Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 26.0 MPa | 3770 psi | ISO 527-3 |
Polimeri Europa Riblene® FF 29 Low Density Polyethylene - Blown Film Extrusion Riblene FF 29 is a high molecular weight low density polyethylene (LDPE), suitable for blown film extrusion. Riblene FF 29 is characterized by a good melt strength leading to a good bubble stabilit.. |
|||
Film Tensile Strength at Break, MD | 26.0 MPa | 3770 psi | ISO 527 |
Premix Thermoplastics PRE-ELEC® PE 1291 PRE-ELEC PE 1291 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 129.. |
|||
Film Tensile Strength at Break, MD | 26.0 MPa | 3770 psi | ASTM D882 |
Petroquimica Triunfo Trithene® TN 7006 LDPE - Coextruded Film The Trithene® TS 7006 resin is a low-density polyethylene (LDPE) with high molecular weight and very good clarity. The unique combination of good processability, bubble stability, gloss, and streng.. |
|||
Film Tensile Strength at Break, MD | 26.0 MPa | 3770 psi | ASTM D882 |
Petroquimica Triunfo Trithene® TS 7006 LDPE - Coextruded Film The Trithene TS 7006 resin is a low-density polyethylene (LDPE) with high molecular weight and very good clarity. The unique combination of good processability, bubble stability, gloss, and strength.. |
|||
Film Tensile Strength at Break, MD | 26.0 MPa | 3770 psi | ISO 527-3 |
Polimeri Europa Greenflex® FD 20 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion Greenflex FD 20 is an ethylene vinyl acetate copolymer (EVA) suitable for blown film extrusion. Films produced with Greenflex FD 20 exhibit good optical properties, high impact resistance, tensile .. |
|||
Film Tensile Strength at Break, MD | 26.0 MPa | 3770 psi | ASTM D882 |
Eastman 1925F Polyethylene Film
(discontinued **) Polyethylene 1925F is a low density formulation with medium slip and medium antiblock. It is suggested for film applications that require heat-sealing treated-to-treated film surfaces and where good.. |
|||
Film Tensile Strength at Break, MD | 26.0 MPa | 3770 psi | ASTM D882 |
Eastman E6838-795F Polyethylene
(discontinued **) E6838-795F is a low density formulation with no slip or antiblock level. It is suggested for film applications that require a good balance of properties such as converter film for industrial packag.. |
|||
Film Tensile Strength at Break, MD | 26.0 MPa | 3770 psi | ASTM D882 |
Eastman E6838-796F Polyethylene
(discontinued **) E6838-796F is a low density formulation with no slip or antiblock. It is suggested for film applications requiring a good balance of properties, such as converter film for industrial packaging, gen.. |
|||
Film Tensile Strength at Break, MD | 26.0 MPa | 3770 psi | ASTM D882 |
ExxonMobil Escorene® LD-317 EVA Film Resin, FMI
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A fractional melt index, 5.5% vinyl acetate copolymer film resin. Film made from LD-317 offers excellent impact strength, tensile properties, and h.. |
|||
Film Tensile Strength at Break, MD | 26.0 MPa | 3770 psi | |
Borealis FA5223 Low Density Polyethylene FA5223 is a Low Density Polyethylene for Film Extrusion. Contains antioxidant and antiblock additive. This grade is developed to give strong film for medium duty applications. Applications FA5223.. |
|||
Film Tensile Strength at Break, MD | 26.0 MPa | 3770 psi | ISO 527-3 |
Borealis FA5224 Low Density Polyethylene FA5224 is a Low Density Polyethylene for Film Extrusion. Contains Antioxidant, Anti-block and Medium Slip additives. This grade is developed to give strong film for medium duty applications. Appl.. |
|||
Film Tensile Strength at Break, MD | 26.0 MPa | 3770 psi | ISO 527-2 |
Borealis FA6220 Low Density Polyethylene FA6220 is a Low Density Polyethylene for Film Extrusion. Includes Antioxidant. This grade is developed for the production of thin blown films. Applications: shrink film, pouches, general packagin.. |
|||
Film Tensile Strength at Break, MD | 26.0 MPa | 3770 psi | ISO 527-3 |
Borealis FA6224 Low Density Polyethylene FA6224 is a Low Density Polyethylene for Film Extrusion. Autoclave Technology. Contains Antioxidant, Anti-block and Medium Slip additives. This grade is developed for the production of thin blown f.. |
|||
Film Tensile Strength at Break, MD | 26.0 MPa | 3770 psi | ISO 527-3 |
Total Lumicene® mPE M6040 S01 Metallocene Polyethylene, Cast Film Lumicene® mPE M 6040 S01 is a second generation metallocene high density polyethylene.Lumicene® mPE M 6040 S01 can be processed at high output rates with low extrusion pressure, low neck-in, excel.. |
|||
Film Tensile Strength at Break, MD | 26.0 MPa | 3770 psi | ASTM D882 |
Teknor Apex Terraloy™ BP 20001A Thermoplastic Starch + Copolyester Notes: Terraloy™ BP-20001A is a Thermoplastic Starch/Biodegradable Copolyester ready-to-process compound that contains up to 40% of TPS renewable content and is 100% biodegradable. This compound i.. |
|||
Film Tensile Strength at Break, MD | 26.0 MPa | 3770 psi | ASTM-D882 |
Braskem LF 118/21 LLDPE Blown Film Extrusion Polyethylene Copolymer LF 118/21 is a LLDPE Butene copolymer produced by Braskem. It was specially designed to provide outstanding processing performance. Films obtained with this grade show good physical and optical prop.. |
|||
Film Tensile Strength at Break, MD | 26.0 MPa | 3770 psi | ISO 1184 |
Carmel Olefins IPETHENE® 111 Low Density Polyethylene IPETHENE® 111 is a low density polyethylene extrusion grade, contains no additives. It exhibits a good balance between mechanical and optical properties. APPLICATIONS IPETHENE® 111 is used to pr.. |
|||
Film Tensile Strength at Break, MD | 26.0 MPa | 3770 psi | ISO 1184 |
Carmel Olefins IPETHENE® 113 Low Density Polyethylene IPETHENE® 113 is a general purpose low density polyethylene film extrusion grade. It contains medium level of anti-blocking and slip additives. It is BHT free. It exhibits a good balance between me.. |
|||
Film Tensile Strength at Break, MD | 26.0 MPa | 3770 psi | ASTM D882 |
Huntsman Rexell® L3103 Blown Film Extrusion LLDPE
(discontinued **) Linear-low density copolymer, cast film extrusion, FDA compliant.Features: Excellent optics and sealability with good toughnessApplications: Stretch wrap and coextruded film for general packaging.FD.. |
|||
Film Tensile Strength at Break, MD | 26.0 MPa | 3770 psi | ASTM D882 |
ExxonMobil Escorene® LD-316 EVA Film Resin, High Clarity, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 1.9% vinyl acetate copolymer, high clarity film resin. Film made from LD-316 offers improved impact strength and heat sealability versus homopoly.. |
|||
Film Tensile Strength at Break, MD | 26.0 MPa | 3770 psi | ASTM D882 |
Eastman D4036-F Polyethylene
(discontinued **) D4036-F is a low density formulation with high slip and high antiblock. It is suggested for film applications requiring a good balance of properties, such as converter film for industrial and gener.. |
|||
Film Tensile Strength at Break, MD | 26.0 MPa | 3770 psi | ASTM D882 |
Eastman E6838-963F Polyethylene
(discontinued **) E6838-963F is a low density formulation with medium slip and medium antiblock. It is suggested for film applications that require a good balance of physical and optical properties.List of Applicati.. |