X Cyanoacrylate Adhesive (Industrial Krazy Glue™) Engineered for high temperature and high impact resistance.Medium gap fill. Ethyl base monomer. Excellent on rubber/plastic substrates. Excellent on metal substrates. Poor on porous substrates. .. |
|||
Processing Temperature | 20.0 - 30.0 °C | 68.0 - 86.0 °F | |
Celanese Hostaform® S 27063 XAP² ™ POM, Impact Modified POM copolymer, impact modifiedImpact modified, low emissionInformation provided by Celanese |
|||
Processing Temperature | 20.0 - 50.0 °C | 68.0 - 122 °F | hopper |
Celanese Celanex® 2002UV PBT, Unfilled Celanex 2002UV is a general purpose,unreinforced polybutylene terephthalate with a good balance of mechanical properties, processability and UV resistance. Celanex 2002UV is a medium flow materialTo.. |
|||
Processing Temperature | 20.0 °C | 68.0 °F | |
3M Pronto™ CA-40H Instant Adhesive One-part, room-temperature curing adhesive that is ready-to-use without metering or mixing. Bonded parts reach handling strength in 5-10 seconds on many applications.A higher viscosity, slower sett.. |
|||
Processing Temperature | 20.0 - 30.0 °C | 68.0 - 86.0 °F | hopper |
Celanese FORTRON MT9205C4 PPS, Medical Technology Fortron MT9205C4 is an unfilled grade with a low melt viscosity used for custom compounding and extrusion. It demonstrates an excellent chemical resistance and thermal stability. Components made wi.. |
|||
Processing Temperature | 20.0 - 30.0 °C | 68.0 - 86.0 °F | hopper |
Celanese Hostaform® S 9243 XAP2 ™ POM, Impact Modified POM copolymer, modifiedIt is normally not necessary to dry HOSTAFORM. However, should there be surface moisture (condensate) on the molding compound as a result of incorrect storage, drying is requi.. |
|||
Processing Temperature | 20.0 - 30.0 °C | 68.0 - 86.0 °F | |
Celanese Hostaform® C 9021 AW POM, Tribological
(Unverified Data**) Chemical abbreviation according to ISO 1043-1: POMInjection molding type like C 9021, with special additive modifiedInformation provided by Celanese |
|||
Processing Temperature | 20.0 - 30.0 °C | 68.0 - 86.0 °F | |
Celanese Hostaform® C 9021 GV1/20 XGM POM, 20% Tribological
(Unverified Data**) Chemical abbreviation according to ISO 1043-1: POMlow wear, 20% fiberglass reinforced, PTFE containing gradeInformation provided by Celanese |
|||
Processing Temperature | 20.0 - 30.0 °C | 68.0 - 86.0 °F | |
Celanese FORTRON 1130L0 PPS, 30% Glass Reinforced
(Unverified Data**) Fortron 1130L0 is a 30% glass-reinforced extrusion grade. It exhibits excellent heat and chemical resistance, good electrical properties and is inherently flame-retardant. The high hardness and rig.. |
|||
Processing Temperature | 20.0 - 30.0 °C | 68.0 - 86.0 °F | |
Celanese FORTRON 4184L6 PPS, 53% Mineral / Glass Reinforced
(Unverified Data**) Fortron 4184L6 is an easier flow version of Fortron 4184L4. It offers similar characteristics to the 4184L4. This grade is especially used for thin walled parts requiring long flow lengths, stiffnes.. |
|||
Processing Temperature | 20.0 - 30.0 °C | 68.0 - 86.0 °F | |
Celanese FORTRON MT9320C0 PPS, Medical Technology
(Unverified Data**) Fortron MT9320C0 is an unfilled grade used for extrusion applications. It demonstrates excellent chemical resistance and thermal stability as well as a high melt strength. Components made of this g.. |
|||
Processing Temperature | 20.0 - 50.0 °C | 68.0 - 122 °F | |
Celanese Celanex® 1400FC PBT
(Unverified Data**) Celanex 1400FC is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability for use in food contact applications. Celanex 1400FC is a.. |
|||
Processing Temperature | 20.0 - 30.0 °C | 68.0 - 86.0 °F | |
Celanese FORTRON 11400000000 PPS, 40% Glass Reinforced
(Unverified Data**) Fortron 1140E7 is an inherently flame-retardant grade exhibiting extremely low flash and fast cycle times. It has excellent electrical properties, high hardness and stiffness. This grade exhibits go.. |
|||
Processing Temperature | 20.0 - 50.0 °C | 68.0 - 122 °F | hopper |
Celanese Celanex® 3116 PBT, 7.5% Glass Reinforced Celanex 3116 is a non-exuding flame retarded (UL and CSA approved V-0 at 1/32 inch and 5V at 1/8 inch), 7.5% fiberglass reinforced polybutylene terephthalate which has an excellent balance of mechan.. |