Polymer Property : Elmendorf Tear Strength, MD = 0.800 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, MD 0.800 g/micron
20.3 g/mil
ASTM D1922
SABIC F00952 High Density Polyethylene for Blown Film
Product Description: F00952 is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, broad molecular weigh..
Elmendorf Tear Strength, MD 0.800 g/micron
20.3 g/mil
ASTM D1922
SABIC F00952EQ High Density Polyethylene for Blown Film
Product Description: F00952EQ is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. the design of the product, molecular architect..
Elmendorf Tear Strength, MD 0.800 g/micron
20.3 g/mil
ASTM D1922
SABIC FJ00952 High Density Polyethylene for Blown Film
Product Description: FJ00952 is a TNPP additive free, high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, ..
Elmendorf Tear Strength, MD 0.800 g/micron
20.3 g/mil
ASTM D1922
Reliance Industries Relene F46003 Polyethylene
Relene F46003 is a High Density Polyethylene grade suitable for producing blown parts with superior stiffness and barrier properties. It is recommended for making liners and coextruded film structu..
Elmendorf Tear Strength, MD 0.800 - 3.94 g/micron
20.3 - 100 g/mil
Average value: 1.83 g/micron Grade Count:9
Overview of materials for Medium Density Polyethylene (MDPE), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Film Grade". Each property range of values reported is minimum and m..
Elmendorf Tear Strength, MD 0.800 g/micron
20.3 g/mil
ASTM D1922
Braskem ES 300 HDPE Blown Film Extrusion Polyethylene  (discontinued **)
38µm film gauge, obtained in 75mm extruder, die gap 1.0mm, output 1.75 kg/h-cm with 2:1 BUR. Applications: Grocery and T-shirt bags; merchandise bags; frozen-food bags; high-strength films. Informa..
Elmendorf Tear Strength, MD 0.800 g/micron
20.3 g/mil
ISO 6383-2
Total Lumicene® mPE M6040 S01 Metallocene Polyethylene, Cast Film
Lumicene® mPE M 6040 S01 is a second generation metallocene high density polyethylene.Lumicene® mPE M 6040 S01 can be processed at high output rates with low extrusion pressure, low neck-in, excel..
Elmendorf Tear Strength, MD 0.800 g/micron
20.3 g/mil
ASTM-D1922
Braskem LL3800N HDPE Cast Film Extrusion Polyethylene Copolymer
The resin LL3800N is a high-density polyethylene, copolymer octene-1, produced by the solution process for the extrusion of plain films with excellent mechanical properties. It has an antirust addit..